Results 1 to 6 of 6

Thread: Welding Zinc Question

  1. #1
    Join Date
    Sep 2019
    Posts
    16
    Post Thanks / Like

    Welding Zinc Question

    Good morning.
    From what I understand, welding Zinc can be deadly/dangerous. I need to make some shutter hangers. They are essentially a lag bolt with a small section of rod at the end that slides inside the shutter hinge. If I buy zinc coated lag bolt at Lowe's, can I grind the end and safely weld a piece of rod on it?
    Thanks
    Nick

  2. #2
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Zinc Question

    Quote Originally Posted by nicksorg View Post
    Good morning.
    From what I understand, welding Zinc can be deadly/dangerous. I need to make some shutter hangers. They are essentially a lag bolt with a small section of rod at the end that slides inside the shutter hinge. If I buy zinc coated lag bolt at Lowe's, can I grind the end and safely weld a piece of rod on it?
    Thanks
    Nick
    Yes, you can grind the zinc off... try not to breathe the fumes while welding as the HAZ will still burn zinc if you don't grind WAY past where the weld will actually be

    I weld zinc plated all the time... just make sure you are upwind, outdoors, or have a good respirator on.

  3. Likes CAVEMANN liked this post
  4. #3
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Zinc Question

    Also when grinding zinc it can get pretty gummy... and will clog up the grinding wheel so there will always be some zinc left in the metal where you will be welding... another option is acid etching the zinc off....

  5. Likes CAVEMANN liked this post
  6. #4
    Join Date
    Sep 2019
    Posts
    16
    Post Thanks / Like

    Re: Welding Zinc Question

    Thanks. I'll plan to do the work outside.

  7. #5
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,865
    Post Thanks / Like

    Re: Welding Zinc Question

    Quote Originally Posted by nicksorg View Post
    Good morning.
    From what I understand, welding Zinc can be deadly/dangerous. I need to make some shutter hangers. They are essentially a lag bolt with a small section of rod at the end that slides inside the shutter hinge. If I buy zinc coated lag bolt at Lowe's, can I grind the end and safely weld a piece of rod on it?
    Thanks
    Nick
    Yes you can. You won't likely even notice after grinding the zinc off a bolt head - barely smell it.

    Welding several beads on zinc coated flat steel is a different animal - it sucks.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  8. Likes ronsii, shovelon, CAVEMANN, farmall liked this post
  9. #6
    Join Date
    Feb 2021
    Posts
    1
    Post Thanks / Like

    Re: Welding Zinc Question

    Quote Originally Posted by ronsii View Post
    ... another option is acid etching the zinc off....
    For small things like bolts, I always use vinegar to remove zinc. 24h in vinear, and there is no more zinc to worrie about.

  10. Likes CAVEMANN liked this post

Posting Permissions