+ Reply to Thread
Results 1 to 3 of 3

Thread: Hobart champion 10k No Weld has 110V

  1. #1
    Join Date
    Apr 2015
    Posts
    41
    Post Thanks / Like

    Hobart champion 10k No Weld has 110V

    Debating on purchasing hobart champion 10,000 from my employer. machine has 500 hrs. kohler motor. it will make light sparks but no weld. 110v works fine. engine also wont idle down it is stuck around 1/2 throttle. checked bridge rectifier it is okay. visual inspection of board see no burnt spots or obvious issues. keeps blowing CB4 breaker. when you push it in it will idle back down but blows after around 10 seconds. i know these are known for bad boards so im not ruling it out... actually think it probably is the board but unsure of the next step. thanks.

  2. #2
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    4,233
    Post Thanks / Like

    Re: Hobart champion 10k No Weld has 110V

    Get owners manual and diagram. figure out why cb4 is tripping.
    CB4 powers SR2. converts AC power from the stator to DC for the pcb
    SR2 lives on the side of the main weld diode assembly.
    Supplies power to the rotor so it makes output. you will need the welder to come up to full operating speed for weld output. so try disconnecting the throttle solenoid near it. welder should go full speed. see if CB4 still trips. If it doesn't solenoid might be bad. if it still trips. pcb might be bad.

  3. #3
    Join Date
    Apr 2015
    Posts
    41
    Post Thanks / Like

    Re: Hobart champion 10k No Weld has 110V

    Quote Originally Posted by ccawgc View Post
    Get owners manual and diagram. figure out why cb4 is tripping.
    CB4 powers SR2. converts AC power from the stator to DC for the pcb
    SR2 lives on the side of the main weld diode assembly.
    Supplies power to the rotor so it makes output. you will need the welder to come up to full operating speed for weld output. so try disconnecting the throttle solenoid near it. welder should go full speed. see if CB4 still trips. If it doesn't solenoid might be bad. if it still trips. pcb might be bad.
    thanks for the reply. machine is still sitting at my employer ive been really busy with work/home life. still deabting on it but its not really going anywhere lol. hopefully i will get some time sooner or later to check it out.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,279,184.63009 seconds with 20 queries