Page 2 of 2 FirstFirst 12
Results 26 to 37 of 37

Thread: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Dentist

  1. #26
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    3,255
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Very nice, I will definitely remember and use that, thanks.

  2. Likes William McCormick liked this post
  3. #27
    Join Date
    Dec 2013
    Posts
    1,741
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    A mini "Jim Crow" rail bender. Whatever works.
    https://www.indiamart.com/universal-...chanical-jacks
    ---Meltedmetal

  4. Likes William McCormick liked this post
  5. #28
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    This is the one I made for the 3/4", 7/8", 1", and 1 1/4" solid bar. I took the right-angle grinder and broke the sharp corner so it would not dig into the stainless pipe and used it, haha. I will make another one just for 1.66" O.D. Pipe.

    Name:  PreLoadGadget.jpg
Views: 282
Size:  213.0 KB


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  6. #29
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    97
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    The JD Square is one of the nicest around for bending tubes. Race car guys love them. Me, I have a Hossfeld with hydraulics, its rough and crude and will bend tube, pipe, square and retangluar tubes, angle iron and flat bar. dies get expensive...
    It seemed like a good idea at the time!

  7. Likes William McCormick liked this post
  8. #30
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by welding1 View Post
    The JD Square is one of the nicest around for bending tubes. Racecar guys love them. Me, I have a Hossfeld with hydraulics, its rough and crude and will bend tube, pipe, square and rectangular tubes, angle iron, and flat bar. dies get expensive...
    I used a couple of different Hossfeld benders, I started on a Hockey stick, and then I used two different hydraulic Hossfeld's. They are good to have around. But if you get a Press brake/break, or even a press and a V-block and ram you start not using the Hossfeld as much. I used it to bend an arc into iron handrails and aluminum and brass handrails with plate aluminum-supported Teflon die's I made for it. I miss it.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  9. #31
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    I got my little bending cart made for the JD Squared bender. It came out nice. Very solid, and stable, with or without the step locks engaged.

    Name:  JD Bender Rolling Cart.jpg
Views: 173
Size:  195.0 KB

    Name:  JD Bender Cart.jpg
Views: 172
Size:  129.2 KB

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  10. Likes Lis2323, wb4rt liked this post
  11. #32
    Join Date
    Nov 2004
    Location
    Southern Montana
    Posts
    970
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by William McCormick View Post
    I got my little bending cart made for the JD Squared bender. It came out nice. Very solid, and stable, with or without the step locks engaged.
    Your support/cart is the cat's meow. Now, if were only remote-controlled for easy movement around your shop.

  12. Likes William McCormick liked this post
  13. #33
    Join Date
    Jan 2011
    Location
    Tx
    Posts
    247
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by William McCormick View Post
    I used a couple of different Hossfeld benders, I started on a Hockey stick, and then I used two different hydraulic Hossfeld's. They are good to have around. But if you get a Press brake/break, or even a press and a V-block and ram you start not using the Hossfeld as much. I used it to bend an arc into iron handrails and aluminum and brass handrails with plate aluminum-supported Teflon die's I made for it. I miss it.

    Sincerely,

    William McCormick
    Why do you prefer the JD to the Hossfeld?


    Sent from my iPhone using Tapatalk
    Miller Bobcat
    Harris cutting outfit
    Miller spectrum 625 plasma
    Variety of shopmade tools

  14. #34
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by jw3 View Post
    Why do you prefer the JD to the Hossfeld?


    Sent from my iPhone using Tapatalk
    I did a lot of stainless steel bends with a Hossfeld, and it is not terrible, but it does make you feel a little like Edward-scissor-hands. There was no angle indicator on the Hossfeld, although I suppose I could have made one. I had noticed that I was getting slightly different bends depending on how well I held the pressure on the pipe while repositioning the point where the cylinder was applying pressure with the Hossfeld.

    It did take me about five bends before I got a feel for the JD Squared bender as well. The auto-locking pin on the JD Squared bender is pretty cool. The only thing I am going to do is paint one of the removable pins, either the pin that locks the pipe to the die or the pin that locks the moving arm to the die, a certain color so that I do not mix them up. So far I am liking the bender.


    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  15. #35
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by Weldordie View Post
    Your support/cart is the cat's meow. Now, if it were only remote-controlled for easy movement around your shop.
    That bender cart moves like a good empty grocery cart once you get over the initial inertia needed to get it moving. Very easy to steer as well because there is only one pivoting wheel.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  16. #36
    Join Date
    Apr 2013
    Location
    Marina del Rey
    Posts
    805
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    This is what I did with my JD2 model 32 bender--mounted on a custom made frame I built to fit an ancient Kennedy roller cabinet. Installed the electro/hydraulic power pack inside the cabinet, with the motor end just barely poking through for cooling. Bending dies are stored in a rack at the bottom; accessories and related tools in the drawers. Wired it through the cabinet for convenience. Also shown is my first bending project done with it.





  17. Likes wb4rt, William McCormick liked this post
  18. #37
    Join Date
    Sep 2014
    Posts
    1,744
    Post Thanks / Like

    Re: Made A Stainless Steel Rail With My New JD2 Bender, After I Got Back From The Den

    Quote Originally Posted by ezduzit View Post
    This is what I did with my JD2 model 32 bender--mounted on a custom made frame I built to fit an ancient Kennedy roller cabinet. Installed the electro/hydraulic power pack inside the cabinet, with the motor end just barely poking through for cooling. Bending dies are stored in a rack at the bottom; accessories and related tools in the drawers. Wired it through the cabinet for convenience. Also shown is my first bending project done with it.





    Nice, I like the bending job too.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  19. Likes ezduzit, Durak liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,757,429.58673 seconds with 13 queries