    Bought one of these little China inverter welders just to see what they are about. I must admit that so far I am pretty amazed. I used it to build some mounts for the front end loader I put on a tractor of mine. Burnt several 3/32" 6013 rods. I have no doubt it will burn 1/8" rods OK too. For less than $100 it is nice and portable. Sometimes I just can't get to my old transformer welder in the shop.
    Name:  IMG_20210208_165251682a.jpg
Views: 1119
Size:  102.8 KB
    Name:  IMG_20210203_150105017.resized.jpg
Views: 1117
Size:  194.4 KB
    Name:  IMG_20210203_150217147.resized.jpg
Views: 1121
Size:  204.8 KB
    Craftsman 230/140 AC/DC Miller HF-251D-1
    Millermatic 130 Linclon 40 amp plasma cutter
    Hypertherm Max 20 O/A cutting and welding stuff
    5HP Ingersoll air compressor

  2. #2
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Yeap, I still have my Tooliom 135S 4lb inverter stick welder. It will run 1/8" 6011s, and just barely enough grunt for 1/8" 7018s @ ~112-115A. Cute lil bugger. Is yours on 120V or 240V?
    1st on WeldingWeb to have a scrolling sig!



  3. Likes ronsii liked this post
  4. #3
    Join Date
    Mar 2015
    Location
    NW Florida
    Posts
    78
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Mine is 240 volt. I have a 10,000 watt generator I can hang off the back of my tractor so I can weld anywhere on my property.
    Craftsman 230/140 AC/DC Miller HF-251D-1
    Millermatic 130 Linclon 40 amp plasma cutter
    Hypertherm Max 20 O/A cutting and welding stuff
    5HP Ingersoll air compressor

  5. #4
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Yea, they do become quite gut-less on 120V because the arc voltage really shoots down. On 240V, they're not all that bad for basic portable welding.

    1st on WeldingWeb to have a scrolling sig!



  6. Likes ronsii, hdonly0 liked this post
  7. #5
    Join Date
    Mar 2015
    Location
    NW Florida
    Posts
    78
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    In between all the rain and cold, I got my loader on the tractor. Little "Baby Welder" did a surprising good job.
    Name:  IMG_20210211_154910453.jpg
Views: 998
Size:  103.4 KB
    Name:  IMG_20210211_154930517.jpg
Views: 1008
Size:  137.1 KB
    Craftsman 230/140 AC/DC Miller HF-251D-1
    Millermatic 130 Linclon 40 amp plasma cutter
    Hypertherm Max 20 O/A cutting and welding stuff
    5HP Ingersoll air compressor

  8. Likes R&I, Shootr liked this post
  9. #6
    Join Date
    Feb 2021
    Posts
    24
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Is that a 600 or a 800...love those things!...Michael

  10. #7
    Join Date
    Mar 2015
    Location
    NW Florida
    Posts
    78
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by R&I View Post
    Is that a 600 or a 800...love those things!...Michael
    It is an NAA/ 1953 Jubilee. I have a 1960 651 Workmaster also.
    Name:  P1301312.resized.JPG
Views: 969
Size:  267.4 KB
    Craftsman 230/140 AC/DC Miller HF-251D-1
    Millermatic 130 Linclon 40 amp plasma cutter
    Hypertherm Max 20 O/A cutting and welding stuff
    5HP Ingersoll air compressor

  11. Likes R&I liked this post
  12. #8
    Join Date
    Jan 2005
    Posts
    5,184
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by Oscar View Post
    Yea, they do become quite gut-less on 120V because the arc voltage really shoots down. On 240V, they're not all that bad for basic portable welding.

    The little bit better 120 volt China inverters do quite well on 120 volts.. I liked the little Ironton from Northern tool.. You can't throw all the machines in the same boat on 120 volts..The very bottom feeders do suffer on 120 volts.. If you stick with 3/32 rod in 7018, some run the same as on 240 volts..
    Blue Demon 140 MSI
    Blue Demon 200 AC/DC
    Esab 160i caddy
    Esab CV353
    INE 1500
    Lincoln 250 Idealarc
    Thermal LM-200
    Thermal 60i- 3phase
    Thermal 15c
    Topshak 40 plasma
    Miller Regency 200/LN-72
    Viking 250 mig/2410 feeder
    Weldcote 140

  13. #9
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by Brand X View Post
    The little bit better 120 volt China inverters do quite well on 120 volts.. I liked the little Ironton from Northern tool.. You can't throw all the machines in the same boat on 120 volts..The very bottom feeders do suffer on 120 volts.. If you stick with 3/32 rod in 7018, some run the same as on 240 volts..
    Mine runs a little cooler on 120V, but it still runs well.
    1st on WeldingWeb to have a scrolling sig!



  14. Likes ronsii liked this post
  15. #10
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    1,029
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Some of the little 160 amp category 120/240 units with PFC do a nice job on all electrodes 5/32 and under on 240v. 1/8 and under on 120v.. Very impressive on extension cords and genertors even on 120v.
    Thermal Arc 320SP ( Lorch )
    Cobra Pythons
    Thermal Arc 300 AC/DC ( Sanrex )
    ESAB 301i AC/DC ( Lorch )
    Thermal Arc 161STL ( WTL )
    Thermal Arc 190S ( Sanrex )
    Cut Master 82, 42. Cut45 ( WTL )
    Victor Gas Apps.
    Boxes and boxes of welding crap.

  16. #11
    Join Date
    Jan 2005
    Posts
    5,184
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    I have yet to find one better then my 240 only small INE unit.. It a step above the Thermal 161s for sure..Jim, has one, and it a lot nicer then his Esab 161i He also had my Old Sanrex TS-160,The Thermal does not have the output of the Esab on 120 volts, but it's still a better machine running both with 3/32 7018 rod.. I am still shocked how some of the cheaper 120 volt only China machines run.. I think my Thermal LM-200 still might be my favorite,very easy to set the arc force for major differences in the arc type. having a 0-100 scale is simple, and effective. It's pretty much the same as a MST-400, just less output, and better with smaller wires
    Blue Demon 140 MSI
    Blue Demon 200 AC/DC
    Esab 160i caddy
    Esab CV353
    INE 1500
    Lincoln 250 Idealarc
    Thermal LM-200
    Thermal 60i- 3phase
    Thermal 15c
    Topshak 40 plasma
    Miller Regency 200/LN-72
    Viking 250 mig/2410 feeder
    Weldcote 140

  17. #12
    Join Date
    Jul 2018
    Location
    Cumbria, UK
    Posts
    2,220
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    My uncle bought one very similar to the one in the OP. It didn't even have an earth wire.

    He used it for roughly 2kg of rods before it died the other day.

    You get what you pay for...
    Murphy's Golden Rule: Whoever has the gold, makes the rules.

  18. #13
    Join Date
    Feb 2021
    Posts
    24
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by hdonly0 View Post
    It is an NAA/ 1953 Jubilee. I have a 1960 651 Workmaster also.
    Name:  P1301312.resized.JPG
Views: 969
Size:  267.4 KB
    I have a 1955 860 that was used(hard) at a junkyard....took some work to bring it back from the dead but boy they are handy!! I got lucky and got the live pto...

    What is that on the back of your NAA?

  19. #14
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by Munkul View Post
    My uncle bought one very similar to the one in the OP. It didn't even have an earth wire.

    He used it for roughly 2kg of rods before it died the other day.

    You get what you pay for...
    Yup, it almost always holds true!
    1st on WeldingWeb to have a scrolling sig!



  20. Likes Munkul liked this post
  21. #15
    Join Date
    Mar 2015
    Location
    NW Florida
    Posts
    78
    Post Thanks / Like

    Re: Baby Chinese Inverter Welders

    Quote Originally Posted by R&I View Post
    I have a 1955 860 that was used(hard) at a junkyard....took some work to bring it back from the dead but boy they are handy!! I got lucky and got the live pto...

    What is that on the back of your NAA?
    That's my "Baby Backhoe"Name:  Done.resized.jpg
Views: 843
Size:  82.0 KB
    Craftsman 230/140 AC/DC Miller HF-251D-1
    Millermatic 130 Linclon 40 amp plasma cutter
    Hypertherm Max 20 O/A cutting and welding stuff
    5HP Ingersoll air compressor

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,245,303.05389 seconds with 22 queries