    Champion 10K red light on board

    OK, I have searched high and low. My Champion 10,000 loses power after a few seconds of running and a red light comes on on the board. I have read every thread I can find and the few times this light was mentioned no one ever explained what it means. I need help.

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,392
    Post Thanks / Like

    Re: Champion 10K red light on board

    The light means the unit has been overloaded either power or weld output.

    PM me an email address and I can send you some troubleshooting information.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. Likes mglsite liked this post
  4. #3
    Join Date
    Mar 2021
    Posts
    8
    Post Thanks / Like

    Re: Champion 10K red light on board

    I got it duaneb55, went to do the test on it. First thing I checked was the brushes. When started they have 125 to 130 volts DC, has power for maybe 30 seconds then the red light comes on and lose power. Voltage slowly drops to around 30 volts, red light goes out, power returns and it goes through the process of tripping out again. The board looks good with no burnt spots.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,632,824,993.40466 seconds with 12 queries