    Advice Fume Extractor

    I want to get a fume extractor for my garage. Space is a premium my LWS sells The Miller FILTAIR 130. Any one use one. The garage door open and fan at the other end is not getting it done, plus its cold as hell.

  2. #2
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,139
    Post Thanks / Like

    Re: Advice Fume Extractor

    I have a coppus. The small ones are really for specification locations. Kinda a pain to move to every joint you weld, but works. I use it onsite. In addition to an extractor you might consider an air scrubber.

  3. #3
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,337
    Post Thanks / Like

    Re: Advice Fume Extractor

    I just sold my Miller 130 Filtair lately......





    and use the blue Covid masks they hand out free at the grocery store.


    Sent from my iPhone using Tapatalk
    :

  4. #4
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    370
    Post Thanks / Like

    Re: Advice Fume Extractor

    Lis2323
    Did you like the Miller 130 Filtair?
    I'm going to try the covid mask. I'm making 2500 brackets and will have a lot of hood time.

  5. #5
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,337
    Post Thanks / Like

    Re: Advice Fume Extractor

    Quote Originally Posted by Reebz View Post
    Lis2323
    Did you like the Miller 130 Filtair?
    I'm going to try the covid mask. I'm making 2500 brackets and will have a lot of hood time.
    The 130 Filtair worked fine. I would prefer a bigger fixed unit with a large overhead swinging extraction tube though. Being “portable” just means it takes up more room.

    You could most likely wall mount the unit if your welding bench is always in the same area though.

    I purchased it new “out of box” off eBay several years ago for a really good price so I certainly didn’t lose money on the deal.


    Sent from my iPad using Tapatalk
    :

  6. #6
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    370
    Post Thanks / Like

    Re: Advice Fume Extractor

    I understand. I may fix it to a wall or hand from the ceiling. Just working in a 2 car garage which I share with my hobby car, space is a premium to say the least.

  7. #7
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,337
    Post Thanks / Like

    Re: Advice Fume Extractor

    Do some research and see who makes that unit for Miller. Like everything else you are paying for the name.

    That model would be easy to wall mount. Just unscrew the casters and put it on a shelf.


    Sent from my iPhone using Tapatalk
    :

  8. Likes Reebz liked this post
  9. #8
    Join Date
    Dec 2015
    Location
    Kentucky
    Posts
    319
    Post Thanks / Like

    Re: Advice Fume Extractor

    Has anyone ever took one apart to see how its made or what it would take to build there own.

  10. #9
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,139
    Post Thanks / Like

    Re: Advice Fume Extractor

    Quote Originally Posted by Ky farmer View Post
    Has anyone ever took one apart to see how its made or what it would take to build there own.
    Yeah. Easy enough. Aside from brand. Filter sets are much of the expense. Portable are for a specific task. Not really permanent or home shop friendly. Pretty annoying if you weld a project with lots of weld locations.

  11. Likes Reebz liked this post
  12. #10
    Join Date
    Sep 2013
    Posts
    1,492
    Post Thanks / Like

    Re: Advice Fume Extractor

    How about using a standard shop vac with a HEPA filter installed? The fumes we don't like to breathe are basically the visible particulates (what causes the smoke to be seen by the naked eye) and certain to be captured by a standard vacuum with a good filter. You could even build a box to hold a second filter inline somewhere if you wanted more protection.

    I visited a shop last year that had a very "simple" solution that amounted to nothing more than a 6" flexible duct that ran from the work table to the wall where there was a standard exhaust fan built in. He'd wired an on/off switch right at the bench so it was easy to turn the fan on when you were positioning things. No filtration needed since the fan got the smoke up and out of the building rather than exhausting into the building.

  13. Likes Reebz liked this post
  14. #11
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    574
    Post Thanks / Like

    Re: Advice Fume Extractor

    Shop vac would not be the right kind of fan for this. They are high suction but low volume. You want to move a higher volume of air but not with a lot of suction power for this. It is more like ventilation than vacuuming stuff. A furnace fan/squirrel cage would be more the type. Just find or buy one of those and add a filter as desired, but be careful the filter is not going to catch a spark and smolder.
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

  15. #12
    Join Date
    Oct 2014
    Posts
    3,526
    Post Thanks / Like

    Re: Advice Fume Extractor

    Shop vac's don't work good as fume extractors and can catch on fire. Maybe all you need is an exhaust fan. The Marley Power Cat has hose that can be connected to it.

    https://www.electricheaterwarehouse....AC_p_1603.html

  16. #13
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    370
    Post Thanks / Like

    Re: Advice Fume Extractor

    I run fans and got a fume extractor. LOL

  17. #14
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,337
    Post Thanks / Like

    Re: Advice Fume Extractor

    Quote Originally Posted by Reebz View Post
    I run fans and got a fume extractor. LOL
    Reebz what did you end up using for an extractor?


    Sent from my iPad using Tapatalk
    :

  18. #15
    Join Date
    Nov 2019
    Location
    North East Ohio
    Posts
    370
    Post Thanks / Like

    Re: Advice Fume Extractor

    I got the miller product, pricey but my LWS stands behind everything they sell. "My nose clean out" is much better, gross but fact.

  19. #16
    Join Date
    Aug 2014
    Location
    B.C. Canada
    Posts
    4,337
    Post Thanks / Like

    Re: Advice Fume Extractor

    Quote Originally Posted by Reebz View Post
    I got the miller product, pricey but my LWS stands behind everything they sell. "My nose clean out" is much better, gross but fact.
    Good choice.


    Sent from my iPhone using Tapatalk
    :

  20. Likes Reebz liked this post
  21. #17
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    574
    Post Thanks / Like

    Re: Advice Fume Extractor

    In addition to the ventilation - It is still worth wearing a respirator under your hood, especially for the messier processes like MIG and stick. I always felt queasy after MIG welding a bit in my garage until I started doing that. TIG I don't do it, even though I know I probably should, especially on SS.
    -Dave
    XMT304 with: 22A Feeder, or HF251 Hi Freq DC TIG air cooled

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,623,866,134.75824 seconds with 14 queries