    Looks like going any bigger than 5/32" on stick electrodes 50lb tins is all I can find. Does anyone know where they might be available, say, in 10lb boxes?

    I'd like to try 3/16" and/or 7/32" 7018, 6011, and 6010. 50lbs is a ton of rod, and even 10lb is for me. Depending on the results, I might get through a 10lb box of 7018 on a project coming up. If I can't find the larger rods I may just settle for what I can source here - 5lb boxes 3/32" to 5/32". I'm going to build up some thick fillets.

  2. #2
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,581
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    It's available. I have Lincoln Excalibur in 10 lb containers. Shipping is usually the killer with online purchases. I get mine thru my LWS which carries mainly Lincoln and Esab electrodes. Maybe a farm store but they tend to have 7018 in the AC configuration.

  3. #3
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    9,654
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    What are you welding for rods that thick.


    Sent from my iPhone using Tapatalk

  4. #4
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    196
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Yeah - that's my question - WHY? I weld a lot of thick (1" +) joints & very seldom do I even use 5/32. Mainly build it up with 3/32 & 1/8.

  5. Likes CAVEMANN liked this post
  6. #5
    Join Date
    Feb 2014
    Location
    VIRGINIA,MN
    Posts
    337
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    I guess one source you could try, is possibly ask your LWS what the price is for a 50lb box and then figure out what the prices per pound. Then perhaps call around at some road construction or heavy equipment shops and see if they have some. Perhaps a box of two dozen donuts and a little cash would get you some to try anyways.

    If I'm doing a lot of welding liners down to excavator buckets or bigger items I will use 3/16 diameter rod. I tried using 1/4 diameter rod and it welded down just fine but had a tendency to crack later on. I'm guessing it was from putting too much weld down all at one time when welding hard wear material. With plain mild steel that would have been fine.
    If you have something that is big enough to carry the heat, 5/32 is nice rod to use out of position as it still carries pretty flat vertical. I have done some welding vertical with 3/16 diameter rod but the base metal has always been at least 2 to 3 in thick to carry the heat. I have access to some 3/16 dia 6010, but never use it. Also some 3/16" 7024 Jetrod, for windy field days.

  7. #6
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    773
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    With 7/32" E7018 5lbs would be about 8 sticks. How many amps does it take to light that up ??

    You can always try Ebay, and craigslist.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  8. #7
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,581
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by albrightree View Post
    With 7/32" E7018 5lbs would be about 8 sticks. How many amps does it take to light that up ??

    You can always try Ebay, and craigslist.
    375 amps or so. They make 1/4" and I believe they used to make 9/32".

  9. #8
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,581
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    The larger electrodes are longer so the amount per pound can be somewhat misleading.

  10. #9
    Join Date
    Jun 2014
    Posts
    169
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by albrightree View Post
    With 7/32" E7018 5lbs would be about 8 sticks. How many amps does it take to light that up ??

    You can always try Ebay, and craigslist.


    According to miller welds app- E7018 = amp range is 260-340.

  11. #10
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,819
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by M J D View Post
    The larger electrodes are longer so the amount per pound can be somewhat misleading.
    Yep, the large 7024 rods I used were 4 rods per pound if I remember right.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  12. #11
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    876
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by BD1 View Post
    What are you welding for rods that thick.
    My guess:

    Name:  a_the_dozer-1.jpg
Views: 245
Size:  84.1 KB
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  13. Likes 12V71, CAVEMANN, welding1 liked this post
  14. #12
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,630
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Great job give driver protection for local
    Will do a Great for street clean up.

    Dave

    Quote Originally Posted by G-ManBart View Post
    My guess:

    Name:  a_the_dozer-1.jpg
Views: 245
Size:  84.1 KB

  15. #13
    Join Date
    Feb 2019
    Location
    Snyder TX
    Posts
    196
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Thats the guy that built that cause he was tee'd off about something & destroyed half a city?

  16. Likes welding1 liked this post
  17. #14
    Join Date
    Sep 2016
    Location
    Detroit, Michigan
    Posts
    876
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by cwby View Post
    Thats the guy that built that cause he was tee'd off about something & destroyed half a city?
    Yes, Marvin Heemeyer....tore up a lot of Granby, Colorado. He was actually a welder and muffler repair shop owner.
    Check out my bench vise website:
    http://mivise.com


    Miller Syncrowave 250DX
    Millermatic 350P with XR AlumaPro
    Miller Regency 200 with 22A feeder and Spoolmatic 3
    Hobart Champion Elite
    Everlast PowerTig 210EXT

  18. #15
    Join Date
    Jul 2020
    Posts
    410
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Looks like the amperage for 3/16-7/32 rods are between about 200-300a, 7018 7/32 goes up to about 330a though. Thats going off of the Lincoln rods for the amperage range for those sizes in 6010, 6011, 7018.

    Might just stick with 5/32.

    As to purpose - burly fillet welds on plate, namely for T joints but I have some large tube to plate fillets to do also.

  19. #16
    Join Date
    May 2017
    Location
    Pitman PA
    Posts
    763
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by albrightree View Post
    With 7/32" E7018 5lbs would be about 8 sticks. How many amps does it take to light that up ??

    You can always try Ebay, and craigslist.
    He was lookin for 5/32 not 7/32 rods. Ive run 7/64" and 1/4 inch rods at what Im thinkin was about 280 amps.

    Someone asked what you would use 5/32 for....rebuild a dragline bucket sometime with no wire feeder. I did it for years with my pipeliner. I resally coukdnt say anymore what the amps was but I know it was pegged and ran wide open with 1/4" 7018s. I was running them vertical too. Try that sometime for thrills, ****z, and giggles. If you can do that you got somethin goin on, not many men can do it.

    I would run a root and a hot pass or 2 with 1/8" 7018, 6010 or 6011 if it was real crummy and then I would jump right up to 3/16" 7018 at about 200 amps, steadily increasing the heat with evry pass, once I got up too about 240 amps i would do a big weave and then jump up to 1/4" or 7/64" whatever was available and crank that ol girl up all the way. The whole truck would shake when I struck an arc with the ol girl...ya gotta listen to an F163 motor when she gets a good quick load like that. My wife asked what was goin on with the truck shakin one morning...I told her the ol girl is having an orgasm...Mrs K just shook her head and walked away

  20. #17
    Join Date
    Jul 2020
    Posts
    410
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by Popeye an old miner View Post
    He was lookin for 5/32 not 7/32 rods.
    If you are referring to me, the OP - reread the original post.

    Quote Originally Posted by FlyFishn View Post
    Looks like going any bigger than 5/32" on stick electrodes 50lb tins is all I can find. Does anyone know where they might be available, say, in 10lb boxes?

    I'd like to try 3/16" and/or 7/32" 7018, 6011, and 6010. 50lbs is a ton of rod, and even 10lb is for me. Depending on the results, I might get through a 10lb box of 7018 on a project coming up. If I can't find the larger rods I may just settle for what I can source here - 5lb boxes 3/32" to 5/32". I'm going to build up some thick fillets.
    5/32 might be the route to go, though, as it is easy to source. The original question was in reference to 3/16 and 7/32 in smaller quantities than 50lb tins.

  21. #18
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    3,821
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    I rebuilt half the "plow"(cowcatcher) on a 125 ton mine locomotive in 1987, most everything was 3/4", and 1 1/2" inch plate, I welded all that back in with 1/8" 7018, it took out several more cows after that & never fell off, LOL & hadn't been touched when they shut the plant down in 1999.
    IMPEACH BIDEN!
    NRA LIFE MEMBER

    UNITWELD 175 AMP 3 IN1 DC
    MIDSTATES 300 AMP AC MACHINE
    GOD HELP AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  22. #19
    Join Date
    May 2021
    Location
    Landrum, SC
    Posts
    25
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by FlyFishn View Post



    5/32 might be the route to go, though, as it is easy to source. The original question was in reference to 3/16 and 7/32 in smaller quantities than 50lb tins.
    Swing by some welding shops, ask around local if you can you may get lucky. Hope you can find some and if you do have fun with it cause large rod is a blast to run.
    Lincoln 330 MPX
    Modified Tombstone
    Lincoln Activ8X / LN-25X-TVT
    Magnum PRO 250LX GT Spool Gun
    ¼ Ton of Torches OFC-A / OFG-A
    SMAW FCAW GMAW

  23. #20
    Join Date
    Dec 2018
    Posts
    5,012
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by G-ManBart View Post
    My guess:

    Name:  a_the_dozer-1.jpg
Views: 245
Size:  84.1 KB
    That was a terrible day. I lived in Colorado for a good part of my life, and was familiar with the town.

  24. #21
    Join Date
    Jul 2008
    Posts
    2,907
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by farmersammm View Post
    That was a terrible day. I lived in Colorado for a good part of my life, and was familiar with the town.
    There's a pretty decent documentary about it available somewhere (Tubi TV maybe? Netflix?) with lots of actual footage from the event. That guy was PISSED.

  25. #22
    Join Date
    Jun 2012
    Location
    Laredo, Tx
    Posts
    5,660
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by cwby View Post
    Yeah - that's my question - WHY? I weld a lot of thick (1" +) joints & very seldom do I even use 5/32. Mainly build it up with 3/32 & 1/8.
    because not everyone wants to do things the way you/others do things. To quote someone else: We tend to judge the actions of others by what we think our own standards are, conveniently forgetting those times when we did what we wanted to do because we wanted to do it, even against our better judgement.
    1st on WeldingWeb to have a scrolling sig!

    HTP Invertig 400
    HTP Invertig 221
    HTP ProPulse 300
    HTP ProPulse 200 x2
    HTP ProPulse 220MTS
    HTP Inverarc 200TLP
    HTP Microcut 875SC

  26. #23
    Join Date
    May 2017
    Location
    Pitman PA
    Posts
    763
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    [QUOTE=FlyFishn;8812516]If you are referring to me, the OP - reread the original post.


    Ok I thought you were lookin for 5/32 rods now I think I see you were lookin for bigger rods in general including 3/16 and bigger.

    Just disregard my post

  27. #24
    Join Date
    Jan 2011
    Location
    Hutchinson Kansas
    Posts
    588
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    I run 5/32 7018 pretty often. Probably more often than 1/8. but then Im working on Ag and construction equipment most of the time. Any time I can run 5/32 or 3/16 in one pass instead of multiple 1/8 passes its a win.
    I also have some 7/32 a buddy gave me. I also lucked out and found a box of 1/4 7018 on clearance sale at airgas. I turned out to have 4, 11#sealed boxes inside.
    Lincolin Power Wave 450, Lincoln Powermig 255, Lincoln Pro Mig 140, Lincoln Squarewave Tig 275, Miller Big 40 G(with Hobart Hefty suitcase), Thermal Arc 95S and Esab PCM875 in an already full machine shop.

  28. #25
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    945
    Post Thanks / Like

    Re: Larger rods in smaller quantities?

    Quote Originally Posted by albrightree View Post
    With 7/32" E7018 5lbs would be about 8 sticks. How many amps does it take to light that up ??

    You can always try Ebay, and craigslist.
    Takes about 380 amps to burn 7/32 7018 on heavy plate with my Hobart gas drive.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,272,464.86112 seconds with 15 queries