    We have an old Esab 350 mpi that is not throwing any trouble codes and will not strike an arc with either MIG or SMAW. I've come to the conclusion that it is something internal. A board maybe? Any help is appreciated.

    Thanks!

  2. #2
    Join Date
    Aug 2020
    Location
    Blumenort, MB
    Posts
    6
    Post Thanks / Like

    Re: Esab 350 mpi

    I had a 450 that I bought a feeder for and it would only arc and then stop. After reading the book I found there was a setting for spot weld time and it was set for .1 second. I removed that setting and everything worked just fine. The 350 doesn't have that setting inside but the feeder might.

  3. #3
    Join Date
    Jun 2010
    Posts
    8
    Post Thanks / Like

    Re: Esab 350 mpi

    The manual has a troubleshooting guide. Doesn't have a ton of answers but should provide more information to narrow down the cause - page 27

    https://www.esabna.com/literature/ar...e_15-481-k.pdf
    Last edited by marcb; 08-23-2020 at 08:25 AM. Reason: fixed link

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,059,601.37662 seconds with 11 queries