    Inexpensive bevel tool

    This video popped up on one of my Facebook groups for CNC plasma cutting.



    It is for an inexpensive bevel tool.

    I found a similar tool on Amazon for an even cheaper price at only $62 so just ordered one.

    https://www.amazon.com/dp/B08FX8741G...HNDBTX0J85QS9S

    I have not received the tool yet, so can't vouch for it. I have spent more money on dumber stuff so don't feel bad about giving it a shot.



    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  2. Likes Shootr, farmersammm, walker, whtbaron, arcflash liked this post
  3. #2
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,823
    Post Thanks / Like

    Re: Inexpensive bevel tool

    It looks pretty handy, probably ok for light to medium work.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  4. #3
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by CAVEMANN View Post
    It looks pretty handy, probably ok for light to medium work.
    That is what a lot of us do on a regular basis. I would not expect this to hold up to extended work or heavy work that some of the other folks on here do.

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  5. #4
    Join Date
    Feb 2015
    Posts
    114
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by psacustomcreations View Post
    That is what a lot of us do on a regular basis. I would not expect this to hold up to extended work or heavy work that some of the other folks on here do.

    Sent from my SM-G930V using Tapatalk


    I just bought one for my own toolbox. It may not hold up for the rest of my life, but at the price I really don't care. There are a lot of times when something like that tool could make a huge difference in some of the stuff I do.
    Thanks a lot for taking the time to post that video. I have never seen a tool just like that one.

    Sent from my E6810 using http://tiny.cc/Forums_reader

  6. Likes psacustomcreations liked this post
  7. #5
    Join Date
    Dec 2018
    Posts
    5,040
    Post Thanks / Like

    Re: Inexpensive bevel tool

    I LIKE THAT TOOL. It beats doing a setup to bevel anything on the mill. It would cut considerable time off of anything that doesn't have to be absolutely centered, and at a precision depth.

  8. #6
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    4,252
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by farmersammm View Post
    I LIKE THAT TOOL. It beats doing a setup to bevel anything on the mill. It would cut considerable time off of anything that doesn't have to be absolutely centered, and at a precision depth.
    But I thought everything had to be absolutely centered and at a precision depth....
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A
    Cut 50 Plasma
    Les

  9. #7
    Join Date
    Aug 2012
    Location
    AR
    Posts
    1,966
    Post Thanks / Like

    Re: Inexpensive bevel tool

    It would be great if they made one like that but was electric, like an angle grinder....(I know, they call them a grinding disk...). An electric bevel tool would at least make for a more uniform angle.

  10. #8
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by shortfuse View Post
    It would be great if they made one like that but was electric, like an angle grinder....(I know, they call them a grinding disk...). An electric bevel tool would at least make for a more uniform angle.
    If they had a bit with replaceable carbide inserts and then the bit fit into a trim router that should probably work light duty jobs.

    Something like this might work.

    https://www.menards.com/main/tools/p...4426656658.htm


    Sent from my SM-G930V using Tapatalk
    Last edited by psacustomcreations; 04-29-2021 at 11:53 AM.
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  11. #9
    Join Date
    Sep 2013
    Posts
    1,497
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by shortfuse View Post
    It would be great if they made one like that but was electric, like an angle grinder....(I know, they call them a grinding disk...). An electric bevel tool would at least make for a more uniform angle.
    Well, they do. Been around for awhile, too.




    The problem with the one in the OP is that it's small, therefore all the components are going to be small. Higher wear, greater noise, etc. Of course, the lower price point will have people buying them in droves, too, so it's a win for the company. Most likely, the folks buying them aren't going to use them nearly as much as they think and won't actually wear them out. Though, the #1 comment I'm seeing is that the customers don't really care if they wear them out or they break after a few months because they're so cheap they can just get another one. They almost don't need replaceable cutters since folks are so happy to just buy a whole new widget!

  12. #10
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,146
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Thanks for the video. I could put that to work.

    Check the link provided. There are larger and electric ones on that page.

  13. #11
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,630
    Post Thanks / Like

    Re: Inexpensive bevel tool

    All I have used all life is hand grinder.
    Simple and cheap.

    Dave

    Quote Originally Posted by psacustomcreations View Post
    This video popped up on one of my Facebook groups for CNC plasma cutting.



    It is for an inexpensive bevel tool.

    I found a similar tool on Amazon for an even cheaper price at only $62 so just ordered one.

    https://www.amazon.com/dp/B08FX8741G...HNDBTX0J85QS9S

    I have not received the tool yet, so can't vouch for it. I have spent more money on dumber stuff so don't feel bad about giving it a shot.



    Sent from my SM-G930V using Tapatalk

  14. #12
    Join Date
    Aug 2012
    Location
    AR
    Posts
    1,966
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Vaughn, Yeah! That Metabo beveling/chamfer tool (the small one) is what I had in mind. Thanks for posting the video.

    OUCH!! I just checked the price of one of them. 5/8" capacity at 45* was over $2700 at MSC.....too rich for my blood!
    Last edited by shortfuse; 04-29-2021 at 09:23 PM.

  15. #13
    Join Date
    Dec 2018
    Posts
    5,040
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by whtbaron View Post
    But I thought everything had to be absolutely centered and at a precision depth....
    Name:  mutley.gif
Views: 519
Size:  9.3 KB

  16. Likes arcflash liked this post
  17. #14
    Join Date
    Apr 2010
    Location
    Kenai, Alaska
    Posts
    755
    Post Thanks / Like

    Re: Inexpensive bevel tool

    I work mainly in aluminum so I've been using wood cutting carbide bits in a router since the '70's to get bevels like those shown in the pneumatic driven steel cutter.

    But the idea is the same, the functionality is the same. 6061 (Aaron the Tig god) uses one (for aluminum) mounted in his drill press table to bevel parts by moving the part not the router.

    Another post here shows a router using a bulb bit to create a U shaped butt joint prep for aluminum TIG in a pipe (vessel) that had to hold 800PSI.

    Of course its easier in aluminum since its so soft by comparison to steel.

    Thanks for posting video and showing this tool.

    Cheers,
    Kevin Morin
    Kenai, AK

  18. Likes VaughnT, psacustomcreations liked this post
  19. #15
    Join Date
    Jan 2005
    Posts
    4,280
    Post Thanks / Like

    Re: Inexpensive bevel tool

    I paid a bit more for a quality tool. It functions well..Amazon price was super cheap, and a much better value. (IMO)

    Esab/Lorch ET-220i
    Esab 160i caddy
    Thermal LM-200 Lincoln feeders
    Thermal Pee-Wee 85s
    Thermal 60i- 3phase /RPC powered (Beast)
    Thermal Drag-gun 35C
    INE 1500
    Klutch 140i

  20. #16
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    I received my small beveler in the mail today. It is indeed small. I will try it out later this weekend and report how it performs.




    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  21. Likes Shootr, Lis2323 liked this post
  22. #17
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    This little beveler works pretty well.
    The material making up the body feels much more robust than the typical Harbor Freight air tools.
    It is very compact and light.

    Here are some bevels on the outside of some 3/8" plate as well as inside some curves from tabs I cut in the plate. I can see that being handy for when you might want to make a bevel like that and a grinder will not fit.







    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  23. Likes Lis2323, VaughnT, Welder Dave liked this post
  24. #18
    Join Date
    Sep 2013
    Posts
    1,497
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Very nice, Pat. I especially like where you let that bevel fade out on the inside curve. Very elegant.

    How do the cutting edges look now that they're broken in? Any chips or other degradation? Are they a standard carbide insert you can buy anywhere?

  25. #19
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Thanks.
    The carbide inserts look good so far.
    They are standard inserts and available on Amazon

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  26. #20
    Join Date
    Nov 2013
    Posts
    443
    Post Thanks / Like

    Re: Inexpensive bevel tool

    And of course they are 6 sided (each triangle is flipped once you go around) so, should last a good bit before you have to even think about buying more....

  27. #21
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    Quote Originally Posted by BaTu View Post
    And of course they are 6 sided (each triangle is flipped once you go around) so, should last a good bit before you have to even think about buying more....
    This tool uses two inserts. These inserts are one sided but triangular shaped so only three cutting edges per insert. That should be plenty of edges for a while .
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  28. #22
    Join Date
    Nov 2013
    Posts
    443
    Post Thanks / Like

    Re: Inexpensive bevel tool

    I don't think you're looking at it right

    You dull an edge, take the screw out of the center, rotate the triangle to a new edge (so 3 cutting edges) THEN,,, you flip the triangle Over and have another 3!

  29. #23
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    788
    Post Thanks / Like

    Re: Inexpensive bevel tool

    German-made BDS heavy duty plate chamfering machine I bought a few weeks ago (not inexpensive). Takes separate carbide inserts (shown in package.



  30. Likes VaughnT liked this post
  31. #24
    Join Date
    Apr 2015
    Location
    Fredericksburg, VA
    Posts
    2,753
    Post Thanks / Like

    Re: Inexpensive bevel tool

    That BDS is ten times the price and I am sure it is worth it.
    I dont mind spending good money on tools I know I will use. I bought the Ellis 1800 for that reason.
    If it turns out I use the beveler more than I thought, I may step up to something more respectable

    Sent from my SM-G930V using Tapatalk
    Millermatic 252 MIG
    Miller Dynasty 200DX TIG
    Miller Spectrum 625 Plasma
    Altas 12x36 Metal Lathe
    Bridgeport Milling Machine
    www.psacustomcreations.com

  32. Likes ezduzit liked this post
  33. #25
    Join Date
    Dec 2003
    Location
    Fairfield,CT
    Posts
    1,415
    Post Thanks / Like

    Re: Inexpensive bevel tool

    pat, does this tool bevel edges that have been plasma cut of course after the dross has been removed. Not sure if you example is of plasma cut plates. Thanks.
    T.J.
    www.tjsperformance.com
    Dynasty 300 DX
    HTP 240
    HTP Microcut 380
    Hyperthem 85
    JD2 Hyd Bender and HF Hyd Ring Roller all in one =(Frankenbender)
    Bpt. Mill/DRO
    4' x 8' CNC Plasma Table
    Instagram: tjsperformance
    YT: TJS Welding and Fabrication

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,369,439.34816 seconds with 13 queries