    I need a blanket

    Until my workshop is complete, I only have a 12' x 16' man cave (which can be described as rough and ready) where the interior walls are a mix of herringbone 1x6's, hardiebacker around the wood stove and some OSB on the walls. Concrete floor.


    So rather then tear everything apart to spark proof, my plan is, using welding curtains, to create a 4 sided work area . But which ones?


    There's vermiculite coated fiberglass, various straight fiberglass with differing finishing processs and carbon fiber felt.


    My main concern is to not buy something that will shed and ptotentially cause skin and lung irritation.


    Any experience that can be shared using blankets for a similar purpose appreciated.
    Attached Images Attached Images  

  2. #2
    Join Date
    Jan 2016
    Location
    northeast USA
    Posts
    11,394
    Post Thanks / Like

    Re: I need a blanket

    cheapest and safest is throw up some 1/2 drywall, tape and spackle the seams..spark and mildly fire proof and safe to work around...

  3. Likes Broccoli1, ronsii, walker, N2 Welding liked this post
  4. #3
    Join Date
    Dec 2020
    Posts
    24
    Post Thanks / Like

    Re: I need a blanket

    Quote Originally Posted by Hobbytime View Post
    cheapest and safest is throw up some 1/2 drywall, tape and spackle the seams..spark and mildly fire proof and safe to work around...
    Thanks Hobbytime. I'll give it serious consideration. It's just that I was hoping to find a simple solution.

  5. #4
    Join Date
    Dec 2018
    Posts
    4,946
    Post Thanks / Like

    Re: I need a blanket

    Any welding blanket I've ever owned sheds fibers. They get worse with age. I hate them, but they do serve a purpose.

  6. Likes 12V71, Lemarque liked this post
  7. #5
    Join Date
    Oct 2019
    Location
    Australia
    Posts
    249
    Post Thanks / Like

    Re: I need a blanket

    There's chrome leather welding blankets and there's also the good old plastic welding curtains - the green or red ones that protect against flashing. None of these shed and are fairly inexpensive and are good for other purposes like wind shielding outside etc. Easy to fold up and put away. Both come with eyelets to hang as a curtain or tie to a frame.

  8. Likes ronsii, Hobbytime, Lemarque liked this post
  9. #6
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,203
    Post Thanks / Like

    Re: I need a blanket

    It doesn’t get simpler, or cheaper than throwing up drywall. Another option would be to use sheets of 20 gauge galvanized steel. The plastic screens do not stop fire.

  10. Likes Hobbytime, Lemarque liked this post
  11. #7
    Join Date
    Dec 2020
    Posts
    24
    Post Thanks / Like

    Re: I need a blanket

    OK then.

    Drywall or plywood it is.

    Gonna take some time moving stuff (alot of stuff) from one area to another but "So it is written, so it shall be".

    Thanks for all the feedback.

  12. #8
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,203
    Post Thanks / Like

    Re: I need a blanket

    Not plywood! Drywall or steel sheets are fire resistant at worst, where plywood is will readily burn.

  13. #9
    Join Date
    Dec 2020
    Posts
    24
    Post Thanks / Like

    Re: I need a blanket

    Quote Originally Posted by walker View Post
    Not plywood! Drywall or steel sheets are fire resistant at worst, where plywood is will readily burn.
    If I must.

  14. #10
    Join Date
    Dec 2020
    Posts
    24
    Post Thanks / Like

    Re: I need a blanket

    Quote Originally Posted by tackit View Post
    The daughter is getting a brake job on her Ford Fusion, $600, I told the SIL it's not safe to drive on the roads anymore, especially now that no jobs Biden is president.
    The point being?
    Attached Images Attached Images  

  15. Likes walker liked this post
  16. #11
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,064
    Post Thanks / Like

    Re: I need a blanket

    The cement board used for tile backing for walls and floors is worth considering. Cheap enough, moisture resistant and should be sturdier than Sheetrock.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  17. Likes ronsii, farmall liked this post
  18. #12
    Join Date
    Dec 2020
    Posts
    24
    Post Thanks / Like

    Re: I need a blanket

    Quote Originally Posted by Oldendum View Post
    The cement board used for tile backing for walls and floors is worth considering. Cheap enough, moisture resistant and should be sturdier than Sheetrock.
    Thanks. I resemble your handle

    I do use cement board on the walls around my old wood stove in the shed. Probably backup my Klutch welding table with some and put one of my work benches behind it.

  19. #13
    Join Date
    Aug 2009
    Posts
    4,228
    Post Thanks / Like

    Re: I need a blanket

    Cement board is far better than sh1t3rock and also used for making home shop coating ovens (I've a pile awaiting motivation so I can Cerakote motorcycle exhausts with their high temp coating).

  20. #14
    Join Date
    May 2011
    Posts
    467
    Post Thanks / Like

    Re: I need a blanket

    Drywall is the cheapest, concrete board is better.

    You can buy rolls of welding curtain online pretty cheap. I got a 6' x 100' roll of yellow see through for like $3 a foot.

    If you want a real expensive way, I have 4' x 6' leather welding blankets that I use in industrial food plants, they cant have any fibers floating there. They are over $100 each.

    Sent from my SM-G960U using Tapatalk

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,623,583,267.93171 seconds with 14 queries