    checking homemade tig torch cooler for leaks

    Temporarily bolted components to plywood to make sure everything works as planned. Ran beads continuously on 1/4" aluminum plates for 20 minutes, only stopping to grab more filler. Flow looked good inside tank (about .25 gpm ). Tank has about 2 gallons of tig coolant in it. Temperature wasn't noticeably Higher. I really like the #20 torch much better than the #26 it replaced.Name:  IMG_0588.jpg
Views: 464
Size:  62.9 KB
    Name:  IMG_0584.jpg
Views: 488
Size:  92.7 KB
    Name:  IMG_0588.jpg
Views: 464
Size:  62.9 KBName:  IMG_0592.jpg
Views: 412
Size:  54.7 KB

    Went to hang torch up, and found the leak.
    Name:  IMG_0604.jpg
Views: 395
Size:  90.4 KB

    lost a little glycol

    Name:  IMG_0612.jpg
Views: 417
Size:  37.1 KB

    I must have loosened the retaining nut on the coolant line when replacing the power cable . Had to replace the power cable after I tried using a small circulator pump in a 5 gal bucket of water. Flow wasn't sufficient, and melted cable/hose. The first power cable I replaced it with from american torch tip was very stiff, had to order an original weld-tec, much more pliable. This inspired me to make a proper cooler for my Airco(esab) Heliwelder 250 IV. Runs off the 115v outlet next to the foot pedal connector. I didn't bother putting through the solenoid, or adding a switch. When the machine is on, the cooler is always running. Put connector and hose back together, and ran for another 20 minutes continuous, no leaks this time. Now its time to get the foot pedal sorted out.



    sorry about the orientation of photos, these are from an iPhone(not my usual camera) will try to figure it out for next time.
    Last edited by albrightree; 01-05-2020 at 09:37 PM. Reason: Photos flipped
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  2. #2
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,172
    Post Thanks / Like

    Re: checking homemade tig torch cooler for leaks

    Testing rotation.
    Attached Images Attached Images  
    Last edited by albrightree; 01-05-2020 at 09:47 PM.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  3. #3
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: checking homemade tig torch cooler for leaks


    albrightree


    Quote Originally Posted by albrightree View Post
    . . . sorry about the orientation of photos . . . will try to figure
    it out for next time -
    Generally - if you shoot the photo while holding your device
    Horizontally - it will post Vertically without a due . . .



    Everything you have done 'is do it yourself' straight forward -
    My interest - is your technique/success in securing the tubes
    to the Torch couples . . .

    Quote Originally Posted by albrightree View Post
    Name:  IMG_0612.jpg
Views: 417
Size:  37.1 KB
    Great photo quality - keep us posted . . .


    Opus

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,664,631,980.19339 seconds with 14 queries