    Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    The price was right - free. First come first serve listing on Craigslist and I finally beat the others.

    Name:  20200909-131334-01.jpg
Views: 1136
Size:  139.2 KB

    Amazingly it works - here's the run down:


    • Tightened up all the bolts and nuts (plenty were loose)
    • Belts are in good shape
    • Motor is smooth and quiet
    • Surface oxidation isn't bad, steel wool will take care of it


    This will be the biggest issue to overcome - the splined shaft that runs thru the drive sheave is worn, as is the bushing in the sheave itself. The other issue is: It seems the splined shaft is too short, because when the spindle is lowered, the splined shaft completely disappears, letting the sheave run loose.

    Name:  20200909-131352-01.jpg
Views: 1106
Size:  185.5 KB
    Name:  20200909-131523-01.jpg
Views: 1096
Size:  146.3 KB
    Name:  20200909-131426-01.jpg
Views: 1093
Size:  211.6 KB

    The internals look and feel fine, no movement or slop - (just the shaft in the sheave has movement) So, either the splined shaft broke or was cut - or it was retrofitted before, but with the wrong replacement.

    I want to disassemble the quill and shaft so I can get accurate measurements of the shaft length, but I do not know exactly the order of steps or what snap rings, screws, etc. need to come out.

    Name:  20200909-132839-01.jpg
Views: 1085
Size:  223.1 KB

    To be continued...
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  2. #2
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    I imagine the design is similar to this:

    Name:  16-16l_spindle_assembly.jpg
Views: 1267
Size:  44.0 KB

    If you can guide me, I can take more pics of what you need to assist me with identifying how to take it apart with minimal errors.

    I can't find much online for this thing, as there is no manufacturer name I can find, just a model number - and searching it just brings up basic info and old sales listings. The 4-spline shaft is also unique - I see lots of 6 spline and more - but the 4 splines I'm finding are thicker than what I'm measuring. I could go to a different spline count if I can match up the rest of the dimensions with something I find - but then I have to track down the corresponding bushing or another sheave to match it.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  3. #3
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Name:  20200909_170327-01.jpg
Views: 1145
Size:  260.6 KB

    Name:  20200909_170200-01.jpg
Views: 1077
Size:  125.9 KB

    Name:  20200909_165736-01.jpg
Views: 1107
Size:  201.2 KB

    Name:  20200909_165852-01.jpg
Views: 1101
Size:  159.1 KB
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  4. #4
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    367
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    My guess is you won't find replacement parts to fit. Might be simplest to take the 4-spline to a machinist and ask him to machine up an extension piece to lengthen it with centre pin and bevel. Then weld the extension on and remove the bead with die grinder and file. Then you're not hunting for parts or overcapitalising a hunk of bamboo.

  5. Likes ronsii liked this post
  6. #5
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Maybe the spline shaft has just slipped too far down into the quill adapter???? Have you tried pulling on it upwards??

    Or maybe someone modified/lost parts so the quill would go down further than it is supposed to...

  7. Likes Shootr, filetobeef liked this post
  8. #6
    Join Date
    Mar 2015
    Location
    Milwaukee, WI
    Posts
    438
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    You need to remove the quill return spring and then the feed shaft pinion before you remove the quill.
    Here's a disassembly video for one similar to yours:

  9. Likes Shootr liked this post
  10. #7
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by ronsii View Post
    Maybe the spline shaft has just slipped too far down into the quill adapter???? Have you tried pulling on it upwards??

    Or maybe someone modified/lost parts so the quill would go down further than it is supposed to...
    No, the spline shaft doesn't budge when I try to pull it up. I don't think it's going any lower than it is supposed to. When the quill is fully extended, the slot for the drift to remove the chuck just clears the housing. Once I get the assembly out I can look closer at it.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  11. #8
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Denis G View Post
    You need to remove the quill return spring and then the feed shaft pinion before you remove the quill.
    Here's a disassembly video for one similar to yours:
    That's the ticket - I watched this and a couple others - they mostly are all alike. Thanks!
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  12. #9
    Join Date
    Feb 2012
    Posts
    4,316
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    I don't rebuild drill presses but I think I have the identical drill press. Let me know if you need pics.

  13. Likes strangebrew liked this post
  14. #10
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Shootr View Post
    Name:  20200909_170327-01.jpg
Views: 1145
Size:  260.6 KB

    Name:  20200909_170200-01.jpg
Views: 1077
Size:  125.9 KB

    Name:  20200909_165736-01.jpg
Views: 1107
Size:  201.2 KB

    Name:  20200909_165852-01.jpg
Views: 1101
Size:  159.1 KB
    The spline is not too short. If you look in your second pic that shows the bottom of the sheave and the top of the spindle you will see that the spline part in the sheave is supposed to be one piece with the part that is held by the bearing that the spindle goes through. It is broken off. Pull that top bearing out and the piece going through it could be removed but is probably a press fit in the bearing .By the look of the grain I would say it is cast iron. It could be brazed back together if you remove the spline part from the sheave and disassemble the spindle. I suspect it will break again if abused though. With that said it will be as strong as it was originally if done correctly .
    Last edited by thegary; 09-10-2020 at 12:05 PM.

  15. Likes Denis G liked this post
  16. #11
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by thegary View Post
    The spline is not too short. If you look in your second pic that shows the bottom of the sheave and the top of the spindle you will see that the spline part in the sheave is supposed to be one piece with the part that is held by the bearing that the spindle goes through. It is broken off. Pull that top bearing out and the piece going through it could be removed but is probably a press fit in the bearing .By the look of the grain I would say it is cast iron. It could be brazed back together if you remove the spline part from the sheave and disassemble the spindle. I suspect it will break again if abused though. With that said it will be as strong as it was originally if done correctly .
    Name:  f0de5cbe6bca37bb9e953cb4523ce0be.jpg
Views: 1013
Size:  31.9 KB

    Dang, those are some sharp eyes you have there! Sure as heck looks like it. I was able to press out the bearing assembly without damage, and get the bushing out as well.

    Name:  20200910-101428-01.jpg
Views: 1015
Size:  247.8 KB

    Name:  20200910-103015-01.jpg
Views: 1009
Size:  247.6 KB

    Is there anything else I can post to help determine if it is indeed cast iron? I want it to be as strong as possible, but I won't be abusing it either - I wanted one more for accurate drilling than hogging out giant holes with twist bits in plate steel.

    Is brazing the best/only choice? I'm going to hire this one out as it is far beyond my available equipment and skill level.

    Thanks again for taking the time to help me out.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  17. Likes whtbaron liked this post
  18. #12
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Shootr View Post
    Name:  f0de5cbe6bca37bb9e953cb4523ce0be.jpg
Views: 1013
Size:  31.9 KB

    Dang, those are some sharp eyes you have there! Sure as heck looks like it. I was able to press out the bearing assembly without damage, and get the bushing out as well.

    Name:  20200910-101428-01.jpg
Views: 1015
Size:  247.8 KB

    Name:  20200910-103015-01.jpg
Views: 1009
Size:  247.6 KB

    Is there anything else I can post to help determine if it is indeed cast iron? I want it to be as strong as possible, but I won't be abusing it either - I wanted one more for accurate drilling than hogging out giant holes with twist bits in plate steel.

    Is brazing the best/only choice? I'm going to hire this one out as it is far beyond my available equipment and skill level.

    Thanks again for taking the time to help me out.
    Its cast iron , it would not break clean like that if it were steel. A new piece could be made from steel but I suspect it would cost you more than the drill press is worth. I would find a V block or use a piece of angle iron to use as a V block then shim the smaller diameter piece to get it centered. If both parts are shamfered so the braze can penatrate completly it should hold fine. Use the quill spline to clock the spline while clamping it then pull it out before brazing. It might wind up with the pully having a slight woble to it but it should work fine.

  19. Likes Shootr, ronsii liked this post
  20. #13
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by thegary View Post
    Its cast iron , it would not break clean like that if it were steel. A new piece could be made from steel but I suspect it would cost you more than the drill press is worth. I would find a V block or use a piece of angle iron to use as a V block then shim the smaller diameter piece to get it centered. If both parts are shamfered so the braze can penatrate completly it should hold fine. Use the quill spline to clock the spline while clamping it then pull it out before brazing. It might wind up with the pully having a slight woble to it but it should work fine.
    I still don't want to try it myself - I've never brazed anything before. Questions:

    Should the mating surfaces be machined down flat for the best joint? I'm assuming so, from what I'm reading the tighter the joint, the stronger it is.

    What would be a "going rate" for a job like this?
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  21. #14
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Shootr View Post
    I still don't want to try it myself - I've never brazed anything before. Questions:

    Should the mating surfaces be machined down flat for the best joint? I'm assuming so, from what I'm reading the tighter the joint, the stronger it is.

    What would be a "going rate" for a job like this?
    Silver braze needs a tight joint. Regular braze does not. It needs to be ground out to a V then use a burr to remove the carbon that the grinding smears on the Ved area.
    I do not know what a shop would charge If I were doing it it would be around $100 . There is prep and some machining after it is brazed. Good luck on finding a shop that will do it.

  22. Likes ronsii liked this post
  23. #15
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Those drill presses are sold under 100 different brands. I would try to fine some place that sells parts like maybe Jet or tractor supply and see if you can get a new piece. It would be inexpensive in comparison if you can find one. Maybe even Sears.

  24. Likes ronsii, Shootr liked this post
  25. #16
    Join Date
    Mar 2015
    Location
    Milwaukee, WI
    Posts
    438
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Shootr View Post
    I still don't want to try it myself - I've never brazed anything before. Questions:

    Should the mating surfaces be machined down flat for the best joint? I'm assuming so, from what I'm reading the tighter the joint, the stronger it is.

    What would be a "going rate" for a job like this?
    If you go to a welding supply place that refills oxy-acetylene tanks, they may be able to give you a contact for someone who might do the job. Leave the details to someone with a good reputation for their work.
    (Edit: They may also know someone that does TIG or MIG brazing with silicone bronze.)
    Last edited by Denis G; 09-11-2020 at 10:50 AM.

  26. Likes Shootr liked this post
  27. #17
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    https://www.ereplacementparts.com/dr...-p-442506.html this is the same part for a jet drill press. It looks like it could be the one you need. If not there are several other model number drill presses that you could look at. You might even try typing in your brand and model number, they might have it.
    Last edited by thegary; 09-11-2020 at 04:07 PM.

  28. Likes Shootr liked this post
  29. #18
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by thegary View Post
    https://www.ereplacementparts.com/dr...-p-442506.html this is the same part for a jet drill press. It looks like it could be the one you need. If not there are several other model number drill presses that you could look at. You might even try typing in your brand and model number, they might have it.
    Now that you showed me the correct name for the part, it's a heck of a lot easier to google! Again, thanks for providing this information. Now the hard part is finding dimensions and/or pictures to try and match it up. My model number (no manufacturer on the tag) only pulls up chinese alibaba type sales sites. I do get the reference West Lake Industries a lot, but still limited search results.

    The exact part in your link is close, but uses a 6204 bearing (20mm bore) and mine uses 17mm 6203 bearings. I'm going through different drill press model parts diagrams to see what bearings go with which drive sleeve. This one appears to be it, but I'm waiting for them to email me back - I can't enlarge the diagram enough to make out the dimensions. https://www.ebuy7.com/item/543503583601

    Name:  driver sleeve.jpg
Views: 954
Size:  53.3 KB
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  30. #19
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    One step forward, two steps back...

    I decided to try and MIG the sleeve back together, so I practiced a bunch to get my settings close, then set up the two pieces in a length of angle, with the spindle in them to keep them clocked together. All I have is a yellow mappro torch, so I used it to preheat the parts, then put 4 tacks around the perimeter, where the thickest parts were. No matter how I tried to clean out the bores, there was still gunk in them so I was getting horrible porosity. I did three tries - clean, tack, test - repeat. On the third try I seemed to have gotten it - after grinding the welds down, even though there was still some porosity, I couldn't snap them apart.

    Name:  20200913-094228-01.jpg
Views: 939
Size:  159.4 KB

    Name:  20200913-104319-01.jpg
Views: 919
Size:  120.2 KB

    Now I'm feeling pretty excited, just cleaning, tightening, regreasing - slowly putting it all back together. The bearings pressed onto the repaired part just right, was able to press the assembly in to the housing, etc. Last thing is the spindle pulley, I put it on and tap it down gently with a rubber mallet - needed a little nudge for the v-grooves to line up. Then, the pulley and shaft go wobbly...I managed to snap the shaft again - further up, where the bearings go.

    So it's time to step away and put this aside for a while. Maybe I'll find a chinaman with the right part, maybe another drill comes up for sale for cheap, maybe I'll disassemble the entire quill/spindle assembly to see if I can just switch to a different design that seems to be all over the alibaba ships. All I know now is I'm too frustrated to mess with it for a while.

    Name:  20200913-115050-01.jpg
Views: 935
Size:  220.7 KB
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  31. #20
    Join Date
    Oct 2015
    Posts
    2,810
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by Shootr View Post
    One step forward, two steps back...

    I decided to try and MIG the sleeve back together, so I practiced a bunch to get my settings close, then set up the two pieces in a length of angle, with the spindle in them to keep them clocked together. All I have is a yellow mappro torch, so I used it to preheat the parts, then put 4 tacks around the perimeter, where the thickest parts were. No matter how I tried to clean out the bores, there was still gunk in them so I was getting horrible porosity. I did three tries - clean, tack, test - repeat. On the third try I seemed to have gotten it - after grinding the welds down, even though there was still some porosity, I couldn't snap them apart.

    Name:  20200913-094228-01.jpg
Views: 939
Size:  159.4 KB

    Name:  20200913-104319-01.jpg
Views: 919
Size:  120.2 KB

    Now I'm feeling pretty excited, just cleaning, tightening, regreasing - slowly putting it all back together. The bearings pressed onto the repaired part just right, was able to press the assembly in to the housing, etc. Last thing is the spindle pulley, I put it on and tap it down gently with a rubber mallet - needed a little nudge for the v-grooves to line up. Then, the pulley and shaft go wobbly...I managed to snap the shaft again - further up, where the bearings go.

    So it's time to step away and put this aside for a while. Maybe I'll find a chinaman with the right part, maybe another drill comes up for sale for cheap, maybe I'll disassemble the entire quill/spindle assembly to see if I can just switch to a different design that seems to be all over the alibaba ships. All I know now is I'm too frustrated to mess with it for a while.

    Name:  20200913-115050-01.jpg
Views: 935
Size:  220.7 KB

    What part of "its cast iron" did you not understand. I hope you can find a new one because that one is beyond hope now.

  32. #21
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by thegary View Post
    What part of "its cast iron" did you not understand. I hope you can find a new one because that one is beyond hope now.

    I know, I know...I F'd up. All the people I contacted locally were either not wanting to do a "small" job, or didn't reply after giving the details (to braze it). One person said $150 to weld it with SS wire - everything I read on that method wasn't very positive (and for $150 I'll go buy a new HF drill).

    I was playing with house money since the press was free to begin with. As I mentioned above, I'll just keep googling and searching until something pops up. I really do appreciate all the help you provided, please don't take my screw up as wasting your time.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  33. #22
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Reason #348 that 2020 is just a f'up year...

    Back in September, as a last effort to find the spindle and pulley sleeve, I hit up the local Harbor Freight to see what the internals on their presses looked like.

    Unbelievable - two of the medium sized models looked and measured correct (save for them being 6 spline vs. my original 4 spline). Great thing about being in a HF store, all the measuring tools are right there to use. I still wasn't sure about the pulley sleeve as I couldn't get a look at it, but when I grabbed a crescent wrench to try and pull the nut off - the employees had had enough of me and told me to knock it off lol.

    Well heck, for $20 +/-, I ordered up the spindle, sleeve, and nut and crossed my fingers...

    In early October I received a package - except only the nut and spindle were in it - no sleeve - BACKORDERED!!!!! AAAARRRRGGGHHHH - I'm so close.... But miracles upon miracles the spindle fit perfectly!

    Name:  20200930-212034-01.jpg
Views: 859
Size:  101.2 KB

    So I patiently waited until the end of October, then I called to see if they had an idea when they would get more inserts in. "Oh yeah, they're here - you want we should send it to you?" Uh yeah, that'd be great. A week later - nada. Called again "So sorry, I'm going to just put a new order in and get it sent right out to you 2nd day air". Another week later (this past Wed) I called again - after 3 different people I got another promise to send one out ASAP.

    'Ding Dong'...I answer the door today and lo and behold there's a fedex envelope with HF address on it! I eagerly pick it up...

    Name:  JFC.jpg
Views: 877
Size:  86.4 KB

    To see a big friggin' tear in it and nothing but a packing list inside...

    2020? Go F yourself...
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  34. #23
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    4,036
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    I would have made new part over welding parts back.
    But I have a machinist background too.

    Dave

    Quote Originally Posted by Shootr View Post
    The price was right - free. First come first serve listing on Craigslist and I finally beat the others.

    Name:  20200909-131334-01.jpg
Views: 1136
Size:  139.2 KB

    Amazingly it works - here's the run down:


    • Tightened up all the bolts and nuts (plenty were loose)
    • Belts are in good shape
    • Motor is smooth and quiet
    • Surface oxidation isn't bad, steel wool will take care of it


    This will be the biggest issue to overcome - the splined shaft that runs thru the drive sheave is worn, as is the bushing in the sheave itself. The other issue is: It seems the splined shaft is too short, because when the spindle is lowered, the splined shaft completely disappears, letting the sheave run loose.

    Name:  20200909-131352-01.jpg
Views: 1106
Size:  185.5 KB
    Name:  20200909-131523-01.jpg
Views: 1096
Size:  146.3 KB
    Name:  20200909-131426-01.jpg
Views: 1093
Size:  211.6 KB

    The internals look and feel fine, no movement or slop - (just the shaft in the sheave has movement) So, either the splined shaft broke or was cut - or it was retrofitted before, but with the wrong replacement.

    I want to disassemble the quill and shaft so I can get accurate measurements of the shaft length, but I do not know exactly the order of steps or what snap rings, screws, etc. need to come out.

    Name:  20200909-132839-01.jpg
Views: 1085
Size:  223.1 KB

    To be continued...

  35. #24
    Join Date
    Dec 2018
    Location
    Southern California
    Posts
    977
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Oh man that is frustrating. At this point you have to finish it or you'll never rest!

    Reminds me of the time I tried ordering a slave roller for a bench belt grinder, 3 different companies (all were great though) and 6 different attempts, each arrived dented. That bench grinder is still in the corner in near perfect condition and some day i'll rig something up (don't have a lathe or mill unfortunately).

  36. Likes Shootr liked this post
  37. #25
    Join Date
    May 2020
    Location
    Arizona
    Posts
    995
    Post Thanks / Like

    Re: Refurb'ing a Chinese Floor Drill Press - Parts and Disassembly Discussion

    Quote Originally Posted by SlowBlues View Post
    Oh man that is frustrating. At this point you have to finish it or you'll never rest!

    Reminds me of the time I tried ordering a slave roller for a bench belt grinder, 3 different companies (all were great though) and 6 different attempts, each arrived dented. That bench grinder is still in the corner in near perfect condition and some day i'll rig something up (don't have a lathe or mill unfortunately).
    Oh it's a full on quest at this point!
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,500,600.67935 seconds with 13 queries