+ Reply to Thread
Page 2 of 4 FirstFirst 1234 LastLast
Results 26 to 50 of 84

Thread: Bird Nest

  1. #26
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    1,081
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Willie B View Post
    No, and it does not with the tip on until you strike an arc. With bigger wires (.035) it welds a while without a problem, squeeze the trigger, nothing happens.
    Okay. So, what happens, if you position the gun so the wire feeds out almost parallel to the work piece, while maintaining an arc?

  2. #27
    Join Date
    Mar 2015
    Posts
    658
    Post Thanks / Like

    Re: Bird Nest

    I had this experience once and it was the coating on the wire like the post said it was a thin coat of rust I know the wire is coated but moisture and dust & rust can build up on the wire causing the drive rolls and liner to get sticky or gummed up. Having burned a lot of 035 I am a firm believer in wipers and lube . We ran two wipers 1 with lube 1 dry you will be amazed at what comes off if that wire. Secondly I am not a firm believer in running oversized tips if you do they wear out fast and it changes your voltage setting

    I know there are arguments both ways just my 2 cents worth

  3. Likes Oscar liked this post
  4. #28
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    6,611
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Leogl View Post
    I had this experience once and it was the coating on the wire like the post said it was a thin coat of rust I know the wire is coated but moisture and dust & rust can build up on the wire causing the drive rolls and liner to get sticky or gummed up. Having burned a lot of 035 I am a firm believer in wipers and lube . We ran two wipers 1 with lube 1 dry you will be amazed at what comes off if that wire. Secondly I am not a firm believer in running oversized tips if you do they wear out fast and it changes your voltage setting

    I know there are arguments both ways just my 2 cents worth
    I would agree with what you said. Oversized tips will cause premature wear at best, erratic arc is more likely. I also use wipers with lube and haven't had issues. It really doesn't take much debris on the wire to cause major feed issues. The brand of wire itself can often be an issue. I've thrown more than a few spools of wire out over the years because they wouldn't feed correctly. It's almost impossible to get that through to someone who is inexperienced and sees it only as a roll of " wire". All in all its a simple process of diagnosis, and the best way to approach it is to start at simple and only change one variable at a time.

  5. #29
    Join Date
    Mar 2015
    Posts
    658
    Post Thanks / Like

    Re: Bird Nest

    Oversized tips will also cause wear in the liner because it isn’t centered like it is supposed to be

  6. #30
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Leogl View Post
    I had this experience once and it was the coating on the wire like the post said it was a thin coat of rust I know the wire is coated but moisture and dust & rust can build up on the wire causing the drive rolls and liner to get sticky or gummed up. Having burned a lot of 035 I am a firm believer in wipers and lube . We ran two wipers 1 with lube 1 dry you will be amazed at what comes off if that wire. Secondly I am not a firm believer in running oversized tips if you do they wear out fast and it changes your voltage setting

    I know there are arguments both ways just my 2 cents worth
    I agree. I use the same 2-wiper system. Lots of crud even on brand new wire.
    1st on WeldingWeb to have a scrolling sig!



  7. #31
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Weldordie View Post
    Okay. So, what happens, if you position the gun so the wire feeds out almost parallel to the work piece, while maintaining an arc?
    Gee, I don't know.

    Today I "welded" several hours. Meaning I cut, grinded, fitted, clamped & welded. The welder was at its best! Every weld was on 1/4" angle & flat. A generator base, not a real grueling test of a MIG welder. All afternoon, not a single birdnest!

    Pictures are of gussets I add, purely cosmetic. The generator has round corners, the bases I build are square. There would be a little triangular hole without these. I don't make a deliberate bevel to leave room for weld metal, I chamfer to clean up plasma dross.

    These are in awkward position, vertical up, and horizontal.

    Name:  MIGHT.jpg
Views: 536
Size:  175.7 KBName:  MIG.jpg
Views: 415
Size:  137.0 KB
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  8. #32
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,805
    Post Thanks / Like

    Re: Bird Nest

    What I was going to suggest is to clean all of the electrical contact surfaces, such as where the MIG gun attaches to the welder, etc. If you have any current problems that may be contributing.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  9. #33
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    9,896
    Post Thanks / Like

    Re: Bird Nest

    It looks fixed
    Do have photos of nest

    Dave

    Quote Originally Posted by Willie B View Post
    Gee, I don't know.

    Today I "welded" several hours. Meaning I cut, grinded, fitted, clamped & welded. The welder was at its best! Every weld was on 1/4" angle & flat. A generator base, not a real grueling test of a MIG welder. All afternoon, not a single birdnest!

    Pictures are of gussets I add, purely cosmetic. The generator has round corners, the bases I build are square. There would be a little triangular hole without these. I don't make a deliberate bevel to leave room for weld metal, I chamfer to clean up plasma dross.

    These are in awkward position, vertical up, and horizontal.

    Name:  MIGHT.jpg
Views: 536
Size:  175.7 KBName:  MIG.jpg
Views: 415
Size:  137.0 KB

  10. #34
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    5,898
    Post Thanks / Like

    Re: Bird Nest

    After 10 yrs. And all you had to do is admit there was an issue on WW.
    Last edited by tapwelder; 11-09-2020 at 01:08 PM.

  11. #35
    Join Date
    Oct 2014
    Posts
    5,270
    Post Thanks / Like

    Re: Bird Nest

    Glad it's working good. It looks like you could turn the heat up a bit.

  12. #36
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by tapwelder View Post
    After 10 yrs. And all you had to do is admit there was an issue on WW.
    I still haven't tried it with .023. I'd be surprised if that issue is cured. Wish there was a lube that'd not cause other problems.
    Last edited by Willie B; 11-09-2020 at 06:40 PM.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  13. #37
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Welder Dave View Post
    Glad it's working good. It looks like you could turn the heat up a bit.
    That was vertical up. I was pulsing. Photo posts sideways almost every time.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  14. #38
    Join Date
    Mar 2015
    Posts
    658
    Post Thanks / Like

    Re: Bird Nest

    I was going to suggest that you clean contacts also but since it is working go for it 1 more thing to check is your ground lead leads tend to take a beating in a shop getting pulled on etc we used to have to cut the clamp end off and redo the clamp the insides of it would be just black dust
    Contrary to popular believe leads do wear out especially on semi automatic processes

    Good luck

  15. #39
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Willie B View Post
    That was vertical up. I was pulsing. Photo posts sideways almost every time.
    So what was the cure?

  16. #40
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by 12V71 View Post
    So what was the cure?
    Don't exactly know. Second new liner this year, adjust the bottom roller alignment, spool off some wire through several birdnests. I can't say. I am perplexed that there seems nothing to do about the top roller adjustment. If the bottom roller was off, it was by thousandths.

    The less than a year old liner was discolored near the tip, but that I would have expected.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  17. #41
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Leogl View Post
    I was going to suggest that you clean contacts also but since it is working go for it 1 more thing to check is your ground lead leads tend to take a beating in a shop getting pulled on etc we used to have to cut the clamp end off and redo the clamp the insides of it would be just black dust
    Contrary to popular believe leads do wear out especially on semi automatic processes

    Good luck
    I did notice the ground clamp was hot several months ago. I bought a new one, but haven't gotten around to install it. I guess I will now.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  18. #42
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Willie B View Post
    I did notice the ground clamp was hot several months ago. I bought a new one, but haven't gotten around to install it. I guess I will now.
    I was going to look at the drive on my 252 today but was up to my armpits in a Kenworth ISX engine and forgot. It's been through millions of feet of .035 and .045 wire without any problems. I've changed one liner since 2016... but I'm the only one that runs it. The first improvement I made was to chuck the ground lead and tin clamp and replace it with 15' of 1/0 cable and a 500 amp Lenco clamp, yeah it's overkill but it doesn't get hot or arc.

  19. Likes ronsii liked this post
  20. #43
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    6,264
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by 12V71 View Post
    Check the wire you pull from the gun when you have these issues. I had an Esab 250 that had a bad connection to the gun connection block on the front of the machine and sent most of the weld current through the wire rather than the gun cable, It made small burns on the wire that were very hard to see and those burns would stick it tight in the contact tip.
    My inverter did that to me after sitting for a while, it uses DINSE connectors on the front for polarity & process swaps, it would have NO power & then the panel would jump to over 60 volts and send about 4 feet of wire out & then stop & do it all again over and over if you tried welding, all it took was a twist on the DINSE connector to secure the connection. I didn't look at the wire, but at the voltage it showed it would get red really quick & managed to get one trial across two fingers for a nice burn-------------------NOT!
    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    LET'S GO BRANDON!"INFLATION-THAT'S THE PRICE WE PAY FOR THOSE GOVERNMENT BENEFITS EVERYBODY THOUGHT WERE FREE."RONALD REAGAN
    JEFF

  21. Likes ronsii liked this post
  22. #44
    Join Date
    Apr 2010
    Posts
    2,963
    Post Thanks / Like

    Re: Bird Nest


    Willie B
    per Leogl

    Quote Originally Posted by Willie B View Post
    I did notice the ground clamp was hot several months ago . . .
    When I suggested 'clean all contacts', it included - but did not
    emphasize
    - the Ground Clamp.

    Before you reattach - cut the cable back 12/16" to guarantee
    fresh-meat . . .

    hth


    Opus



    .


  23. #45
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    & no, I hadn't considered the ground clamp until now. I always grind a clean spot for the ground clamp & shine up the contact on the clamp, but got to the service guy last week with only a scrap of grader blade quite rusty & no grinder with me. He had quite a hard time with birdnest too.

    Maybe that is the secret?
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  24. #46
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Willie B View Post
    That was vertical up. I was pulsing. Photo posts sideways almost every time.
    This forum, and many others on the same platform, has a problem with cell phone pictures taken with the phone held vertically (portrait orientation). There's a fix from what I've read on other forums. I started this thread on it, but it's not getting any traction.

    https://weldingweb.com/vbb/showthrea...05#post8775805
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  25. #47
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Leogl View Post
    Oversized tips will also cause wear in the liner because it isn’t centered like it is supposed to be
    On cheap chinese liners maybe. We are talking less than .005" on one side of the tip. Way closer than you would get with cheap chinese mig welders and torches.
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  26. Likes ronsii liked this post
  27. #48
    Join Date
    Jan 2020
    Posts
    62
    Post Thanks / Like

    Re: Bird Nest

    I've seen cheap imported wire cause problems like OP described. But sounds like hes got it cornered with the ground situation. Miller feeders imo have always been more "sensitive" to these kind of issues. If the arc is not initiating properly with a faulty ground, a bird nest is very possible to occur. Have you tested wire tension by spooling the wire into a gloved hand (with and without a tip). That would eliminate some variables. Start working backwards from there until you find the problem or get to the wire itself.

  28. #49
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,586
    Post Thanks / Like

    Re: Bird Nest

    Did try the bend the wire trick. Tighten the roller tension just enough to bend the wire. The wire is Maine OXY branded. They tell me hundreds of rolls have been run without complaints.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  29. #50
    Join Date
    Jun 2012
    Location
    Big Lake/Monticello MN
    Posts
    15,406
    Post Thanks / Like

    Re: Bird Nest

    Quote Originally Posted by Willie B View Post
    Did try the bend the wire trick. Tighten the roller tension just enough to bend the wire. The wire is Maine OXY branded. They tell me hundreds of rolls have been run without complaints.
    I've never actually used that one - I pinch the wire with my gloved hand and adjust until it can moderately push wire through but still slips without bird nesting when I stop it.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  30. Likes Rondo liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,296,902.61390 seconds with 22 queries