Results 1 to 14 of 14

Thread: TIG welding cast iron

  1. #1
    Join Date
    Apr 2021
    Posts
    7
    Post Thanks / Like

    TIG welding cast iron

    I'd like to attempt a small TIG welding project - welding cast iron to steel.


    What TIG settings would you recommend?


    What type of filler rod is best?


    thanks a bunch

  2. #2
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,638
    Post Thanks / Like

    Re: TIG welding cast iron

    I would per heat parts before welding around 500° to 800°F.
    I use a torch for my cast iron work as do not have tig anymore.

    Dave

    Quote Originally Posted by lpm View Post
    I'd like to attempt a small TIG welding project - welding cast iron to steel.


    What TIG settings would you recommend?


    What type of filler rod is best?


    thanks a bunch

  3. #3
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    9,840
    Post Thanks / Like

    Re: TIG welding cast iron

    I use EZ Weld Tig wire which has never failed me yet, especially on some irreplaceable expensive parts. Follow the instructions and keep the part cool.

    https://ezweldtigwire.com/
    Weld like a "WELDOR", not a wel-"DERR"
    MillerDynasty700DX,Dynasty350DX4ea,Dynasty200DX,Li ncolnSW200-2ea.,MillerMatic350P,MillerMatic200w/spoolgun,MKCobraMig260,Lincoln SP-170T,PlasmaCam/Hypertherm1250,HFProTig2ea,MigMax1ea.

  4. Likes Woznme liked this post
  5. #4
    Join Date
    Dec 2016
    Posts
    130
    Post Thanks / Like

    TIG welding cast iron

    I hear aluminum bronze works good.


    Sent from my iPhone using Tapatalk

  6. #5
    Join Date
    Nov 2012
    Location
    North Port Florida
    Posts
    87
    Post Thanks / Like

    Re: TIG welding cast iron

    Do you mean Silcone bronze?
    Quote Originally Posted by ljmelius View Post
    I hear aluminum bronze works good.


    Sent from my iPhone using Tapatalk
    It seemed like a good idea at the time!

  7. #6
    Join Date
    Mar 2018
    Posts
    97
    Post Thanks / Like

    TIG welding cast iron

    Quote Originally Posted by welding1 View Post
    Do you mean Silcone bronze?
    Do you mean silicon bronze?

    Silicone is a synthetic elastomer. Silicon is an element.

    But more pertinently, why is silicon bronze better than aluminum bronze for cast iron?
    Last edited by jwmelvin; 05-08-2021 at 12:39 PM.

  8. #7
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,638
    Post Thanks / Like

    Re: TIG welding cast iron

    Most old cast iron is only Tensile strength: 25,000 psi.
    Brass brazing rod is Tensile strength: 65,000 PSI
    Brassing rod lower cost than silicon brazing rod

    Dave

    Quote Originally Posted by jwmelvin View Post
    Do you mean silicon bronze?

    Silicone is a synthetic elastomer. Silicon is an element.

    But more pertinently, why is silicon bronze better than aluminum bronze for cast iron?

  9. #8
    Join Date
    Dec 2016
    Posts
    130
    Post Thanks / Like

    Re: TIG welding cast iron

    Quote Originally Posted by welding1 View Post
    Do you mean Silcone bronze?
    Nope





    Jody does a good job explaining why he chose al bronze over silicon bronze.


    Sent from my iPhone using Tapatalk

  10. #9
    Join Date
    May 2021
    Location
    USA
    Posts
    2
    Post Thanks / Like

    Re: TIG welding cast iron

    If you also want to know the procedure. I am sharing a link about welding cast iron here. Hopefully it would be helpful.


  11. #10
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    878
    Post Thanks / Like

    Re: TIG welding cast iron

    Lots of questions....is it mild steel? How thick are the pieces you want to join, what sort of joint configuration and how critical are these welds (any load on them)?

    I have had zero success with the EZ Weld stuff for some reason, but I know others have had good luck. Brazing with either silicon bronze or aluminum bronze is a good option as suggested. I've had very good luck using Inconel filler rod to join cast iron and ductile iron to mild steel....but the rod isn't cheap. It's mostly nickel, so it's similar to using a nickel stick welding rod for cast iron. I actually keep an eye on eBay for old Inconel filler rod that's new old stock or just old. Often Inconel is being used on jobs with a defined process and they require documentation on the various components, so nobody is going to use an old batch of rods....and it winds up selling pretty cheap. The last tube I got was 8lbs and I paid $30 for it...not too painful.

    One thing I've found that works really well is to use a carbide bit in a die grinder to get the cast piece down to clean, white metal...you don't want to use a grinding wheel or flap disc as they leave behind residue (at least sometimes). I get the pieces set up and then run just an arc at low amperage (no filler) along the area to be welded. You'll get black soot coming out of the cast iron...that's carbon. Stop, use a stainless brush to clean off the carbon and repeat a few times until the black soot stops, then put down your first pass with filler rod. Cooking the carbon out seems to make a big difference and it also adds some preheat to the work as well.

    If it's a small piece that you didn't put a lot of heat into you may not even have to worry about trying to cool it slowly. If it's bigger, and/or got hotter I'll throw a welding blanket over the work to help keep heat in it longer.

    If there is any way you can do a practice weld with similar pieces that's always a good idea since older cast iron can really be mystery metal and there's no way of knowing exactly what you're dealing with.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  12. #11
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,638
    Post Thanks / Like

    Re: TIG welding cast iron

    You can weld with cast iron rod.
    When had a TIG weld I would weld with cast iron rod you still need to per heat

    Dave

  13. #12
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,839
    Post Thanks / Like

    Re: TIG welding cast iron

    Quote Originally Posted by Sophie View Post
    If you also want to know the procedure. I am sharing a link about welding cast iron here. Hopefully it would be helpful.

    More spam! She's Sophie on Welding Web and Emalia John on the link she posted about cast iron, says she's from Texas but her language skills scream India , or some other scam place.
    Last edited by CAVEMANN; 05-11-2021 at 03:46 PM.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  14. #13
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,156
    Post Thanks / Like

    Re: TIG welding cast iron

    Quote Originally Posted by Sophie View Post
    If you also want to know the procedure. I am sharing a link about welding cast iron here. Hopefully it would be helpful.

    Emilia, that’s a good overall summary article about the options.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  15. #14
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    1,156
    Post Thanks / Like

    Re: TIG welding cast iron

    Quote Originally Posted by CAVEMANN View Post
    More spam! She's Sophie on Welding Web and Emalia John on the link she posted about cast iron, says she's from Texas but her language skills scream India , or some other scam place.
    I did not get that impression from reading the article, but you may be right.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,567,868.27358 seconds with 14 queries