    Has anyone tried running self shielding wires like NR-211 with shielding gas, and if so, what were the results?
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  2. #2
    Join Date
    Jan 2004
    Location
    Northern Cal., Shasta County
    Posts
    9,327
    Post Thanks / Like

    Re: Flux core self shielding wire

    Lincoln is very specific in stating to 'not' use any shielding gas with self shielded flux core so I just never got around to trying to use it.
    "The things that will destroy America are prosperity at any price, peace at any price, safety first instead of duty first, the love of soft living and the get rich quick theory of life." -Theodore Roosevelt

  3. #3
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,837
    Post Thanks / Like

    Re: Flux core self shielding wire

    I think I'm gonna try it, I think I have a roll of Forney .030 in right now I'll give it a try on both polarities with the C25. I had been wondering about and was just hoping someone had tried it.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  4. #4
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    1,343
    Post Thanks / Like

    Re: Flux core self shielding wire

    I tried NR211 with argoshield light, just out of interest, and it welded just like solid wire without gas - i.e. fizzing and popping and loads of porosity. Terrible idea

  5. #5
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,461
    Post Thanks / Like

    Re: Flux core self shielding wire

    The result is going to be an unnecessary increase in your welding cost. If you want to weld with gas shielded flux cor wire, buy some.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  6. #6
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,837
    Post Thanks / Like

    Re: Flux core self shielding wire

    I'm just curious as to how or if it would work, I'm happy with mig, flux or stick, you know what they say a bout curiosity & the cat!
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  7. #7
    Join Date
    Apr 2012
    Location
    NW OR
    Posts
    132
    Post Thanks / Like

    Re: Flux core self shielding wire

    Innershield wire needs atmospheric elements for proper flux reaction. NR211 flux reacts with the oxidizing elements in the air to create correct alloying. Trying to use shielding gas with fluxcore defeats the flux in the wire. Absolute waste of time.

    EDIT: https://www.lincolnelectric.com/en-u...lectrodes.aspx

  8. #8
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Flux core self shielding wire

    for me the whole point of running innershield wire was the elimination of shielding gas. i guess it wouldn't hurt anything to try it out on some non load bearing scrap to satisfy your curiosity. afterward give it the sledge-o-matic test and report back.
    i.u.o.e. # 15
    queens, ny and sunny fla

  9. #9
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,837
    Post Thanks / Like

    Re: Flux core self shielding wire

    It would definitely be on something non-critical, probably more on the line of padding some beads on some scrap, & I won't go to much effort to try it, I've got some .030 Forney in the machine right now so it's just a matter of turning on the bottle, and trying the wire on each polarity which is swapping a dinse connector from one side of the machine to the other.
    Last edited by CAVEMANN; 03-14-2019 at 07:30 PM.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  10. #10
    Join Date
    May 2017
    Location
    Pitman PA
    Posts
    763
    Post Thanks / Like

    Re: Flux core self shielding wire

    Quote Originally Posted by CAVEMANN View Post
    It would definitely be on something non-critical, probably more on the line of padding some beads on some scrap, & I won't go to much effort to try it, I've got some .030 Forney in the machine right now so it's just a matter of turning on the bottle, and trying the wire on each polarity which is swapping a dinse connector from one side of the machine to the other.

    Just to satisfy your own curiosity go ahead and give it a whirl, noones gonna get hurt if you try it like that so why not? I don't think its gonna work but what the hell. I use NR 233 all the time and never had any desire to mess with what works even though I could if I wanted too. Im curious myself to see what you come up with though. Have fun you old mad welding scientist

  11. #11
    Join Date
    Dec 2018
    Location
    Southern California
    Posts
    801
    Post Thanks / Like

    Re: Flux core self shielding wire

    Curious to see what will happen too. I once thought about running just low pressurized atmospheric air through a gun once with gasless flux core, to cool the gun so I wouldn't have to stop as much as i was laying looooooooooong fillet beads in the hot california sun on shiny metal bins (one of THOSE days) with a low duty cycle gun.

  12. #12
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,819
    Post Thanks / Like

    Re: Flux core self shielding wire

    Not sure why anyone would want to "try it" when the results are already known - as posted by the wire manufacturers.

    In my opinion, the worst result you could get would be to have it seem to weld "fine" thus encouraging you to further ignore the manufacturer published information

    Name:  Screenshot_2019-03-14-21-32-37.jpg
Views: 303
Size:  135.1 KB
    Last edited by MinnesotaDave; 03-14-2019 at 10:33 PM.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  13. #13
    Join Date
    Dec 2018
    Location
    Southern California
    Posts
    801
    Post Thanks / Like

    Re: Flux core self shielding wire

    Good info MinnesotaDave. What if he was curious to see what kind of bead profile/look it would leave for artistic purposes? Be careful not to dismiss curiosities too quickly, sometimes they work put pretty well, even if completely without logical merit. That's my excuse for putting liquid paper on a bumble bee, anyway. (silly movie reference)

  14. #14
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,819
    Post Thanks / Like

    Re: Flux core self shielding wire

    Quote Originally Posted by SlowBlues View Post
    Good info MinnesotaDave. What if he was curious to see what kind of bead profile/look it would leave for artistic purposes? Be careful not to dismiss curiosities too quickly, sometimes they work put pretty well, even if completely without logical merit. That's my excuse for putting liquid paper on a bumble bee, anyway. (silly movie reference)
    Yeah, I don't play "what if." When people ask questions about artistic look and feel I'm happy to talk about that stuff
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  15. #15
    Join Date
    May 2017
    Location
    Pitman PA
    Posts
    763
    Post Thanks / Like

    Re: Flux core self shielding wire

    Thanks Dave for that info, I always wondered myself and a young fella asked me the same thing a few weeks ago, and I told him the same thing I said earlier...why mess with whats been workin for years?...and now we know

  16. #16
    Join Date
    Jul 2013
    Location
    North Carolina
    Posts
    296
    Post Thanks / Like

    Re: Flux core self shielding wire

    Curiosity got the best of me one day and I used a 75/25 shielding on with .068 NR-211 innershield just to see what would happen. The process resulted in a beautiful weld. However, the weld did have some small cracks if you turned the heat up.
    Lincoln Electric:
    Ranger GXT 250
    SA-200
    LN-25
    Pro MiG 256
    Pro Mig 180
    Esab CV 251
    Invertec 160
    Victor Torches”

  17. #17
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,837
    Post Thanks / Like

    Re: Flux core self shielding wire

    Well, I haven't tried it yet, got too many irons in the fire, it will happen tho, it has to, My parents were from Missouri, so I gotta have some of that "SHOWME " in there somewhere, I'll try to remember to post it up when I git-r-done. Right now I gotta get a bathroom floor fixed and finish running a dog fence.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,504,690.32395 seconds with 14 queries