    A little brazing, brass to brass

    1) test coupon. Brazed with 45 percent silver. Practice for a metal sculpture/cabinet. Done earlier this year. The brass is almost 3/16 thick. The metal is from a watchmaker, bought out from my neighbor a jeweler. He cut gears for it, suspect.

    2) tig power lug. Brazed/welded? with bronze rod. Done about 10 yrs ago

    3+) repair lamp. Done Monday. 45 percent silver. Not sure if it is antique or upcycled, it has a gas valve on the large part. Wiring was done after retro. There are epoxy filled external holes drilled in the tube for routing.
    Attached Images Attached Images      
    Last edited by tapwelder; 06-04-2020 at 07:57 AM.

  2. Likes pigpen60 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,026,751.46130 seconds with 13 queries