    I would take the Eastwood machine with you so you learn on your machine.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  2. #27
    Join Date
    Jul 2019
    Posts
    9
    Post Thanks / Like

    Re: TIG welder recommendation for 0.025" 6061 aluminum? Eastwood TIG 200 AC/DC?

    I'm super excited about welding again: I had today my 1.5 hour training session with the welding instructor!
    While my welds are certainly far from perfect, I am already pretty happy with the results and feel that further improvement is mainly a question of additional practice.

    First we ran beads on 0.125" 6061-T6. The red arrow is pointing at by last bead:
    Name:  fullsizeoutput_8e7.jpg
Views: 129
Size:  110.3 KB

    Once we were done with the beads, I also gave an inside corner joint a try, same material:
    Name:  jpuHv6rqTpyoBleND4ugRg.jpg
Views: 130
Size:  74.1 KB

    I'm fairly optimistic that I will be able to achieve similar results with my Eastwood welder, I'll practice with it this weekend!
    I feel that I should have started with 0.125" material in the first place, instead of the much thinner 6061-T6 I actually used.

    Oliver
    Last edited by OliverR; 08-01-2019 at 12:34 AM. Reason: Typos

  3. #28
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,907
    Post Thanks / Like

    Re: TIG welder recommendation for 0.025" 6061 aluminum? Eastwood TIG 200 AC/DC?

    Not that far off. It needs more amps tho

  4. #29
    Join Date
    Jul 2019
    Posts
    9
    Post Thanks / Like

    Re: TIG welder recommendation for 0.025" 6061 aluminum? Eastwood TIG 200 AC/DC?

    Quote Originally Posted by motolife313 View Post
    Not that far off. It needs more amps tho
    I was also thinking that a higher ac balance for better cleaning action might not hurt.
    Anyways, I'm pretty stoked since these are finally my first successful welds on aluminum. Can't wait to practice more!

    Oliver

  5. #30
    Join Date
    Oct 2007
    Posts
    174
    Post Thanks / Like

    Re: TIG welder recommendation for 0.025" 6061 aluminum? Eastwood TIG 200 AC/DC?

    I weld this type of stuff of this thickness with my Lincoln 175 square wave. It doesn’t have any bells or whistles. Mostly for racers who are trying save the last ounce.
    I turn the power way down almost to 0. On some edges like your edge weld I clamp a strip of copper along it and move as required. I let the copper stick out the start end about half an inch. I light the torch off on this to get rid of the slightly higher start current. Then move on to the weld. I use the pedal for more of less current? At this level you need really good hand support. Even a slight movement out of line and the weld fails or looks terrible. This is a tricky weld on a good day.
    I use both 5356 and 4043. 5356 would be my choice first. The hard...expensive part is getting rod or wire. Most of the time I just use MiG wire I think we still have some .023 and .030. You should experiment with .o35 too. You can’t even read the size on the rods. It’s a bit tricky to get this small MiG wire straight. I use bent brake line to straighten it. Then cut it into about 18” pieces. The fillet weld looks easier but you can burn a hole in it so easy. Just a wiggle the wrong way and.....scrapo

    I stopped building these thin wall tanks for the racers years ago. The small amount of weight saved wasn’t worth the loss of round money of the race money. Some tanks now are .090. They are bullet proof. Rarely if ever crack and can withstand rough handling.

    I also repair model airplane mufflers out of this thin stuff. The problem is that where it is formed the metal is stretched even thinner. Then it’s hard to clean both sides. It’s very tough to weld these. Usually not cost effective for me or customer. The same goes for the stainless steel ones even more so.

  6. #31
    Join Date
    Jul 2019
    Posts
    9
    Post Thanks / Like

    Re: TIG welder recommendation for 0.025" 6061 aluminum? Eastwood TIG 200 AC/DC?

    @bentwings: Very interesting. Thank you for the detailed description!

    Oliver

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,430,357.27182 seconds with 12 queries