Howdy mates,
This is on request, N2 spotted another project I fumbled together in the background of another thread.
A personal interpretation of the R2D2 droid (lotsa droids in that universe)
This is what I fumbled together,
Everything was cleaned, cut and pre-fit outdoors at the wonderful pitchblack stonecold winter. Borrowed my pears garage to weld it together. (Additional grinding back to outside)
Wanted some cool textures so decided to reshape a rim.
Split it, turned the halfs the same way to achieve a roundish shape.
Crappyweldingdude strikes again
Smacked it on R2's *** (Even Bender would envy this shiny *** dont you think?)
to be cont'd