+ Reply to Thread
Results 1 to 2 of 2

Thread: Powcon 300sm remote weld power

  1. #1
    Join Date
    Dec 2020
    Location
    UK
    Posts
    3
    Post Thanks / Like

    Powcon 300sm remote weld power

    Hello fellow Powcon users!

    i have recently purchased a 300SM, PDII and a 550smp all for less than £400 (bargain!)

    My question is this, has anyone modded their wirefeed to have the weld power control on it as well as the wirefeed speed?

    I’m looking to do this so as to save going back the the 300 every time i want to make an adjustment

    Any help or input/thoughts would be appreciated

    Thanks!

    BTW, how do you do the signature this at the bottom with the list of kit you use etc?

  2. #2
    Join Date
    Jun 2020
    Posts
    22
    Post Thanks / Like

    Re: Powcon 300sm remote weld power

    To create a signature, go to settings and select Edit Signature.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,257,011.43637 seconds with 18 queries