    Water cooler failure??? bad day....

    Well my case has been altered quite a bit obviously.
    I added the PSI gauge and WhirlyGig water flow gadget and also a digital readout for water temperature going in/out

    Also has a large computer fan for the radiator

    Not that itís even needed with 5 gallons of coolant
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  2. #77
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,780
    Post Thanks / Like

    Re: Water cooler failure??? bad day....

    I was trying to account for mods. The Hot and cold lines were relocated... through me off.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,656,132,106.71708 seconds with 13 queries