+ Reply to Thread
Page 2 of 2 FirstFirst 12
Results 26 to 42 of 42

Thread: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

  1. #26
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,879
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    hard to say without actually being there to see what is happening.

    To me it looks like a drive roll/wire feed problem and possibly a Contact to Work Distance issue.

    is the drive roll the correct one for .035?

    Is the drive roll tension set correctly?

    You could try .030 wire. Looks ike you are welding 1/8" angle.

    Good luck.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  2. #27
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Are those welds done in the horizontal position? Looks like there's some gravity sag .

    The steel in the pics has not been ground clean.

    Check your ground connections, make sure you have a cleaned spot for the clamp.


    Higher voltage makes your weld flatten out. Try turning the volts up, and not just one setting. Turn up the volts, then adjust the wire while welding, till you get a nice crackling sound.

    Different gas flow rates are not going to flatten anything out, the gas only stops porosity, it doesn't affect the heat.

  3. #28
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Is there any way you can try another bottle? I've gotten several bottles that were contaminated in the past (different sources) and it can be very frustrating. I have multiple bottles for everything now, but any time I bring home a new bottle I run do a quick test run to make sure the gas is good...that way I can return it right away and they don't ask why it took a couple of months for me to figure out it was bad gas.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  4. #29
    Join Date
    Dec 2012
    Location
    Rochester, NY
    Posts
    17
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Sorry for the absence guys. I needed a couple of days to let the frustration subside, and then it got HOT. With the shop being on the West side of the building and the blacktop, I was looking at 120 degrees ambient in the sun.

    Anyway, it cooled off and I got back to the project. I literally changed NOTHING but now all of a sudden most of the beads are much better. Same program on the welder. Same technique. Same gas bottle. Same CFH (25 static, 21-22 with the trigger pulled). I am doing nothing different, and getting different results.

    Everyone is asking for my settings. Here they are. It's the bog standard 10ga preprogrammed setting on the welder. Welding 1/8" mild steel. As I stated earlier, ANY variation from the preprogrammed settings makes the welds WORSE. Even if it's still in the green.
    Attached Images Attached Images  

  5. #30
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    1,029
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    I think you just need to get more comfortable before you pull the trigger. The welds look like one handed attempts.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  6. Likes denverguy liked this post
  7. #31
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by BarnyardEngineering View Post
    Same gas bottle. Same CFH (25 static, 21-22 with the trigger pulled).
    I'm not expert, but I've always believed gas flow settings are when the trigger is depressed. 21-22 is on the low side....I'd at least bump it to 25 and see what happens and then maybe a touch higher like 28. You obviously don't want to waste gas, and way too much can cause problems, but better to have a little bit more than you need than be on the low side.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  8. #32
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,879
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by G-ManBart View Post
    I'm not expert, but I've always believed gas flow settings are when the trigger is depressed. 21-22 is on the low side....I'd at least bump it to 25 and see what happens and then maybe a touch higher like 28. You obviously don't want to waste gas, and way too much can cause problems, but better to have a little bit more than you need than be on the low side.
    I have my gas flow down around 15 CFH.


    I still don't think it is a gas flow problem.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  9. #33
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    You probably just weren't holding your mouth right.

  10. #34
    Join Date
    Jan 2004
    Posts
    1,875
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    The brand of wire you're running can have an influence on the quality of the results you're able to achieve. Welding over mill scale definitely kills weld puddle wet out some. Pulling the weld puddle tends to want to make a weld bead that is on the ropey side if you don't use a fair amount if oscillation. Based on what I am seeing in your pics, I'd try increasing the inductance.
    Last edited by Dan; 06-13-2020 at 08:31 PM.
    ESAB Migmaster 250
    Hobart Ironman 230
    Multimatic 215
    TWECO Fabricator 181i & 211i
    HH125EZ - nice little fluxcore only unit


    Maxstar 150 STH - very nice

  11. #35
    Join Date
    Dec 2012
    Location
    Rochester, NY
    Posts
    17
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by Rondo View Post
    I think you just need to get more comfortable before you pull the trigger. The welds look like one handed attempts.
    Nope, two handed, braced, as comfortable as I can get, making small cursive e's like all the howto videos tell you to.

  12. #36
    Join Date
    Dec 2012
    Location
    Rochester, NY
    Posts
    17
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by Dan View Post
    The brand of wire you're running can have an influence on the quality of the results you're able to achieve. Welding over mill scale definitely kills weld puddle wet out some. Pulling the weld puddle tends to want to make a weld bead that is on the ropey side if you don't use a fair amount if oscillation. Based on what I am seeing in your pics, I'd try increasing the inductance.
    ...and how would you go about that? My welder does not have any "inductance" setting.

    I can change voltage, and I can change wire feed speed. Any more voltage results in burnback to the tip, and a ruined tip. Any less voltage results in the wire "poking" at the work, lots of pops, and lots of spatter. Any less wire again results in burnback and a ruined tip. Any more wire again results in the wire "poking" at the work, lots of popping and spatter.

  13. #37
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by BarnyardEngineering View Post
    .Any more wire again results in the wire "poking" at the work, lots of popping and spatter.
    this is where you play with the voltage as well. It's a combination of the two that results in the proper operation. Make sure you are running a ~1/4 to 3/8" CTWD. What you just mentioned is the exact jist of what it means to "learn how to weld", at least with MIG welding.
    1st on WeldingWeb to have a scrolling sig!



  14. #38
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    1,414
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Press for Options
    press the knob below the screen to change options as noted on my picture, (

    Just in case you lost the manual: https://www.lincolnelectric.com/asse...3/imt10164.pdf
    pages 19, and 20 should help.
    From the symptom you describe ,the most likely problems are: bad ground, mill scale in weld zone, wrong size tip , nozzle loaded with spatter making it not arc properly.
    Things I noticed in picture: not welding in a straight line(can't see weld area?) , travel speed, or movement inconsistent(bead goes narrow to wide?). Inconsistent gun angle (starts out tall and lumpy, and widens/flattens out as it goes,as if SMAW)
    Consistent distance, movement, angle are needed to get a good weld. Almost like the gun is on rail and sliding in one axis. I don't mean to be overly critical, this is just what I'm guessing from the pictures you posted. I have the same welder, and have made, and continue to make some of these worms. Thats why I do a test weld to check setting before welding a finished piece, often need to adjust a little, unless your welding the same thing over, and over. There are also many you tube videos on setting up the 210mp. I'm sure there must be someone in your area who could help. Are you located right in Rochester NY ? My Inlaws used to live in Danville NY, just south of there.

    Hope it helps, wish you luck.


    \
    Last edited by albrightree; 06-16-2020 at 11:40 AM.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D
    Primeweld 225 ac/dc
    Primeweld mig180
    Miller AEAD-200

  15. Likes lars66 liked this post
  16. #39
    Join Date
    Nov 2012
    Posts
    3,274
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    If you adjust one, you generally need to adjust the other accordingly.

  17. #40
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    8,879
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by BarnyardEngineering View Post
    ...and how would you go about that? My welder does not have any "inductance" setting.

    I can change voltage, and I can change wire feed speed. Any more voltage results in burnback to the tip, and a ruined tip. Any less voltage results in the wire "poking" at the work, lots of pops, and lots of spatter. Any less wire again results in burnback and a ruined tip. Any more wire again results in the wire "poking" at the work, lots of popping and spatter.
    Your machine does have inductance.
    it is in the manual.
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Klutch 120v Plasma cutter
    SO 2020 bender
    Beer in the fridge

  18. #41
    Join Date
    Jan 2005
    Posts
    5,184
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by BarnyardEngineering View Post
    ...and how would you go about that? My welder does not have any "inductance" setting.
    Best leave it me to argue with Dan..Even then I only can ding him on the fringes...
    Blue Demon 140 MSI
    Blue Demon 200 AC/DC
    Esab 160i caddy
    Esab CV353
    INE 1500
    Lincoln 250 Idealarc
    Thermal LM-200
    Thermal 60i- 3phase
    Thermal 15c
    Topshak 40 plasma
    Miller Regency 200/LN-72
    Viking 250 mig/2410 feeder
    Weldcote 140

  19. #42
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Is it me or is it the machine? Lincoln MP-210 MIG mode layin' worms

    Quote Originally Posted by Broccoli1 View Post
    Your machine does have inductance.
    it is in the manual.
    Yup. School'ed! Page 22.
    1st on WeldingWeb to have a scrolling sig!



+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,282,685.37007 seconds with 22 queries