    Champion 10K red light on board

    OK, I have searched high and low. My Champion 10,000 loses power after a few seconds of running and a red light comes on on the board. I have read every thread I can find and the few times this light was mentioned no one ever explained what it means. I need help.

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    18,081
    Post Thanks / Like

    Re: Champion 10K red light on board

    The light means the unit has been overloaded either power or weld output.

    PM me an email address and I can send you some troubleshooting information.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. Likes mglsite liked this post
  4. #3
    Join Date
    Mar 2021
    Posts
    8
    Post Thanks / Like

    Re: Champion 10K red light on board

    I got it duaneb55, went to do the test on it. First thing I checked was the brushes. When started they have 125 to 130 volts DC, has power for maybe 30 seconds then the red light comes on and lose power. Voltage slowly drops to around 30 volts, red light goes out, power returns and it goes through the process of tripping out again. The board looks good with no burnt spots.

  5. #4
    Join Date
    Nov 2023
    Posts
    3
    Post Thanks / Like

    Re: Champion 10K red light on board

    Hi Duane, I am having a similar issue with my champion 10000. The unit creates voltage for around 5-10 seconds upon startup then the red light on the circuit board comes on and voltage falls off. Mine does not come and go however it stays off once it loses it and red light stays on. Any ideas? I have read that the current sensor could be bad. However I haven’t had any luck finding a place to order a new one.

  6. #5
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    18,081
    Post Thanks / Like

    Re: Champion 10K red light on board

    Check the thread you started. There's a test for the current sensor (hall device).
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,269,189.11190 seconds with 21 queries