    Dual shield settings

    I should take a picture of the chart in my Millermatic 252. Where they give recommended settings for dual shield they are markedly different from those I see in demonstrations.

    Typically, internet demos are using 1.5 to 2 volts higher, and wire speeds 100 or more IPM slower than recommended in my welder. Have I missed something?

    When the stars are aligned, I hear a hissing sound, and the wire seems to lose its outer shell leaving only the flux core visible. Settings seem a mystery.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  2. #2
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Dual shield settings

    Quote Originally Posted by Willie B View Post
    I should take a picture of the chart in my Millermatic 252. Where they give recommended settings for dual shield they are markedly different from those I see in demonstrations.

    Typically, internet demos are using 1.5 to 2 volts higher, and wire speeds 100 or more IPM slower than recommended in my welder. Have I missed something?

    When the stars are aligned, I hear a hissing sound, and the wire seems to lose its outer shell leaving only the flux core visible. Settings seem a mystery.
    I usually crank it up hot around 75/25 settings and fine tune from there off the door chart. Takes a bit of twiddling to get it figured out.
    The "hiss" is what I want to hear.

  3. #3
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Dual shield settings

    I think you're doing what any decent welder would do...….you're setting the machine to where it runs right for you. The stuff on the door is only a ballpark "suggestion".

  4. #4
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Dual shield settings

    Lincoln’s settings for tig welding 1/8” joint says I should be at about 125 amps when really I was using 210 amps and it worked just fine

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,255,023.34332 seconds with 20 queries