    Re: Welding Fixture Table

    That's turning into a really scary visual...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  2. Likes ronsii, Lis2323, 12V71, William McCormick liked this post
  3. #52
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by whtbaron View Post
    That's turning into a really scary visual...
    OK now that was funny!!!!!! almost can't stop laughing
    Last edited by ronsii; 01-19-2021 at 10:40 PM.

  4. Likes whtbaron, William McCormick liked this post
  5. #53
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    You guys are whack


    Sent from my iPhone using Tapatalk
    :

  6. Likes ronsii, whtbaron, William McCormick liked this post
  7. #54
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    4,252
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post
    You guys are whack


    Sent from my iPhone using Tapatalk
    When that table shows up, I'd suggest getting those latex blankets off of it real fast...
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  8. Likes ronsii, William McCormick liked this post
  9. #55
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by whtbaron View Post
    When that table shows up, I'd suggest getting those latex blankets off of it real fast...
    Good plan


    Sent from my iPhone using Tapatalk
    :

  10. Likes ronsii, whtbaron, William McCormick liked this post
  11. #56
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    4,252
    Post Thanks / Like

    Re: Welding Fixture Table

    Good thing you ordered when you did, it will probably double in price in the coming year.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  12. Likes ronsii, William McCormick liked this post
  13. #57
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Welding Fixture Table

    Quote Originally Posted by whtbaron View Post
    Good thing you ordered when you did, it will probably double in price in the coming year.


    No kidding!! It arrived at my freight forwarders in Blaine Wa last nite. (I guess Mac didn't get the payment to them in time ). LOL

    I might have it tomorrow or Monday after I pay taxes to Canada Border Services. That's always a joy......


    Sent from my iPhone using Tapatalk
    Last edited by Lis2323; 01-21-2021 at 03:54 PM.
    :

  14. #58
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    335
    Post Thanks / Like

    Re: Welding Fixture Table

    Darn it... oh well.... guess it wasn't that tired.
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  15. #59
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post
    No kidding!! It arrived at my freight forwarders in Blaine Wa last nite. (I guess Mac didn't get the payment to them in time ). LOL

    I might have it tomorrow or Monday after I pay taxes to Canada Border Services. That's always a joy......


    Sent from my iPhone using Tapatalk
    That's when you ask the texas guys to split your invoice in half..... and you simply show one to the BP at least that what I've heard people do when buying things from down here to go up there

  16. Likes William McCormick liked this post
  17. #60
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Welding Fixture Table

    Quote Originally Posted by ronsii View Post
    That's when you ask the texas guys to split your invoice in half..... and you simply show one to the BP at least that what I've heard people do when buying things from down here to go up there
    No way. These guys Google everything. If there’s a big discrepancy they “reassess” the value.

    Plus I never argue with someone with a gun. The women agents are the meanest!!!!


    Sent from my iPad using Tapatalk
    Last edited by Lis2323; 01-21-2021 at 09:31 PM.
    :

  18. Likes ronsii, William McCormick liked this post
  19. #61
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post
    No way. These guys Google everything. If there’s a big discrepancy they “reassess” the value.

    Plus I never argue with someone with a gun. The women agents are the meanest!!!!


    Sent from my iPad using Tapatalk
    So much for the good old days... I can remember several customers I had..... er... I mean a friend of mine had from up north every year they'd come down and spend a few grand and like clockwork they would have my friend make up two invoices for half the amount each...

  20. Likes Lis2323, William McCormick liked this post
  21. #62
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Welding Fixture Table

    I especially like this little detail.....



    Square tube shelf shelf support for the expanded metal affording smooth slide out of “stuff”.

    Plus it appears the square tube has the fuller radiused edges which matches the pipe legs nicely.
    Last edited by Lis2323; 01-22-2021 at 10:31 AM.
    :

  22. Likes ronsii, tackit, William McCormick liked this post
  23. #63
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Welding Fixture Table

    My table arrived. It must have taken one guy at least a day to prep for shipping as it took me a couple of hours to just REMOVE the wrapping.






    A close up of the intermediate shelf....




    At least ronsii shouldn’t be whining about the color.
    :

  24. #64
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    335
    Post Thanks / Like

    Re: Welding Fixture Table

    Good looking table...

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  25. Likes ronsii liked this post
  26. #65
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Fixture Table



    It does have a very nice look to it especially the intermediate shelf



    It's just....just..... BEAUTIFUL!!!!!!!

  27. Likes William McCormick liked this post
  28. #66
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Mac's Crew View Post
    Good looking table...

    Sent from my SM-G960U using Tapatalk
    Thanks Mac!


    Sent from my iPhone using Tapatalk
    :

  29. #67
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by ronsii View Post


    It does have a very nice look to it especially the intermediate shelf



    :
    Yeah me too. Somewhat whimsical, definitely extravagant and impractical.

    The perfect touch for a welding table. LOL.


    Sent from my iPhone using Tapatalk
    :

  30. Likes ronsii liked this post
  31. #68
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    576
    Post Thanks / Like

    Re: Welding Fixture Table

    That shore is purdy!
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  32. Likes William McCormick liked this post
  33. #69
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    4,252
    Post Thanks / Like

    Re: Welding Fixture Table

    She's a beauty, but you're going to cry when the first welding beads stick to it. I like it. A "Lincoln" decal opposite the brand logo would look good too. Glad you got the rubber sheets disposed of before Ronsii and Sid got there. I was also drooling over the forklift a little... working on my table for a while yesterday with the engine hoist I found out that isn't the safest way to be flipping around something heavy. Might have to build a quick disconnect for the CAT and get some pallet forks for it too.
    Last edited by whtbaron; 01-23-2021 at 10:39 AM.
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  34. Likes Lis2323, ronsii, William McCormick liked this post
  35. #70
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    I bought that Yale forklift used over 30 years ago.

    6000 Lb capacity, sideshift, auto trans, little Mitsubishi diesel, free lift mast and wide solid front tires. It’s had regular maintenance, a couple of batteries and finally a new starter just last month.

    $8500 (initial purchase price) + maintenance divided by 30 years = around $400 per year. Doesn’t owe me a thing.


    Sent from my iPad using Tapatalk
    :

  36. Likes ronsii, whtbaron, William McCormick liked this post
  37. #71
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,630
    Post Thanks / Like

    Re: Welding Fixture Table

    Just all my work just did not fit tables.
    What I use was a transit and shiming the saw horse.
    I all ways want build saw horse with screw adjustments.

    FYI concrete floors are not leave

    Dave

    Quote Originally Posted by Lis2323 View Post
    I had been planning on building a new welding table for quite some time. I had a pretty good idea of how it should be but was (as usual) struggling somewhat with logistics.

    Since discovering the thread started by Rustyshackleford (Brett) I have been working with John from Texas Metal Works on a custom table with some unique features.

    I’m usually the type to build things myself but in this case.....My cost for locally laser cutting the pieces alone would have been considerably more than my entire purchase price having John build it.

    It has been a several month process incorporating my ideas into a buildable product from a manufacturing standpoint and John has been very patient with me. Hopefully my input will result in future welding table options/upgrades available from Texas Metal Works.

    Here are a few random photos taken during construction. The table size without extensions is 40” x 80” with a 1/4” table top braced from the underside to achieve and maintain flatness.

    A photo of underside. Note the 2inch square holes at each corner of the table. These line up with the oversized 3” square tube legs I specified to accommodate the 2.5” receiver tubing for four vertical receivers.




    Bolt on plates with custom slots to accommodate vertical receivers ...



    Heavy 11 gauge center mounted drawer with industrial slides ...



    To be continued.......


    Sent from my iPad using Tapatalk

  38. Likes whtbaron, William McCormick liked this post
  39. #72
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    UHMW tape ..








    for the sliding clamp rack


    with soft close slides.





    Sent from my iPad using Tapatalk
    :

  40. #73
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    375
    Post Thanks / Like

    Re: Welding Fixture Table

    Damn you/they of every thing.

  41. Likes whtbaron, ronsii, William McCormick liked this post
  42. #74
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,630
    Post Thanks / Like

    Re: Welding Fixture Table

    I like all Vise-Grips

    Dave

    Quote Originally Posted by Lis2323 View Post
    UHMW tape ..








    for the sliding clamp rack


    with soft close slides.





    Sent from my iPad using Tapatalk

  43. Likes William McCormick liked this post
  44. #75
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,357
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by smithdoor View Post

    FYI concrete floors are not leave

    Dave
    I got them to install adjustable self leveling swivel pads in lieu of casters.





    Sent from my iPhone using Tapatalk
    :

  45. Likes whtbaron, ronsii, William McCormick liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,380,861.01729 seconds with 13 queries