Re: John Deere 4410 Draft Arm Break
It definitely wasnt grooved out enough to get good penatration. If I did that repair I would have tacked it together, gouged almost halfway thru on one side , then welded. Then I would gouge down to the weld from the other side and welded it. Not sure but I imagine that T-1 steel would be used in that application , so a 80-90,000 tensile electrode with some preheat should have been used .