+ Reply to Thread
Page 2 of 2 FirstFirst 12
Results 26 to 34 of 34

Thread: Tig Cooler water temerature?

  1. #26
    Join Date
    Sep 2014
    Posts
    2,372
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    You should use the reinforced hose for the times it or another hose in the system gets pinched or stepped on and the temperature goes up for a minute or two. A filter in the system clogs, the pump does not put out because it froze and no longer maintains pressure or just wears out. I like the reinforced silicon hose myself, pricey for sure. Currently, I use the reinforced rubber hose it is a high-pressure hose for pneumatics like oxy-acetylene, which does get crunchy with time and needs to be replaced.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  2. Likes John T liked this post
  3. #27
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    140 big guy

  4. #28
    Join Date
    Apr 2020
    Posts
    55
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    Quote Originally Posted by Willie B View Post
    If it's that hot I'd say there is something wrong.
    Not really, just running 300 amps thru a 250 amp wp20 torch on a syncrowave 250.
    Once the coolant in the line boils the machine could use a rest too...

    Hasnt hurt anything so far
    Last edited by 2strokeforever; 05-16-2021 at 03:08 AM.

  5. #29
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    Quote Originally Posted by 2strokeforever View Post
    Not really, just running 300 amps thru a 250 amp wp20 torch on a syncrowave 250.
    Once the coolant in the line boils the machine could use a rest too...

    Hasnt hurt anything so far
    I'd say that's outside the norm though.
    1st on WeldingWeb to have a scrolling sig!



  6. #30
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    11,368
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    You might need to run a hose to the end of your tig torch lines then and fill up a trash can with the outlet water. That way it’s always cold water. Sounds like your water cooler you have know is not big enough or have a good enough cooling system.

    Mine has a radiator but no fan because it doesn’t need it yet. I do have 230 amps available

  7. #31
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    Quote Originally Posted by motolife313 View Post
    You might need to run a hose to the end of your tig torch lines then and fill up a trash can with the outlet water. That way it’s always cold water. Sounds like your water cooler you have know is not big enough or have a good enough cooling system.

    Mine has a radiator but no fan because it doesn’t need it yet. I do have 230 amps available
    You make a good point.
    My new/improved cooler runs in/out of a 5 gallon bucket of water
    I also have a radiator but I installed a electric cooling fan ( through a 220 V - 12V DC converter)

    Works great, i’ve welded at 220 A pretty steady and the water doesn’t even get warm. (On DC)
    So the fan is just overkill/peace of mind.

    I guess.

    I would imagine it would take a lot to get 5 gallons of water to the boiling point.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  8. #32
    Join Date
    Dec 2013
    Location
    Mount Tabor VT
    Posts
    10,585
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    Compare the stinger lead from your stick welder to the tiny braided line inside your cooler hose. It can be small because the heat is carried away by the water. If the water gets too hot it doesn't transfer enough heat.
    Zap ran years cooling only with city water. I tried it after I had ordered the cooler, but it was back ordered. I feel that would be fine, but our water supply isn't what it used to be. In the 1990s the 200 home system was supplied by two natural springs. There was very little mineral or other contaminants. US Government forced a "new" system on us at a cost of 2.2 million 1996 dollars. Water is warmer now, and leaves a film in a glass you can't hardly scrub out with steel wool. I'd worry about plugging a torch.
    An optimist is usually wrong, and when the unexpected happens is unprepared. A pessimist is usually right, when wrong, is delighted, and well prepared.

  9. #33
    Join Date
    Jun 2012
    Location
    Laredo + Midland/Odessa
    Posts
    7,132
    Post Thanks / Like

    Re: Tig Cooler water temerature?

    Quote Originally Posted by John T View Post
    You make a good point.
    My new/improved cooler runs in/out of a 5 gallon bucket of water
    I also have a radiator but I installed a electric cooling fan ( through a 220 V - 12V DC converter)

    Works great, i’ve welded at 220 A pretty steady and the water doesn’t even get warm. (On DC)
    So the fan is just overkill/peace of mind.

    I guess.

    I would imagine it would take a lot to get 5 gallons of water to the boiling point.
    Curious why you did not go with 240VAC fans instead?
    1st on WeldingWeb to have a scrolling sig!



  10. #34
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Tig Cooler water temerature?

    Quote Originally Posted by Oscar View Post
    Curious why you did not go with 240VAC fans instead?
    I did look into that..

    But couldn't find one in 200mm size.
    also, I'm using a digital temp display which runs on 12v.

    happy with the fan... it's silent.

    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  