    I've ran a 44lb spool of 71A85 through my XMT with a 74dx feeder about a year ago. I was doing 1" plate to 8x8x40lb h beams for building columns for my new building. Not sure what my settings were but i ran 1" to 1-1/4" stickout. I got some worm tracks but mine were all surface and not porosity. Material wasn't very clean, a little paint in the grinder grooves and some light flash rust. When i got the tracks i took the spool off the machine and baked it in the kitchen oven for 30 minutes at 250. Just over 212 to boil the water and not burn the fiber spool. Threw it on the welder right away and it ran fine. Preheating the first weld with a little propane torch helped too. After that the welds helped with preheat around the column. Started the building about 2 years ago and lumber prices spiked so i stalled on the building. Will post pictures of the steel sometime soon. Going to have a bridge crane in this one... maybe two!!

  2. #77
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    7,972
    Post Thanks / Like

    Re: Worm tracks

    Quote Originally Posted by ferrret3238 View Post
    I've ran a 44lb spool of 71A85 through my XMT with a 74dx feeder about a year ago. I was doing 1" plate to 8x8x40lb h beams for building columns for my new building. Not sure what my settings were but i ran 1" to 1-1/4" stickout. I got some worm tracks but mine were all surface and not porosity. Material wasn't very clean, a little paint in the grinder grooves and some light flash rust. When i got the tracks i took the spool off the machine and baked it in the kitchen oven for 30 minutes at 250. Just over 212 to boil the water and not burn the fiber spool. Threw it on the welder right away and it ran fine. Preheating the first weld with a little propane torch helped too. After that the welds helped with preheat around the column. Started the building about 2 years ago and lumber prices spiked so i stalled on the building. Will post pictures of the steel sometime soon. Going to have a bridge crane in this one... maybe two!!
    Worm tracks & porosity seem cured, I guess by being indoors. Mostly I weld outdoors, as clearing an area of everything flamable is a job.

    My wife has these space bags she put away summer clothes in. Seal them up & vacuum the air out. They are amazing! 80 LBS of clothing fits in the space of a white garbage bag, maybe 20 gallons. I'm going to try them for wire storage. I don't need Dual Shield often, so a reel lasts a long while.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,638,354,020.61696 seconds with 11 queries