I have never run their 6010, but their 7018 has always been great.
In the middle of a big fence project and tired of buying 10 lb boxes of Washington Alloy 6010 from LWS and not willing to fork over $180 for a 50 lb can of Lincoln. Found a deal online for 50 lb of ESAB Sureweld 6010 for $94. Are these decent rods? I don’t need X-ray quality, just for high school boys to run on pipe fence.
Sent from my iPhone using Tapatalk
I have never run their 6010, but their 7018 has always been great.
Just a thought, if this is for a school, you may be able to get some samples from ESAB. That would allow you to try some before you commit to an order.
I recall CEP really liked Esab Sureweld 10P 6010 and said it runs the best on an inverter. 6010 can be a challenge on some inverters so I'd say you should be good.