    Re: 5460 DV cooler FLOW ALARM !!

    Absolutely.
    Depending on what you’re welding and how hard you are running the machine...

    Most guys could probably get away with a 5 gallon bucket of water and a pro con motor and pump sitting on top.

    No fan
    No cooler/ radiator
    Just in and out.

    You would be hard-pressed to heat up A 5 gallon bucket of water to the point that it affects the torch.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  2. #77
    Join Date
    Dec 2003
    Location
    Fairfield,CT
    Posts
    1,554
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Oberdorfer....straight cut gears.
    www.tjsperformance.com
    Dynasty 300 DX
    HTP 240
    HTP Microcut 380
    Hyperthem 85
    JD2 Hyd Bender and HF Hyd Ring Roller all in one =(Frankenbender)
    Bpt. Mill/DRO
    4' x 8' CNC Plasma Table
    Instagram: tjsperformance
    YT: TJS Welding and Fabrication

  3. #78
    Join Date
    Oct 2015
    Posts
    91
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Thanks for the thoughts gentlemen. I've had my 221 now for around 5years and I love it! Not a lick of trouble out of it, but I've grown tired of cooking my hand hanging on to that torch for hours so I decided it's time to do something about it. When I see a water cooler is 250bucks on scamazon and this one is 450, I have to start asking questions. After buying a torch and by the time I toss in a bag of consumables, it's starting to get close to a grand. I believe in paying for quality, but I expect something in return. The fact it will be wired to always work is something I've considered. I'm the guy that occasionally forgets to flip on the argon, but it's a game changer when you forget to flip on the cooler. Goodbye torch with a quickness!

  4. #79
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    I'm sure you can take the cover off your 221 and find the power wire(s) that go to the receptacle in the back....
    maybe even find the proper plug ... then wire whatever cooler you want.... to come on with the welder.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  5. Likes jagboy69 liked this post
  6. #80
    Join Date
    Mar 2015
    Location
    usa
    Posts
    1,201
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by jagboy69 View Post
    it's a game changer when you forget to flip on the cooler. Goodbye torch with a quickness!
    i wouldnt go that far. ive forgot to turn on the cooler and welded for a decent amount of time and nothing was burned up. but having it turn on with the welder isnt a bad idea if your absent minded like me
    hypertherm powermax 30xp
    fronius transpocket 180
    fronius transsteel 2200
    fronius iwave 230i water cooled
    hobart handler 100

  7. Likes jagboy69 liked this post
  8. #81
    Join Date
    Oct 2015
    Posts
    91
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    The cooler finally arrived. I've only used it about 5mins so far and the torch is nice and cool. One thing I wasn't ready for was how loud it is. I still think it's way overpriced so I sure hope to hell I don't need it's 18month warranty. Interesting piece of info for anyone is when I bought it, the girl on the phone said it was made in Taiwan. I can absolutely confirm the box says made in CHINA. China is actually capable of making decent stuff, but it's a rarity. I think I would have been happy to part with this amount of cash if it came from Italy or Taiwan. SO yeah, I'm a little sideways to see china at this price.

    For this kind of money, I could have bought almost 3 cheapazz amazon coolers and I doubt they are any better that this thing. Time will tell! :-/

    Name:  20210510_200511.jpg
Views: 347
Size:  202.5 KB

  9. #82
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    The fan does move a lot of air, so i guess its a necessary evil.
    1st on WeldingWeb to have a scrolling sig!



  10. #83
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    2,221
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Most decent coolers are fairly loud... a decent pump and a decent fan always makes a racket. You can quieten it down if you put some acoustic insulation on the insides of the case - it worked well on my Esseti cooler which uses a Procon pump.
    The new Lorch cooler I have also uses a procon, and the fan is even louder... but it's pump on demand, which is a lovely luxury!

    Anyway, reading through this thread, I didn't see John's eventual diagnosis? He burned his torch up, and surmised that the pump was bad, given no other obvious faults.

    I'd like to see pics of the pump opened up and to see in what way it failed...
    Murphy's Golden Rule: Whoever has the gold, makes the rules.

  11. #84
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Munk
    The key on the motor shaft that drives the pump Failed/busted

    Not sure why this happened
    Perhaps it was never sized properly and there was some movement and it eventually wore out and started spinning the pump slower???

    Who knows…
    It was probably a slow process because first the flow alarm started going off
    And then not too much longer it stopped pumping water completely.
    And unfortunately when that happened I burned up my hose.

    Sorry I do not have any pictures of the internals

    I just moved on and rebuilt it with a procon.

    There is also another thread on this.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  12. Likes Munkul liked this post
  13. #85
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Sorry, i know this thread is a little bit old, but i am having issues with my arctic chill cooler.
    Machine is a invertig 221 DV and i bought both at the same time. I love the machine, and the cooler has worked fine up until recently. I have had the machine and cooler for probably like 10 years now, i always used the HTP coolant but when covid hit i got a little behind on that. I wasn't using the machine regularly for a while. I did drain, flush and replace with new HTP coolant last year and it has been working great but the other day the flow alarm came on and would not shut off. I could see the bybass was really shooting water in, but the return was not flowing very much.
    I received my new torch and hoses today, figured that would fix it but it did not.
    I did take the cooler apart, removed the flow sensor/orifice and used vinegar to clean it. No dice. Clamped off the bypass and flow increased. I ended up removing the reservoir from the machine and even took the pump apart, looking for trash/restrictions. Didn't find much. I put a gallon of vinegar in the reservoir and let that run for a while, and the return is flowing about twice as much as it was before (bypass no longer crimped) but the damn alarm is still going off.

    At this time, i have tightened the wires to the alarm itself, and got it to stop. But when i turn the cooler on, i don't get the initial single beep like i usually do when it is turned on. So it seems like it is either constantly on, or constantly off.
    I have had it running for like an hour now, and all of a sudden the alarm started to come on slowly, very short beeps that eventually turned into the regular alarm.

    Can i get a new flow sensor and alarm from HTP? I will call tomorrow but just wondering if anyone knew for sure. I really don't want to have to spend $600 on a new cooler because of the damn alarm.

    Thanks for reading, and have a nice day!
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  14. #86
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    11,003
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by massacre View Post
    Sorry, i know this thread is a little bit old, but i am having issues with my arctic chill cooler.
    Machine is a invertig 221 DV and i bought both at the same time. I love the machine, and the cooler has worked fine up until recently. I have had the machine and cooler for probably like 10 years now, i always used the HTP coolant but when covid hit i got a little behind on that. I wasn't using the machine regularly for a while. I did drain, flush and replace with new HTP coolant last year and it has been working great but the other day the flow alarm came on and would not shut off. I could see the bybass was really shooting water in, but the return was not flowing very much.
    I received my new torch and hoses today, figured that would fix it but it did not.
    I did take the cooler apart, removed the flow sensor/orifice and used vinegar to clean it. No dice. Clamped off the bypass and flow increased. I ended up removing the reservoir from the machine and even took the pump apart, looking for trash/restrictions. Didn't find much. I put a gallon of vinegar in the reservoir and let that run for a while, and the return is flowing about twice as much as it was before (bypass no longer crimped) but the damn alarm is still going off.

    At this time, i have tightened the wires to the alarm itself, and got it to stop. But when i turn the cooler on, i don't get the initial single beep like i usually do when it is turned on. So it seems like it is either constantly on, or constantly off.
    I have had it running for like an hour now, and all of a sudden the alarm started to come on slowly, very short beeps that eventually turned into the regular alarm.

    Can i get a new flow sensor and alarm from HTP? I will call tomorrow but just wondering if anyone knew for sure. I really don't want to have to spend $600 on a new cooler because of the damn alarm.

    Thanks for reading, and have a nice day!
    Have you tried giving USA Weld a call? Name:  Screenshot_20231023_213840_Chrome.jpg
Views: 105
Size:  90.6 KB
    Sent via smoke signals using my Lincoln buzzbox

  15. Likes massacre liked this post
  16. #87
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by massacre View Post
    Sorry, i know this thread is a little bit old, but i am having issues with my arctic chill cooler.
    Machine is a invertig 221 DV and i bought both at the same time. I love the machine, and the cooler has worked fine up until recently. I have had the machine and cooler for probably like 10 years now, i always used the HTP coolant but when covid hit i got a little behind on that. I wasn't using the machine regularly for a while. I did drain, flush and replace with new HTP coolant last year and it has been working great but the other day the flow alarm came on and would not shut off. I could see the bybass was really shooting water in, but the return was not flowing very much.
    I received my new torch and hoses today, figured that would fix it but it did not.
    I did take the cooler apart, removed the flow sensor/orifice and used vinegar to clean it. No dice. Clamped off the bypass and flow increased. I ended up removing the reservoir from the machine and even took the pump apart, looking for trash/restrictions. Didn't find much. I put a gallon of vinegar in the reservoir and let that run for a while, and the return is flowing about twice as much as it was before (bypass no longer crimped) but the damn alarm is still going off.

    At this time, i have tightened the wires to the alarm itself, and got it to stop. But when i turn the cooler on, i don't get the initial single beep like i usually do when it is turned on. So it seems like it is either constantly on, or constantly off.
    I have had it running for like an hour now, and all of a sudden the alarm started to come on slowly, very short beeps that eventually turned into the regular alarm.

    Can i get a new flow sensor and alarm from HTP? I will call tomorrow but just wondering if anyone knew for sure. I really don't want to have to spend $600 on a new cooler because of the damn alarm.

    Thanks for reading, and have a nice day!
    I posted my finding in another thread. Potential issue.... The valve /switch is adjustible. It looks like a black plastic coupler wires attached. There is a flat side with a panel held in place with tiny screws. The panel is adjustable. It will slide a couple millimeters.

    The panel is a magnet. The generic switch will operate to sense flow or no flow and is sensitive to the direction the panel is shifted.

    I think in posted photos in a John T thread about 3 years ago.

    The switch is readily available online no need to go to htp. I search,. but did not mine.

    Also, If it is coolant is Flowing then turn off the alarm.
    Last edited by tapwelder; 10-23-2023 at 11:54 PM.

  17. Likes massacre liked this post
  18. #88
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by 52 Ford View Post
    Have you tried giving USA Weld a call? Name:  Screenshot_20231023_213840_Chrome.jpg
Views: 105
Size:  90.6 KB
    I will call them tomorrow, thanks.
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  19. Likes 52 Ford liked this post
  20. #89
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by tapwelder View Post
    I posted my finding in another thread. Potential issue.... The valve /switch is adjustible. It looks like a black plastic coupler wires attached. There is a flat side with a panel held in place with tiny screws. The panel is adjustable. It will slide a couple millimeters.

    The panel is a magnet. The generic switch will operate to sense flow or no flow and is sensitive to the direction the panel is shifted.

    I think in posted photos in a John T thread about 3 years ago.

    The switch is readily available online no need to go to htp. I search,. but did not mine.

    Also, If it is coolant is Flowing then turn off the alarm.
    Thank you! I did see your response in this thread and i did try adjusting the panel with the little screws in both directions, but it didn't make much difference. I did not realize it was a magnet. I wonder if that black plastic coupling could be the culprit?
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  21. Likes 52 Ford liked this post
  22. #90
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Just as a follow up-
    Talked to HTP today. Pretty sure i can get the parts i need to get this flow alarm taken care of. HTP was very helpful on the phone and they also emailed me some helpful schematics and troubleshooting information.
    They will call tomorrow and we will get this ironed out.
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  23. Likes tapwelder, 52 Ford liked this post
  24. #91
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    11,003
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by massacre View Post
    Just as a follow up-
    Talked to HTP today. Pretty sure i can get the parts i need to get this flow alarm taken care of. HTP was very helpful on the phone and they also emailed me some helpful schematics and troubleshooting information.
    They will call tomorrow and we will get this ironed out.
    That's awesome!
    Sent via smoke signals using my Lincoln buzzbox

  25. Likes massacre liked this post
  26. #92
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Minor setback, HTP said they would have someone call me today. Well, no one called. So i emailed them and hopefully i will get a call back at some point?
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  27. Likes 52 Ford liked this post
  28. #93
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    I received an answer to my email- not sure where the miscommunication was, but now i have to wait until tomorrow to order the parts i need. 24hrs behind now. Not too happy about this, like they completely forgot all about my problem. At this rate i will likely have to spend a ton of cash to get what i need in a timely manner which is not ideal.
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  29. #94
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    can you operate te cooler without the alarm. I never notice flow issues when alarm went off. you can cool the torch manually.

    The lady, apparently forgot me when I called them.....

  30. Likes massacre liked this post
  31. #95
    Join Date
    Dec 2020
    Location
    Virginia, USA
    Posts
    11,003
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by tapwelder View Post
    can you operate te cooler without the alarm. I never notice flow issues when alarm went off. you can cool the torch manually.

    The lady, apparently forgot me when I called them.....
    I think the flow alarm is more important if your moving around a lot and worried about a hose kinking or something like that. If you're just at the bench welding something, what are the odds the pump is going to stop or a line get plug by... I dunno. Shouldn't be anything in the coolant since they use a biocide... I guess they use one... It's a handy feature, but I see no reason he couldn't run the cooler without it for a few week or two.
    Sent via smoke signals using my Lincoln buzzbox

  32. Likes tapwelder, massacre liked this post
  33. #96
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    With that in mind could the blockage be in the hose or torch? Is there a flow rate through the hose that can be measured?

  34. Likes massacre liked this post
  35. #97
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Follow up-
    Was able to get in touch with HTP today, everything went well. Was able to order what i needed. I did have to overnight ship everything which is a bitter pill to swallow. But i need my machine back up and running. Everyone at HTP was very friendly and helpful.
    Last edited by massacre; 10-26-2023 at 07:47 PM.
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  36. #98
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Quote Originally Posted by tapwelder View Post
    can you operate the cooler without the alarm. ..
    yes, it can be easily bypassed.

    Anyway, that "alarm" is a joke. You would be better served installing a Whirrly-gig flow gauge.

    I installed one on mine when I redid my cooler.

    If the gauge is spinning.... YOUR GOOD. End of story.

    That said.... ( I also have a pressure gauge and temperature sensors for in/out water temp) but basically if it's flowing and you have a moderate size water tank ..... you are good for most applications / and or weldORS ......

    don't get your brain in a frazzle.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  37. Likes Munkul, massacre liked this post
  38. #99
    Join Date
    Feb 2015
    Posts
    142
    Post Thanks / Like

    Re: 5460 DV cooler FLOW ALARM !!

    Received my parts today, replaced the flow switch and now all is well! Flow stops, alarm sounds. Flow begins, alarm stops. The only thing i can figure is that the flow switch got gummed up over time. I am flushing now with distilled water, then i have 2 gallons of HTP coolant and anti-algae/lubrication additive ready to go in.
    Looking forward to putting it all back together and using my new torch!

    Thanks again to everyone here for all of the helpful replies. Really appreciate it!
    2 Hobart MIG welders, 1 on the gas 1 flux core
    HTP Invertig 221 DV
    Eastwood TIG200
    HTP MIG 2400

  39. Likes 52 Ford liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,300,038.93894 seconds with 22 queries