Thread: 5460 DV cooler FLOW ALARM !!

  1. #76
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,035
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Absolutely.
    Depending on what you’re welding and how hard you are running the machine...

    Most guys could probably get away with a 5 gallon bucket of water and a pro con motor and pump sitting on top.

    No fan
    No cooler/ radiator
    Just in and out.

    You would be hard-pressed to heat up A 5 gallon bucket of water to the point that it affects the torch.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  2. #77
    Join Date
    Dec 2003
    Location
    Fairfield,CT
    Posts
    1,403
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Oberdorfer....straight cut gears.
    www.tjsperformance.com
    Dynasty 300 DX
    HTP 240
    HTP Microcut 380
    Hyperthem 85
    JD2 Hyd Bender and HF Hyd Ring Roller all in one =(Frankenbender)
    Bpt. Mill/DRO
    4' x 8' CNC Plasma Table
    Instagram: tjsperformance
    YT: TJS Welding and Fabrication

  3. #78
    Join Date
    Oct 2015
    Posts
    86
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Thanks for the thoughts gentlemen. I've had my 221 now for around 5years and I love it! Not a lick of trouble out of it, but I've grown tired of cooking my hand hanging on to that torch for hours so I decided it's time to do something about it. When I see a water cooler is 250bucks on scamazon and this one is 450, I have to start asking questions. After buying a torch and by the time I toss in a bag of consumables, it's starting to get close to a grand. I believe in paying for quality, but I expect something in return. The fact it will be wired to always work is something I've considered. I'm the guy that occasionally forgets to flip on the argon, but it's a game changer when you forget to flip on the cooler. Goodbye torch with a quickness!

  4. #79
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    6,035
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    I'm sure you can take the cover off your 221 and find the power wire(s) that go to the receptacle in the back....
    maybe even find the proper plug ... then wire whatever cooler you want.... to come on with the welder.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  5. Likes jagboy69 liked this post
  6. #80
    Join Date
    Mar 2015
    Location
    usa
    Posts
    154
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by jagboy69 View Post
    it's a game changer when you forget to flip on the cooler. Goodbye torch with a quickness!
    i wouldnt go that far. ive forgot to turn on the cooler and welded for a decent amount of time and nothing was burned up. but having it turn on with the welder isnt a bad idea if your absent minded like me
    invertig 221 water cooled
    millermatic 211

  7. Likes jagboy69 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,620,873,078.62519 seconds with 12 queries