    Looking for a quality electrode holder that doesnt come off the lead

    I have been having trouble with my electrode holder coming off of the lead, but the electrode holder I bought to replace it because of this problem is worse about it. what electrode holders and leads do you guys use, and how do you connect them so that they don't come apart?

  2. #2
    Join Date
    May 2010
    Location
    ct.
    Posts
    1,353
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    That’s an unusual problem.
    Is the welding lead too small for the clamp?
    A pic of welder,cables,electrode holder might
    be helpful (and/or interesting).
    400 amp Bernard short stub and
    tong type holder that came with Thunderbolt
    work fine for me on both#4 and #2 cable.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A
    Hobart Champion Elite

  3. #3
    Join Date
    Dec 2018
    Posts
    5,251
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Another thing that pulls cable out of the handle..…………...pulling your leads around by the stinger. Tempting when you're in a hurry, but will work the cable loose over time.

  4. #4
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    3,994
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead


  5. #5
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,544
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Quote Originally Posted by farmersammm View Post
    Another thing that pulls cable out of the handle..…………...pulling your leads around by the stinger. Tempting when you're in a hurry, but will work the cable loose over time.
    I’m glad you posted that. It’s such a common sense thing I wouldn’t have even thought to mention it.

    Too often we assume a faulty product is the cause of our carelessness.


    Sent from my iPad using Tapatalk
    :

  6. #6
    Join Date
    Dec 2008
    Location
    Lockhart,Tx (BBQ capitol of the world)
    Posts
    1,163
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Part of the problem is the set screw doesn't grab all of the strands of the cable.
    I like to cut a piece of copper tubing that just BARELY fits over the cable strands then tighten the whole assembly under the set screw.
    I also agree with what Farmersamm said. When you need to move hold the stinger in one hand and grab the cable with the other!

  7. #7
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    11,394
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Quote Originally Posted by rexcormack View Post
    Part of the problem is the set screw doesn't grab all of the strands of the cable.
    I like to cut a piece of copper tubing that just BARELY fits over the cable strands then tighten the whole assembly under the set screw.
    I also agree with what Farmersamm said. When you need to move hold the stinger in one hand and grab the cable with the other!
    well you just found your problem, most if not all electrode holders come with that copper piece you want to make, maybe it fell out of the bag when you opened it up, but that is your answer...

  8. #8
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    1,376
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    yeah you need that copper piece. even a bit of steel will do.

  9. #9
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Quote Originally Posted by rexcormack View Post
    Part of the problem is the set screw doesn't grab all of the strands of the cable.
    I like to cut a piece of copper tubing that just BARELY fits over the cable strands then tighten the whole assembly under the set screw.
    I also agree with what Farmersamm said. When you need to move hold the stinger in one hand and grab the cable with the other!
    this! the duro type holder use to come with a piece of curved copper for fitting between set screw and stripped cable. now i just use a piece of plumber's copper tube. i worked with someone that silver soldered the cable into the holder socket but to me that's kind of drastic.
    Last edited by docwelder; 01-27-2019 at 04:15 PM.
    i.u.o.e. # 15
    queens, ny and sunny fla

  10. #10
    Join Date
    Mar 2009
    Posts
    3,553
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    I like to put a little dielectric grease on the allen screw and give it a good bull hunchin’.
    "You can't out puke a buzzard"

  11. #11
    Join Date
    Aug 2012
    Location
    AR
    Posts
    1,980
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    I use a piece of copper tubing and one of those swage tools to seat the cable in it, then the set screw fits really tight and the swaged end won't come loose as easy.

  12. #12
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,544
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    I make my own crimped fittings to add a little strain relief to my ground clamp connections. Sort of the same scenario as electrode holders.




    They’re not idiot proof, but then again I never drag cables around by pulling on the clamps or rod holders.


    Sent from my iPad using Tapatalk
    :

  13. #13
    Join Date
    Apr 2012
    Location
    socal
    Posts
    546
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    I cut a longish strip of copper flashing (from a rich folk house!), clean it, & wrap it around the strands two times or so.
    Much more flexable than copper (plumbing) tube.
    Works for me.
    What is the sound of one knee jerking?

  14. #14
    Join Date
    Nov 2012
    Posts
    3,039
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    If your cable is small, you can always fold it over before you put it in the holder.

  15. #15
    Join Date
    Dec 2008
    Location
    Lockhart,Tx (BBQ capitol of the world)
    Posts
    1,163
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Quote Originally Posted by Hobbytime View Post
    well you just found your problem, most if not all electrode holders come with that copper piece you want to make, maybe it fell out of the bag when you opened it up, but that is your answer...
    It was in the new stinger but was very thin and flimsy!
    Copper tubing worked much better.
    Been doing that for years.

  16. #16
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    3,994
    Post Thanks / Like

    Re: Looking for a quality electrode holder that doesnt come off the lead

    Dunno. When I arc or tig the lead is wrapped once around my forearm. The grounds give me fits sometimes.

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,733,646.45845 seconds with 13 queries