    New rods at Tractor Supply

    I was perusing a newly opened Tractor Supply near me today and notice they now have hermetically sealed 10 lb cans of 7018 H4R rods. The packaging looks almost identical to the Lincoln Excalibur H4R rods. Same white tin with the pull tab lid. Could be a fluke I guess, but I wonder if they are produced in the same plant as the Lincoln rods. They were cheap too...$36 for a 10 lb can. The web site has them for $46. I wonder if it was a grand opening sale or something specific to the store I was in? In any case if you need to pick up a can of sealed 7018 rods on a Sunday, TSC ought to be able to help you out now.

    Name:  welding rods.jpg
Views: 1139
Size:  17.5 KB

  2. #2
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,819
    Post Thanks / Like

    Re: New rods at Tractor Supply

    That's perfect, I wonder if my local L&M Fleet store will start carrying them too.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  3. #3
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,287
    Post Thanks / Like

    Re: New rods at Tractor Supply

    So they are a bit different than the Excalibur rods. The flux coating is noticeably thinner on the Hobart rods. They don't seem to need as much heat to run (they seem to run hot) as Excalibur and the flux is pretty standard Hobart flux. It is not going to peel off. But they weld nice. I like them.

  4. #4
    Join Date
    Jul 2014
    Posts
    1,953
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I love Excalibur rods When I was welding cap pass on pipe guys used to come over and watch the flux peal off as I went up hill around the pipe ,but I used to put it in hot.

  5. #5
    Join Date
    Mar 2018
    Location
    Lititz, PA
    Posts
    119
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I noticed these the other day too, can't wait to give them a try once my short hood is up and running.

  6. #6
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,336
    Post Thanks / Like

    Re: New rods at Tractor Supply

    Iíll have to give those a try.
    I was disappointed to see that
    the 25 lb.boxes of 1/8 6011 and 6013
    at Tractor Supply have gone up
    to something like $58.
    At $50,they were the deal of the day.
    Iíve been using them for almost
    everything.


    Sent from my iPhone using Tapatalk
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  7. #7
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,064
    Post Thanks / Like

    Re: New rods at Tractor Supply

    Search the web for McKay 7018 XLM. Lots of good feedback on welding forums. A lot of folks do not like the Excaliburs.

    Other preferences include Murex MR and Hobart 418
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  8. #8
    Join Date
    Mar 2012
    Location
    Australia
    Posts
    667
    Post Thanks / Like

    Re: New rods at Tractor Supply

    Quote Originally Posted by Oldendum View Post
    Search the web for McKay 7018 XLM. Lots of good feedback on welding forums. A lot of folks do not like the Excaliburs.

    Other preferences include Murex MR and Hobart 418
    I'm one that's not a fan of excalibur's for pipe welding, they're fine for a weave cap on a vertical weld, but almost everyone wants stringers these days and excaliburs are to liquid for stringers I find.

    I much rather use lincoln conarc 49 C rods.

  9. #9
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,336
    Post Thanks / Like

    Re: New rods at Tractor Supply

    Quote Originally Posted by Oldendum View Post
    Search the web for McKay 7018 XLM. Lots of good feedback on welding forums. A lot of folks do not like the Excaliburs.

    Other preferences include Murex MR and Hobart 418
    Anyone familiar with the 25 lb. boxes of Hobart 7018 at Tractor Supply?
    Is it the same as the 418?
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  10. #10
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,287
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I have bought and used the 25 lb box of 7018 at TSC as well. I don't know if they are the same as Hobart 418. The slag is pretty hard to get off of those weld beads if you don't run it exactly perfect. Very thick slag. are 418s the same?

  11. #11
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,336
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I donít know that Iíve ever run 418. Some
    people seem to like it. Was wondering if
    the stuff in the 25# box was the same or
    similar. Iíve been using Excalibur for 7018.
    I donít use it often, but I like using it and it
    is pretty expensive at the lws.
    As a side note: the Lincoln 7018ac at
    Home Depot runs really well for me,
    (and is available on Sunday).


    Sent from my iPhone using Tapatalk
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  12. #12
    Join Date
    Jun 2012
    Location
    CT
    Posts
    4,287
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I have never been a fan of 7018 AC rods. Personal preference I guess. The TSC 7018 rods in the carboard box are great for learning on, practice and noncritical applications. But I do like the way the new 7018 XLM rods run. Like them a bit more than the cardboard box 7018s

  13. #13
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,336
    Post Thanks / Like

    Re: New rods at Tractor Supply

    There seems to be a lot of variables when it
    comes to welding electrode preference:
    Machine type, operator experience,work
    type as well as just personal preference.



    Sent from my iPhone using Tapatalk
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  14. #14
    Join Date
    Sep 2013
    Location
    west texas
    Posts
    2,372
    Post Thanks / Like

    Re: New rods at Tractor Supply

    I think 7018AC running AC is really only good for 1G, 1F maybe 2G.
    old Miller spectrum 625
    Lincoln SP-135 T, CO2+0.025 wire
    Miller model 250 and WP-18V torch
    Craftsman 100amp AC/DC and WP-17V torch
    Century 115-004 HF arc stabilizer
    Home made 4 transformer spot welder
    Home made alternator welder

  15. #15
    Join Date
    Mar 2014
    Location
    NH
    Posts
    663
    Post Thanks / Like

    Re: New rods at Tractor Supply

    The past couple of years when Zoro has their end of year 25% off I stock up on Excalibur at slightly over $2/lb. and they are the best 7018 I've run. The guy that does my mechanical work has been a fan of Murex lately, I might try them.
    Thunderbolt AC/DC
    330AB/P + Bernard cooler
    Syncrowave 250
    Oxy/Ace torch
    Dayton 160 MIG
    6CF pot with 185 compressor
    Too much big equipment
    Even more small tools

  16. #16
    Join Date
    Feb 2011
    Posts
    179
    Post Thanks / Like

    Re: New rods at Tractor Supply

    My local Tsc has been selling those for 2+ years. I tried them when I first saw them then and really like them. I usually buy excaliburs for structural work but these work just as good for me. I’ve run them off a ranger 305g, big 20, bobcat 225, and a trailblazer 302. They work well with all these machines. The slag also peels just like the excaliburs. I’ve never ran them on pipe.

  17. #17
    Join Date
    Dec 2015
    Location
    Western New York State, USA
    Posts
    2,002
    Post Thanks / Like

    Re: New rods at Tractor Supply

    i remember decades ago my old company used to buy Airco welding rod by the pallet maybe 2000 to 3000 lbs on a pallet.
    .
    once we got rod when you struck a arc the flux would fall off half the rod length. had dozens of welders using hundreds of lbs getting same problem. so they sent the unopened welding rod back and complained about it. obviously they had a manufacturing problem and were not doing 100% inspection.
    .
    just saying normally it was very very good welding rod. but that dont mean its always very good welding rod.
    .
    as for price its obviously cheaper by the pallet or ton. you can pay 30 to 100% more buying in small quantities.

  18. #18
    Join Date
    Nov 2009
    Location
    Hellinois
    Posts
    5,793
    Post Thanks / Like

    Re: New rods at Tractor Supply

    Quote Originally Posted by Oldendum View Post
    Search the web for McKay 7018 XLM. Lots of good feedback on welding forums. A lot of folks do not like the Excaliburs.

    Other preferences include Murex MR and Hobart 418

    I used to love McKay electrodes. I believe ITW bought them with Hobart and Miller.......anyway, they got rid of McKay and merged it with Hobart. McKay had 7018 that was called "7018XLM". This is why Hobart called it that. I have not used it since it's been taken over by Hobart, but it was my favorite rod.



    Quote Originally Posted by Louie1961 View Post
    I have bought and used the 25 lb box of 7018 at TSC as well. I don't know if they are the same as Hobart 418. The slag is pretty hard to get off of those weld beads if you don't run it exactly perfect. Very thick slag. are 418s the same?

    I had some 418 in Plastic packs, and yes the slag was very thick and hard to remove. That aside, they ran nice. A guy that used to frequent this site always raved about the 418's. I don't know if they're different in the tin than cardboard or plastic.
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,496,614.71949 seconds with 14 queries