    Millermatic 200, GA-20c gun update

    Bought a MM 200 and the GA- 20C gun is beat up. The nozzle and the defuser and insulator need replacing. Profax has defuser, nozzle and tips. The insulator is harder to get. The Profax catalog list the thread sizes for these parts.
    Put a miller Roughneck gun on the MM200, the Miller defused is 1/4" NPT thread. Thought how hard can it be to convert the GA-20C to accept miller Rough neck parts.
    The GA-20C has 7/16-14 female thread.
    Got a 3/8" barb x 1/4" NPT fitting( Milton). On the 3/8" barb side ran a 7/16-14 die to make threads. Then cut fitting to length.
    Now can attach Miller Roughneck parts.
    Bernard center fire parts are 1/4" NPT and Miller M25 are 1/4" NPT . Some of the Tregaskiss are 1/4" NPT.
    Name:  20190627_223439.jpg
Views: 812
Size:  64.8 KBr

  2. #2
    Join Date
    Jul 2012
    Posts
    875
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Name:  20190627_223739.jpg
Views: 749
Size:  79.5 KB

  3. #3
    Join Date
    Jul 2012
    Posts
    875
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Name:  20190627_223838.jpg
Views: 745
Size:  83.9 KB
    Going put heat shrink tube to cover gooseneck.
    Need to find a liner for this GA-20C gun.
    Miller Spoolmatic 15 and 30 A use the same parts as the Roughneck gun.

  4. #4
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Quote Originally Posted by guajilloweld03 View Post
    Name:  20190627_223838.jpg
Views: 745
Size:  83.9 KB
    Going put heat shrink tube to cover gooseneck.
    Need to find a liner for this GA-20C gun.
    Miller Spoolmatic 15 and 30 A use the same parts as the Roughneck gun.
    You will find that liners are very expensive for the GA-20C gun. The cost of liners and the fact that new switches for the GA -20 are not sold anymore is the reason I finally switched guns on my MM200. I still have the GA-20 hoping I might find a switch . I did find one on ebay once but they wanted $69 for it. I replaced the liner in mine and a few days latter the switch went bad. Good luck but I feel your putting money in a dead horse.

  5. #5
    Join Date
    Jul 2012
    Posts
    875
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Your right about putting money on a dead horse. Already had the parts from my other guns. It was fun getting it together and simple getting it to work. The liner looks like a miller # 194010 ($ 11.00) can be bought on EBay and made to work. The old liner has a bushing with a set screw, so cut new liner and fit it on. Think I have a spare liner some where, will have to look.

  6. #6
    Join Date
    Jul 2012
    Posts
    875
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Found two miller 081957 switches on EBay and a article on how to rebuild these leaf switches.

    https://www.ebay.com/itm/Miller-Elec...t/303110378353
    https://pinside.com/pinball/forum/to...-leaf-switches

    Name:  20190704_135547.jpg
Views: 651
Size:  115.8 KB

    Put 1/2" hose on neck.
    Last edited by guajilloweld03; 07-05-2019 at 07:38 AM.

  7. #7
    Join Date
    Mar 2022
    Posts
    8
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Thanks for the info. My main problem is on the power point end. I can't find any pin that fits. I'm going to have to try to fab one. Thanks again

  8. #8
    Join Date
    Jul 2012
    Posts
    875
    Post Thanks / Like

    Re: Millermatic 200, GA-20c gun update

    Quote Originally Posted by turkeyjoe View Post
    Thanks for the info. My main problem is on the power point end. I can't find any pin that fits. I'm going to have to try to fab one. Thanks again
    So you are talking about the two wires that go to the trigger.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,665,018,444.55254 seconds with 14 queries