Results 1 to 8 of 8

Thread: stainless structural welding

  1. #1
    Join Date
    Dec 2019
    Posts
    2
    Post Thanks / Like

    stainless structural welding

    hi, i'm looking to see if anyone knows of any types of stainless wire that is structurally rated for welding T304 ss you regular mild steel. any ideas? i haven't been able to find anything.

  2. #2
    Join Date
    Nov 2012
    Posts
    3,039
    Post Thanks / Like

    Re: stainless structural welding

    Stainless to carbon takes 309 wire.

  3. #3
    Join Date
    Dec 2019
    Posts
    2
    Post Thanks / Like

    Re: stainless structural welding

    but i don't think that's structurally rated though, is it?

  4. #4
    Join Date
    Nov 2012
    Posts
    3,039
    Post Thanks / Like

    Re: stainless structural welding

    They use it on high pressure pipe, why couldn't you use it on structural? What does that even mean, 'structurally rated'?


    https://www.lincolnelectric.com/en-u...al-detail.aspx

  5. #5
    Join Date
    Jun 2016
    Location
    SE Saskatchewan, Canada
    Posts
    360
    Post Thanks / Like

    Re: stainless structural welding

    Quote Originally Posted by hunter111222 View Post
    but i don't think that's structurally rated though, is it?
    As long as it meets the requirements of the code you are working to.

    Our shop has a welding procedure for carbon steel to 304 using 309L wire. The procedure for 304 to 304 uses 308 filler wire. Here in at our shop (in Canada) we work to CSA W47.1 & W59.1 which is very similar to AWS D1.1.
    Red Seal Journeyman Welder (2003), Red Seal Journeyman Metal Fabricator (2018), Welding Engineering Technologist (2005)
    Pressure - ASME Section IX
    Structural - CSA W47.1, CSA W47.2
    Transport tanker - CSA B620
    Aerospace - AWS D17.1

  6. #6
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,141
    Post Thanks / Like

    Re: stainless structural welding

    Quote Originally Posted by TimmyTIG View Post
    Stainless to carbon takes 309 wire.
    Or ER312.

    ER312 has a high ferrite level like ER309 but is much more versatile for other applications. I gave up using 309 years ago because of cracking problems. As told by Lincoln electric ER312(the base for Harris SUPERMISSILEWELD), is a formula suited to weld steel to steel, steel to stainless steels, and stainless steels of unknown composition. ER312 is a staple in the maintenance weldor's tool box.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  7. #7
    Join Date
    Jan 2012
    Posts
    217
    Post Thanks / Like

    Re: stainless structural welding

    312 is not listed as a prequalified filler metal in AWS D1.6 . Use 309 unless the carbon content of the steel is greater than 0.3%, then use 312.
    Last edited by ironrail; 12-18-2019 at 12:07 AM.

  8. #8
    Join Date
    Jul 2008
    Posts
    3,312
    Post Thanks / Like

    Re: stainless structural welding

    Quote Originally Posted by ironrail View Post
    312 is not listed as a prequalified filler metal in AWS D1.6 .
    What about 310?

Tags for this Thread

Posting Permissions