    hypertherm powermax 30 air problems

    So I bought a hypertherm powermax 30 air about a year ago and used it a bunch when I first got it and loved it but I got busy with work and other projects and just barely started using it again and now I'm having all sorts of problems. I made 3 or 4 cuts today and basically burned up a consumable set every cut. The arc wont stay lit and its constantly grounding out the side. Even after changing the consumables the arc comes out the end of the torch at a slight angle for some reason. The drag end is not working either the tip just sticks to the piece I'm trying to cut. The torch cap light keeps coming on and as far as i can tell i have put the torch together correctly. I just followed the diagram on the back of the machine. The temp led kept coming on as well but it was just like 60 in my shop not hot or cold and i was only cutting 1/8 steel so not very thick. Anybody else had problems like this?

  2. #2
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    update messed with it a little today machine seems to be way down on power arc wont stay lit and keeps arcing off of the retaining cap.

  3. #3
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,079
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Sounds as if the Pilot arc is staying engaged, and it is not transferring. I'm not a hypertherm person, but that is typically what happens when you see what you describe. Check your work clamp connections.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  4. #4
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    430
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Quote Originally Posted by banditman View Post
    So I bought a hypertherm powermax 30 air about a year ago and used it a bunch when I first got it and loved it but I got busy with work and other projects and just barely started using it again and now I'm having all sorts of problems. I made 3 or 4 cuts today and basically burned up a consumable set every cut. The arc wont stay lit and its constantly grounding out the side. Even after changing the consumables the arc comes out the end of the torch at a slight angle for some reason. The drag end is not working either the tip just sticks to the piece I'm trying to cut. The torch cap light keeps coming on and as far as i can tell i have put the torch together correctly. I just followed the diagram on the back of the machine. The temp led kept coming on as well but it was just like 60 in my shop not hot or cold and i was only cutting 1/8 steel so not very thick. Anybody else had problems like this?
    Did you happen to put in a new o-ring with the correct grease on it? I was having trouble with my hypertherm a few weeks ago after changing most all the consumables with neg results I tried a new oring with the grease and also made sure that I had a good ground problem solved.

  5. #5
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    ill try that and see if it works

  6. #6
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    The o ring you are talking about is the one one the torch head when you take the consumables off correct?

  7. #7
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    430
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Yes, here is a picture of my PAC 110 consumables. My Hypertherm is a old Powermax 350
    Attached Images Attached Images  
    Last edited by gnewby; 4 Weeks Ago at 10:34 PM.

  8. #8
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    5,983
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Quote Originally Posted by banditman View Post
    So I bought a hypertherm powermax 30 air about a year ago and used it a bunch when I first got it and loved it but I got busy with work and other projects and just barely started using it again and now I'm having all sorts of problems. I made 3 or 4 cuts today and basically burned up a consumable set every cut. The arc wont stay lit and its constantly grounding out the side. Even after changing the consumables the arc comes out the end of the torch at a slight angle for some reason. The drag end is not working either the tip just sticks to the piece I'm trying to cut. The torch cap light keeps coming on and as far as i can tell i have put the torch together correctly. I just followed the diagram on the back of the machine. The temp led kept coming on as well but it was just like 60 in my shop not hot or cold and i was only cutting 1/8 steel so not very thick. Anybody else had problems like this?
    Not familiar with the "air" hypertherm versions.... Does it have a built in water separator/filter?
    That would be the first thing I check.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  9. #9
    Join Date
    May 2015
    Posts
    79
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Hi,
    You might want to E-mail Jim Colt, he has been VERY helpful in the past!

    https://www.thefabricator.com/author/jim-colt

  10. #10
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    cant find the part number for the oring on the torch anybody know what it is by chance?

  11. #11
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    where did you get your orings from?

  12. #12
    Join Date
    Mar 2017
    Posts
    8
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Quote Originally Posted by gnewby View Post
    Did you happen to put in a new o-ring with the correct grease on it? I was having trouble with my hypertherm a few weeks ago after changing most all the consumables with neg results I tried a new oring with the grease and also made sure that I had a good ground problem solved.
    where did you get your orings from?

  13. #13
    Join Date
    Jan 2004
    Location
    South Central Kansas
    Posts
    430
    Post Thanks / Like

    Re: hypertherm powermax 30 air problems

    Quote Originally Posted by banditman View Post
    where did you get your orings from?
    I bought mine from Hypertherm along with other consumables including a tube of the grease.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,618,152,496.05537 seconds with 13 queries