    HYW products welding wire

    Has anyone used wire from HYW products ?they have pretty good prices for er70-s6 44lbs for 52 bucks, 4043 1lbs for 6 bucks. And dual shield wire was pretty cheap too.
    I'm thinking about trying it out just wanted to know if anyone else has used it and what they thought.

  2. #2
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: HYW products welding wire

    I have some stick welding rods of theirs. Work fine. I think I had ordered some wire from them a while back but never used it.
    1st on WeldingWeb to have a scrolling sig!



  3. #3
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    10,930
    Post Thanks / Like

    Re: HYW products welding wire

    Quote Originally Posted by K98dkmauser View Post
    Has anyone used wire from HYW products ?they have pretty good prices for er70-s6 44lbs for 52 bucks, 4043 1lbs for 6 bucks. And dual shield wire was pretty cheap too.
    I'm thinking about trying it out just wanted to know if anyone else has used it and what they thought.
    Do they offer MTRs with the wire?
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  4. #4
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: HYW products welding wire

    It was actually metal-core wire I bought from them. Haven't used it yet though.

    1st on WeldingWeb to have a scrolling sig!



  5. #5
    Join Date
    Dec 2007
    Location
    Central West Virginia
    Posts
    209
    Post Thanks / Like

    Re: HYW products welding wire

    I buy pallet quantities of E71 T1 .045 Works great for us.
    IF IT WORKS, DON'T FIX IT

    2 Lincoln CV-300 / LN-7 GMA
    Lincoln Power MIG 256
    CNC Table with Oxweld O/A & Hypertherm 1250G3
    Lincoln Ranger GXT 250
    Hobart-MicroWire 300
    ESAB Heliarc 161
    ESAB-Mobilemaster 2 CC/CV Feeders
    & More

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,249,331.92214 seconds with 18 queries