    Looking for a spoolmatic 3 for my millermatic 200 and cables to for a wc1 to connect to my other Miller matic 200 for spoolmatic 1

  2. #2
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,389
    Post Thanks / Like

    Re: Wanted spoolmatic 3

    Prior to the MM200 serial number JJ407380, the Spoolmatic 1 is a direct connect that doesn't require the WC1 weld control. Effective with serial number JJ407380 the WC1 is required to use the Spoolmatic 1 but the Spoolmatic 3 is a direct connect.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  3. #3
    Join Date
    Dec 2014
    Location
    sw minnesota
    Posts
    46
    Post Thanks / Like

    Re: Wanted spoolmatic 3

    I couldn't tell you the serial numbers of the machines of hand right now but they both have 14 pin plugs on them

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,389
    Post Thanks / Like

    Re: Wanted spoolmatic 3

    The 14-pin receptacles make the SM-3 a direct connect for both machines. You could also use the current - and lighter - Spoolmatic 15A or 30A guns with the WC-24 with both machines.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  5. #5
    Join Date
    Dec 2014
    Location
    sw minnesota
    Posts
    46
    Post Thanks / Like

    Re: Wanted spoolmatic 3

    Yeah I have thought about getting a 30a but I can't afford it for my shop.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,623,729,264.39280 seconds with 13 queries