    Welding Fixture Table

    I had been planning on building a new welding table for quite some time. I had a pretty good idea of how it should be but was (as usual) struggling somewhat with logistics.

    Since discovering the thread started by Rustyshackleford (Brett) I have been working with John from Texas Metal Works on a custom table with some unique features.

    Iím usually the type to build things myself but in this case.....My cost for locally laser cutting the pieces alone would have been considerably more than my entire purchase price having John build it.

    It has been a several month process incorporating my ideas into a buildable product from a manufacturing standpoint and John has been very patient with me. Hopefully my input will result in future welding table options/upgrades available from Texas Metal Works.

    Here are a few random photos taken during construction. The table size without extensions is 40Ē x 80Ē with a 1/4Ē table top braced from the underside to achieve and maintain flatness.

    A photo of underside. Note the 2inch square holes at each corner of the table. These line up with the oversized 3Ē square tube legs I specified to accommodate the 2.5Ē receiver tubing for four vertical receivers.




    Bolt on plates with custom slots to accommodate vertical receivers ...



    Heavy 11 gauge center mounted drawer with industrial slides ...



    To be continued.......


    Sent from my iPad using Tapatalk
    :

  2. #2
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    387
    Post Thanks / Like

    Re: Welding Fixture Table

    Nice little table

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  3. Likes William McCormick liked this post
  4. #3
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Mac's Crew View Post
    Nice little table

    Sent from my SM-G960U using Tapatalk
    I hope so. It just came out of the powder coat shop today. With a little luck they will ship early next week. Iím not holding my breath for a delivery date. Itís a long way from Texas to BC.


    Sent from my iPad using Tapatalk
    :

  5. Likes William McCormick liked this post
  6. #4
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    387
    Post Thanks / Like

    Re: Welding Fixture Table

    Well if it needs to rest for a couple years, I can give you my addy.

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  7. Likes leightrepairs, William McCormick liked this post
  8. #5
    Join Date
    Aug 2018
    Location
    'ta town, KS
    Posts
    387
    Post Thanks / Like

    Re: Welding Fixture Table

    It is a long trip. HeHe

    Sent from my SM-G960U using Tapatalk
    I haven't built anything I can't throw away. Perfection is the journey.

    Mac

  9. Likes William McCormick liked this post
  10. #6
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Mac's Crew View Post
    Well if it needs to rest for a couple years, I can give you my addy.

    Sent from my SM-G960U using Tapatalk



    Sent from my iPad using Tapatalk
    :

  11. Likes William McCormick liked this post
  12. #7
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Re: Welding Fixture Table

    This is a pic of my welding table base (sitting on a welding table).

    I opted to delete the casters and add cross bracing to accommodate moving the table with a pallet jack. Adjustable height swivel pads will replace the casters and allow for levelling the table.

    The lower bracing also allowed for extra storage area. Initially I planned on two powder coated MDF panels mounted flush with the crossmembers so stuff could slide out easily but John from Texas Metals suggested black HDPE panels which dropped right in the cross bracing.

    No painting necessary or dealing with inevitable scratching. Plus totally moisture resistant.




    I had John laser cut and pedestal mount an intermediate shelf for storing sh*t but mainly for interest and aesthetics. Even had matching holes cut (but a few thou in diameter larger to allow for the paint).



    View from the underside of intermediate shelf showing streamlined gussets for the suspended pedestal look.





    And hereís a pic of the base with its special BLUE multi-coat powder process....




    Sent from my iPad using Tapatalk
    :

  13. #8
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,838
    Post Thanks / Like

    Re: Welding Fixture Table

    Wow... that's going to look bright, even in your shop where there's a lot of shiny and bright. Sweeet...
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  14. Likes ronsii, William McCormick liked this post
  15. #9
    Join Date
    Apr 2007
    Location
    Portland, OR
    Posts
    121
    Post Thanks / Like

    Re: Welding Fixture Table

    Are you up for sharing cost prior to shipping?

    Looks great!
    Miller Syncrowave 180SD

  16. Likes William McCormick liked this post
  17. #10
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by slodat View Post
    Are you up for sharing cost prior to shipping?

    Looks great!
    If it helps. Keep in mind tables are shipped assembled.

    Might not be applicable as truck freight is based on deck space used. Unless they are able to double stack.


    Sent from my iPhone using Tapatalk
    :

  18. Likes ronsii, William McCormick liked this post
  19. #11
    Join Date
    Apr 2007
    Location
    Portland, OR
    Posts
    121
    Post Thanks / Like

    Re: Welding Fixture Table

    Iíve been looking at the 28mm tables from Build Pro and Seigmond. Interested in other options.
    Miller Syncrowave 180SD

  20. Likes William McCormick liked this post
  21. #12
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Welding Fixture Table

    I wanted mine nitrided but apparently no one in North America has tanks big enough.

    Most are done in Europe and Asia.




    Sent from my iPhone using Tapatalk
    :

  22. #13
    Join Date
    Mar 2011
    Location
    Western Washington
    Posts
    10,551
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post
    This is a pic of my welding table base (sitting on a welding table).

    I opted to delete the casters and add cross bracing to accommodate moving the table with a pallet jack. Adjustable height swivel pads will replace the casters and allow for levelling the table.

    The lower bracing also allowed for extra storage area. Initially I planned on two powder coated MDF panels mounted flush with the crossmembers so stuff could slide out easily but John from Texas Metals suggested black HDPE panels which dropped right in the cross bracing.

    No painting necessary or dealing with inevitable scratching. Plus


    And here’s a pic of the base with its special BLUE multi-coat powder process....




    Sent from my iPad using Tapatalk
    It's BEAUTIFUL!!!!!!!

  23. Likes William McCormick liked this post
  24. #14
    Join Date
    Dec 2018
    Posts
    6,505
    Post Thanks / Like

    Re: Welding Fixture Table

    GAWD THAT'S NICE!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!

  25. Likes William McCormick liked this post
  26. #15
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    3,176
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post

    A photo of underside. Note the 2inch square holes at each corner of the table. These line up with the oversized 3Ē square tube legs I specified to accommodate the 2.5Ē receiver tubing for four vertical receivers.



    It took a couple of seconds trying to figure this sentence out. At first, I couldn't see how you would drop 2-1/2" receiver tune into a 2" hole.

    I assume/remembered from some of your pics that you have a long section of 2" tube with a small collar of 2-1/2" tube welded to the outside to act as stop when you drop in into the hole. I am still on my first cup of coffee so I am a bit slow right now.
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  27. Likes William McCormick liked this post
  28. #16
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Welding Fixture Table

    Quote Originally Posted by psacustomcreations View Post
    It took a couple of seconds trying to figure this sentence out.
    .
    Sorry Pat you're right. My attempt at describing the vertical receiver setup was unnecessarily wordy. You have probably noticed I have a bad habit of doing that ...

    IMO vertical receivers in the workplace are just so underrated. Their uses are only limited to one's imagination and the best part is they don't take up ANY valuable space.

    Here's an elevated offset swivel work table.




    Sent from my iPhone using Tapatalk
    Last edited by Lis2323; 01-08-2021 at 10:39 AM.
    :

  29. #17
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,838
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by ronsii View Post
    It's BEAUTIFUL!!!!!!!
    And I thought you were going to whine about the color looking more purple than Miller blue....
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  30. #18
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    494
    Post Thanks / Like

    Re: Welding Fixture Table

    Amazing

  31. Likes ronsii, William McCormick liked this post
  32. #19
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by whtbaron View Post
    And I thought you were going to whine about the COLOUR (color) looking more purple than Miller blue....
    Donít you find it amusing how we deliberately misspell words so that we donít look like high school dunces to our American friends?


    Sent from my iPad using Tapatalk
    :

  33. Likes whtbaron, ronsii, William McCormick liked this post
  34. #20
    Join Date
    Sep 2013
    Posts
    1,715
    Post Thanks / Like

    Re: Welding Fixture Table

    Really amazing and I can't wait to see it in place, nestled comfortably amongst all your other goodies.

    I keep saying I'm going to rent a mag drill so I can make some holes in my bench. Gotta clean it first, though.

  35. Likes ronsii, Lis2323, William McCormick liked this post
  36. #21
    Join Date
    Feb 2015
    Location
    Texas
    Posts
    298
    Post Thanks / Like

    Re: Welding Fixture Table

    That is a work of art Lis! Actually, from the photos you’ve posted your whole shop is a work of art! I’ve tried to keep a neat shop but usually after a full day I’m so worn out and sore the last thing I want to do is sweep up the shop.
    Miller 350 Dynasty
    Miller Trailblazer
    Miller 625 Plasma

    Lincoln Power MIG
    Victor oxy/acetylene
    Hyperthem 85

  37. #22
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    5,838
    Post Thanks / Like

    Re: Welding Fixture Table

    Quote Originally Posted by Lis2323 View Post
    Don’t you find it amusing how we deliberately misspell words so that we don’t look like high school dunces to our American friends?


    Sent from my iPad using Tapatalk
    I've actually gotten so tired of Spelchek telling me I've spelled things wrong when I really spelled them right, that I've kind of joined them... I'm only 27 miles from the border...
    The harder you fall, the higher you bounce...

    250 amp Miller DialArc AC/DC Stick
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  38. Likes ronsii, William McCormick liked this post
  39. #23
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    494
    Post Thanks / Like

    Re: Welding Fixture Table

    Lis2323
    Your ears burning? I was at my LWS and a local company makes fixture tables. The sales man saw me standing there and put the press on. Damn they are neat

  40. Likes William McCormick liked this post
  41. #24
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    6,039
    Post Thanks / Like

    Welding Fixture Table

    Quote Originally Posted by Reebz View Post
    Lis2323
    Your ears burning? I was at my LWS and a local company makes fixture tables. The sales man saw me standing there and put the press on. Damn they are neat
    You guys are fortunate. In my area youíre lucky if an LWS even has a welding machine on their showroom floor.

    That is a bit of an exaggeration of course but not by much....

    Whatís the plan? Acorn table? Build a fixture table?


    I think my table is being shipped today.
    :

  42. Likes William McCormick liked this post
  43. #25
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    494
    Post Thanks / Like

    Re: Welding Fixture Table

    My LSW is pretty nice.

    Still no plan on a table. I'm going to look at the those down the road I told you about. I do have this plan, no more gym equipment or I'm going to charge what I should charge. If they walk they walk. I try and stay under "Rogues fitness" price but I can not compete with a robot. If I lose work fine, I can work on the old car, do art and furniture. If I do art and furniture I'm will drop insurance. Plus the "maker space looks like its going to happen. I sold $22,000 worth of gym equipment but really did not net enough to amount to much. RANT OVER lol. I may send a PM about the art furniture world.

  44. Likes ronsii, William McCormick liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,642,817,116.76302 seconds with 12 queries