    Tasty beads Brah!

    Name:  IMG_1309.jpg
Views: 647
Size:  127.3 KBWell almost, LOL. I just did a job at a water treatment plant. Had 350' of 14" .375 pipe, compressed air moves thru it for airiation of waste water. Disclaimer: I'm not a pipe liner more of a pipe dreamer. I'm rocking a Pipe Pro 400 w/catapillar, awesome machine but haven't found the perfect settings yet.
    We've done so much, for so long, with so little. Were now qualified to do anything with nothing !

  2. Likes Oscar, SweetMK, 12V71, CAVEMANN, Kelvin, Mikel_24 liked this post
  3. #2
    Join Date
    Dec 2018
    Posts
    10,053
    Post Thanks / Like

    Re: Tasty beads Brah!

    Better than I can do. If it's round, I just walk away.

  4. Likes 12V71, welding1 liked this post
  5. #3
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    8,196
    Post Thanks / Like

    Re: Tasty beads Brah!

    Quote Originally Posted by farmersammm View Post
    Better than I can do. If it's round, I just walk away.
    Where is the fun in that?

  6. Likes farmersammm liked this post
  7. #4
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    6,264
    Post Thanks / Like

    Re: Tasty beads Brah!

    Quote Originally Posted by farmersammm View Post
    Better than I can do. If it's round, I just walk away.
    Wouldn't it be easier to roll it away since it's round.
    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    LET'S GO BRANDON!"INFLATION-THAT'S THE PRICE WE PAY FOR THOSE GOVERNMENT BENEFITS EVERYBODY THOUGHT WERE FREE."RONALD REAGAN
    JEFF

  8. Likes 12V71, farmersammm liked this post
  9. #5
    Join Date
    Nov 2009
    Location
    Tennessee
    Posts
    5,989
    Post Thanks / Like

    Re: Tasty beads Brah!

    Awe c'mon sammm, if you tried it I bet you would master it in no time. For someone that shoots for perfection like you do......
    "Where's Stick man????????" - 7A749
    "SHHHHHH!! I sent him over to snag that MIC-4 while tbone wasn't looking!" - duaneb55
    "I have bought a few of Tbone's things unlike Stick-Man who helps himself" - TozziWelding
    "Stick-man"

  10. Likes 12V71, farmersammm liked this post
  11. #6
    Join Date
    Mar 2015
    Posts
    95
    Post Thanks / Like

    Re: Tasty beads Brah!

    Just a bit of loose ripple, no biggie. You'll find your ripples will get more uniform the more you do it, until you don't even think about rod manipulation.

  12. Likes 12V71 liked this post
  13. #7
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    497
    Post Thanks / Like

    Re: Tasty beads Brah!

    I need to burn a truck load of those 6010's to find my style. Im more of a up hill weldor, with LoHi.
    We've done so much, for so long, with so little. Were now qualified to do anything with nothing !

  14. #8
    Join Date
    Mar 2011
    Location
    Bilbao, Spain
    Posts
    929
    Post Thanks / Like

    Re: Tasty beads Brah!

    That looks awesome to me! Good job.

    Mikel

  15. Likes welding1 liked this post
+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,308,034.31071 seconds with 20 queries