    Hypertherm Powermax 45 Dross

    I get a lot of dross when I cut. I have my air adjusted correctly. any suggestions

  2. #2
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,250
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Quote Originally Posted by txrpls View Post
    I get a lot of dross when I cut. I have my air adjusted correctly. any suggestions
    what size material are you cutting?
    How are your consumables?

    usually I've found excessive dross is from moving too slow.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  3. #3
    Join Date
    Apr 2016
    Location
    CA
    Posts
    8,103
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Yes lots of dross usually moving to slow.
    Lincoln, ESAB, Thermal Dynamics, Victor, Miller, Dewalt, Makita, Kalamzoo. Hand tools, power tools, welding and cutting tools.

  4. #4
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    65
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Quote Originally Posted by John T View Post
    what size material are you cutting?
    How are your consumables?

    usually I've found excessive dross is from moving too slow.
    I just changed them out and will see if that makes a difference. I'm cutting 1/4" thick pipe 1.5' in diameter.

  5. #5
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    65
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Ok, so I changed out the consumables and that made a difference. I want to cut slow as this is a weird irregular cut. How do you cut slow with this machine?

  6. #6
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    65
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Well, I figured it out, just cut slow and knocked of the dross with a chipping hammer.

  7. #7
    Join Date
    Apr 2008
    Location
    NW ON Canada
    Posts
    3,461
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Itís a combination of cut amps and travel speed. Get the combination correct and you get relatively clean cuts.
    Jason
    Lincoln Idealarc 250 stick/tig
    Thermal Dynamics Cutmaster 52
    Miller Bobcat 250
    Torchmate CNC table
    Thermal Arc Hefty 2
    Ironworkers Local 720

  8. #8
    Join Date
    Jun 2016
    Location
    Back to the jungle
    Posts
    3,994
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    One setting. WFO and pull accordingly. See the spray angle ? Too slow is straight down
    Name:  plasmalaser02.jpg
Views: 484
Size:  152.4 KB

    Name:  plasmalase01.jpg
Views: 499
Size:  154.1 KB

    Name:  plasmalaser.jpg
Views: 493
Size:  97.7 KB
    Last edited by Bonzoo; 12-16-2019 at 10:51 AM.

  9. #9
    Join Date
    Oct 2007
    Location
    New Hampshire, North Carolina
    Posts
    3,337
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Dross is caused by: 1. Cutting too slow, 2. Cutting with torch too high off material. If the part is detailed and you need to move slow.....turn the amperage knob down unil you are comfortable (that is what the Amp setting is there for). With experience, just like with welding processes, you will find a sweet spot that works for you. You will find that low speed dross is very easy to knock of with chisel (buy a concrete chisel at the local hardware). Finding the ideal speed by machine cutting is easy, by hand it is hard to find the sweet spot between low speed dross and high speed dross. If the height is right (correct height with shielded hand cutting parts on a Hypertherm is dragging) and the speed is right, and the retaining cap is perpendicular to the material....you will see the sparks (that exit the bottom) actually lead the torch by about 10-15 degrees when using an air plasma on steel (on stainless and aluminum the sparks should trail by 15 to 30 degrees). The manual has some good info on cutting technique.....check it out! Jim Colt

  10. #10
    Join Date
    Sep 2013
    Location
    Near San Antonio, Texas
    Posts
    65
    Post Thanks / Like

    Re: Hypertherm Powermax 45 Dross

    Thanks, Jim. I finally got it figured out.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,351,529.10722 seconds with 12 queries