    I did this for a friend after work in a few hours. They use them at weddings or events. It is aluminum, 3/4" pipe. I rolled it with a manual Harbor Freight pipe roller. I then welded it to some cut-offs of a large U-channel. It came out great. The trick is rolling a half-turn of the wheel and then straightening the pipe in the roller. It tends to walk one way or the other.

    The ring splits between the angles so you can screw it through tight openings. There is a butt pipe welded at one end of the pipe. Try not to get too excited about "butt pipe", haha I miss you guys been crazy busy.

    Name:  IMG_6839.jpg
Views: 447
Size:  171.8 KBName:  IMG_6819.jpg
Views: 447
Size:  177.0 KB

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  2. #2
    Join Date
    Nov 2012
    Location
    new york city
    Posts
    6,918
    Post Thanks / Like

    Re: Wedding Or Event Ring

    looks safer than jumping the broom.
    i.u.o.e. # 15
    queens, ny and sunny fla

  3. #3
    Join Date
    Sep 2014
    Posts
    1,742
    Post Thanks / Like

    Re: Wedding Or Event Ring

    After I welded in the butt pipe, I rolled it again over the joint and it came out almost perfect.
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  4. #4
    Join Date
    Sep 2014
    Posts
    1,742
    Post Thanks / Like

    Re: Wedding Or Event Ring

    Quote Originally Posted by docwelder View Post
    looks safer than jumping the broom.
    Anything is safer than that today, haha.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  5. #5
    Join Date
    Sep 2014
    Posts
    1,742
    Post Thanks / Like

    Re: Wedding Or Event Ring

    The next day I sanded it down and then painted it. A lot of work for a hoop but it does look nice.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  6. #6
    Join Date
    Jul 2011
    Location
    Bossier Parish La.
    Posts
    5,824
    Post Thanks / Like

    Re: Wedding Or Event Ring

    When I read the title, I was thinking something to wear on the finger. Then I put my cursor over the title to read the first few lines and wondered why you needed a pipe bender for this. So I opened the thread to see what it was about & it became more apparent. One thing that came to mind to really set one off is to have it with a series of tiny holes drilled around the outside perimeter(or inside) and run LP gas through it to have small jets of flame shooting out of them. Obviously ONLY for outdoor use, but that would be an even more unique twist on something like this. It also put me in mind of the old Johnny Cash song, Burning Ring of Fire. That might be something good to play at one of these event with one of them burning.



    How does that idea sound, pretty HOT, HUH?

  7. #7
    Join Date
    Sep 2014
    Posts
    1,742
    Post Thanks / Like

    Re: Wedding Or Event Ring

    Quote Originally Posted by Bistineau View Post
    When I read the title, I was thinking something to wear on the finger. Then I put my cursor over the title to read the first few lines and wondered why you needed a pipe bender for this. So I opened the thread to see what it was about & it became more apparent. One thing that came to mind to really set one off is to have it with a series of tiny holes drilled around the outside perimeter(or inside) and run LP gas through it to have small jets of flame shooting out of them. Obviously ONLY for outdoor use, but that would be an even more unique twist on something like this. It also put me in mind of the old Johnny Cash song, Burning Ring of Fire. That might be something good to play at one of these event with one of them burning.




    How does that idea sound, pretty HOT, HUH?
    I do love fire and explosives, haha.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  8. #8
    Join Date
    Dec 2018
    Posts
    5,229
    Post Thanks / Like

    Re: Wedding Or Event Ring

    Bill, next thing ya gonna be into is bird bowers

    https://video.nationalgeographic.com...c-7b3d40110000

    Yer goin' down the slippery slope, and ya ain't wearin' sneakers

  9. #9
    Join Date
    Sep 2014
    Posts
    1,742
    Post Thanks / Like

    Re: Wedding Or Event Ring

    Quote Originally Posted by farmersammm View Post
    Bill, next thing ya gonna be into is bird bowers

    https://video.nationalgeographic.com...c-7b3d40110000

    Yer goin' down the slippery slope, and ya ain't wearin' sneakers
    Haha, that is crazy.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,398,009.94236 seconds with 12 queries