    i got the millermatic211 about a week ago and noticed right away the gas is leaking from the bottom port on the regulator which seems to be the pressure relief valve. based on the stamping on the back of the valve im assuming 3000psi is blow off. my c25 when full was 1900. is there any adjustment or repair that can be done on the valve ? i havent yet put any wrenches on it because i didnt want to leave a bunch of tool marks in case i have to send it back for replacement and they say i damaged it. heres photo of the bottom port and inscribed backside
    Attached Images Attached Images   
    hypertherm powermax 30xp
    fronius transpocket 180
    fronius transsteel 2200
    fronius iwave 230i water cooled
    hobart handler 100

  2. #2
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    1,534
    Post Thanks / Like

    Re: c25 regulator help

    I have had that happen on two different flow meters....one it took just a little turn and the leak stopped while the other kept leaking even after I tightened the fitting a bit (returned that one). There's a good chance yours just needs a little nudge, but it's not a bad idea to make a call before you try doing anything to it. That way if a bit of tightening doesn't solve the issue you already have a reason why you messed with it.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  3. #3
    Join Date
    Nov 2014
    Location
    Southern CT
    Posts
    1,082
    Post Thanks / Like

    Re: c25 regulator help

    If it's leaking from that relief valve return it. Something inside is bad, maybe the diaphragm. Threaded fittings another story, I had one (Miller) that extremely tight hose fitting still had a slight leak. I put one layer of Teflon tape and it holds gas for days on end. Some times the treads are just not perfect.
    Ernie F.

  4. #4
    Join Date
    Mar 2015
    Location
    usa
    Posts
    1,201
    Post Thanks / Like

    Re: c25 regulator help

    i called miller and they sending a new regulator no questions asked so that cool
    hypertherm powermax 30xp
    fronius transpocket 180
    fronius transsteel 2200
    fronius iwave 230i water cooled
    hobart handler 100

  5. Likes Louie1961, walker liked this post
  6. #5
    Join Date
    Mar 2015
    Location
    usa
    Posts
    1,201
    Post Thanks / Like

    Re: c25 regulator help

    update. 3dys after calling miller there was brand new regulator at my house with no question asked. doesnt get any better service than that
    hypertherm powermax 30xp
    fronius transpocket 180
    fronius transsteel 2200
    fronius iwave 230i water cooled
    hobart handler 100

  7. Likes G-ManBart liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,301,269.45925 seconds with 22 queries