    The baffles on the muffler on my friend Rick’s tractor were shot, so it was very noisy. The original muffler had been welded to the exhaust pipe, so I cut through the weld of the old worn out muffler and welded on a new one. I like to weld the muffler to the pipe or a Nipple, because the threads of the muffler are in thin sheet metal and they crack off as shown in the following link.

    https://forum.millerwelds.com/forum/...ohn#post598219

    The first picture shows where I cut through the original weld. The weld looked like bird $hit, but it held up until the muffler wore out so I can’t complain.

    1. Old Muffler
    Name:  1. Old Muffler.jpg
Views: 669
Size:  102.0 KB

    The new muffler had a 1” NPT thread on it and the pipe was ¾” nominal pipe size, so I screwed in a 1” NPT close nipple into the muffler to reduce the hole size as shown below.

    2. Muffler with nipple
    Name:  2.  Muffler with nipple.jpg
Views: 686
Size:  39.9 KB
    Last edited by Don52; 09-25-2020 at 02:19 PM.
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  2. Likes ronsii liked this post
  3. #2
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    921
    Post Thanks / Like

    Re: Muffler Replacement

    More to come.
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  4. Likes ronsii liked this post
  5. #3
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    921
    Post Thanks / Like

    Re: Muffler Replacement

    Next I sawed off the nipple with about 1/16” protruding as shown below.

    3. Muffler with cut down nipple
    Name:  3. Muffler with cut down nipple.jpg
Views: 665
Size:  37.6 KB

    Unfortunately, I didn’t take a picture of the weld, but I welded the nipple to the muffler. Then I welded the muffler to the exhaust pipe as shown below.

    4. Muffler welded to pipe
    Name:  4. Muffler welded to pipe.jpg
Views: 680
Size:  100.7 KB

    Last but not least I painted it. I didn’t bother to purchase high temperature paint so it will burn off the hot exhaust pipe, but the paint should still protect the muffler.

    5. Muffler painted
    Name:  5. Muffler painted.jpg
Views: 665
Size:  79.7 KB

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  6. Likes ronsii liked this post
  7. #4
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    11,394
    Post Thanks / Like

    Re: Muffler Replacement

    why didnt you just weld a threaded coupling onto the pipe so the next time it needs replacing you just unscrew the old and screw the new one on??

  8. #5
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    921
    Post Thanks / Like

    Re: Muffler Replacement

    Quote Originally Posted by Hobbytime View Post
    why didnt you just weld a threaded coupling onto the pipe so the next time it needs replacing you just unscrew the old and screw the new one on??
    I wasn't sure if the tractor could accommodate the additional length of the coupler and nipple.
    You will also notice that I welded the muffler crooked, just like the original, for the same reason.
    I am familiar with the nipple approach and have used it in the past:

    https://forum.millerwelds.com/forum/...ohn#post598219



    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  9. Likes Hobbytime, ronsii liked this post
  10. #6
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    11,394
    Post Thanks / Like

    Re: Muffler Replacement

    Quote Originally Posted by Don52 View Post
    I wasn't sure if the tractor could accommodate the additional length of the coupler and nipple.
    You will also notice that I welded the muffler crooked, just like the original, for the same reason.
    I am familiar with the nipple approach and have used it in the past:

    https://forum.millerwelds.com/forum/...ohn#post598219



    -Don
    I guess not having the unit the muffler goes on makes fitting it a bit difficult...better safe than sorry...nice repair either way...

  11. #7
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    921
    Post Thanks / Like

    Re: Muffler Replacement

    On a previous repair, my customer didn't tighten the 1" NPT nipple properly into the exhaust pipe and the threads rattled around and wore out. Fortunately the nipple that I welded on was long enough to add additional threads. The first picture shows how I clamped the muffler to chase the 1" NPT threads deeper on the nipple.

    11. Muffler clamped to table with 1 inch NPT die
    Name:  11. Muffler clamped to table with 1 inch NPT die.jpg
Views: 659
Size:  106.5 KB

    The next picture shows my friend John manually chasing the threads with a home made die stock.

    12. Chasing 1 inch NPT thread
    Name:  12. Chasing 1 inch NPT thread.jpg
Views: 654
Size:  147.1 KB

    The next picture shows the deeper threads. If you look closely, you can see that the original threads are undersize compared to the new ones.

    13. Threads on nipple chased
    Name:  13. Threads on nipple chased.jpg
Views: 657
Size:  80.2 KB

    The next picture shows me cutting off the damaged thread from the nipple on the muffler.

    14. Cutting off damaged threads
    Name:  14. Cutting off damaged threads.jpg
Views: 648
Size:  89.2 KB

    And here it is all done.

    15. Nipple cut down.
    Name:  15. Nipple cut down..jpg
Views: 659
Size:  82.5 KB

    The moral of the story is if you use the welded on nipple approach, be sure to firmly tighten the muffler.

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  12. Likes ronsii liked this post
  13. #8
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    921
    Post Thanks / Like

    Re: Muffler Replacement

    Here is a picture of the muffler installed on the tractor.
    Name:  02748854-1A06-41A1-9CAF-682CD207F415.jpeg
Views: 432
Size:  110.5 KB


    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Mast Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP
    Everlast PowerTIG 400 EXT

  14. Likes ronsii liked this post
  15. #9
    Join Date
    Mar 2011
    Location
    Bilbao, Spain
    Posts
    929
    Post Thanks / Like

    Re: Muffler Replacement

    Great save!

    I usually have any kind of muffler work. Steel is paper thin, rusted, etc.

    Mikel

  16. Likes ronsii liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,252,551.40920 seconds with 22 queries