    This project was to build a mount for a forward-facing camera for a power boat. The camera mount will attach to the bottom of the roof of the cockpit. The channel detail will be mounted to the bottom of the roof of the cockpit and will support the cables that go to the camera. The purpose of the camera is to provide excellent forward visibility even when the boat occupants are in sub-optimal locations. The first picture shows my friend and customer Ray holding the completed camera mount. It is ready for powder coating.

    1. Camera Mount
    Name:  1. Camera Mount.jpg
Views: 561
Size:  93.3 KB

    This was mostly a machining project, but I did have one weldment. Unfortunately, the weld maxed out my Miller Dynasty 200 DX welder. The foot was Ύ” x 1” x 4” Aluminum and the channel was 1/8” x 1” x 2”. I used the following parameters for the TIG weld:

    A/C Current output: 200 amps.
    Balance: 70% Electrode Negative
    Frequency: 50 Hz
    Electrode: 3/32” Tri Mix from Arc Zone.
    Shielding Gas: 75% Argon 25% He
    Shielding flow rate: 15 CFH

    Below is picture of one weld and a second picture of the entire 8’ weldment:

    2. Foot welded on
    Name:  2. Foot welded on.jpg
Views: 566
Size:  111.4 KB

    3. Entire channel
    Name:  3. Entire channel.jpg
Views: 554
Size:  71.5 KB

    The next picture shows the access cover removed to gain access to the cable.

    4. Access cover removed
    Name:  4.  Access cover removed.jpg
Views: 553
Size:  105.6 KB

    And here is the access cover installed.

    5. Access cover installed
    Name:  5. Access cover installed.jpg
Views: 556
Size:  108.3 KB
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  2. Likes William McCormick liked this post
  3. #2
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    This is a picture of the camera mount all done.

    6. Camera mount done
    Name:  6. Camera mount done.jpg
Views: 557
Size:  87.3 KB

    I used my Bridgeport for most of the work, but I used a router table to make the radii on all of the parts:

    7. Router table setup
    Name:  7. Router table setup.jpg
Views: 554
Size:  226.0 KB

    Here is a view from the camera. (As you can see the boat is still in its winter storage.)

    8. The cameras view
    Name:  8. The cameras view.jpg
Views: 564
Size:  105.3 KB

    Here is a front view of the boat. The camera mount will be installed on the bottom of the roof of the cockpit.

    9. Front view of boat
    Name:  9. Front view of boat.jpg
Views: 553
Size:  66.9 KB

    Last but not least here is a side view of the boat for perspective.

    10. Side view of boat
    Name:  10. Side view of boat.jpg
Views: 561
Size:  111.2 KB

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  4. Likes Shootr liked this post
  5. #3
    Join Date
    Feb 2009
    Location
    Central CA
    Posts
    340
    Post Thanks / Like

    Re: Camera Mount

    Maybe I don't understand how this whole thing is supposed to work, but it looks to me like every component of the project was designed to capture and hold water around the cable.

    Tim

  6. #4
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by timrb View Post
    Maybe I don't understand how this whole thing is supposed to work, but it looks to me like every component of the project was designed to capture and hold water around the cable.

    Tim
    Here is Ray’s response:

    Don, the camera mount and cable tray are going to be mounted on the top of the hard top, not the bottom. So the cable would be protected from the elements. Mostly the sun. The camera
    Will be hanging down.
    Name:  2A832769-9516-4315-849D-347D394B5229.jpg
Views: 501
Size:  95.4 KB

    This is the view of my stern camera as seen on my Garmin GPSMAP 7612.

    Name:  B936447F-0BB2-488C-975B-EFE310E49FAC.jpg
Views: 503
Size:  66.1 KB
    The new camera will be viewed in a similar fashion. My iPad or iPhone can connect to this device so I can see the camera image when not at the helm. Also I can change the heading of the auto pilot when trolling.

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  7. #5
    Join Date
    May 2020
    Location
    Arizona
    Posts
    610
    Post Thanks / Like

    Re: Camera Mount

    Yeah, I'm gonna have to go with the theory that the camera manufacturer probably planned for water exposure, seeing how it was designed for boating. (FLIR-type system?)

    And I'll bet a nickel to a dollar I couldn't slide a gnats a$$-hair between that cord cover plate and the mount.
    Yeswelder MIG-205DS
    (3) Angle Grinders at the Ready
    Just a hobbyist trying to improve

  8. #6
    Join Date
    Dec 2011
    Location
    Tampa FL
    Posts
    1,210
    Post Thanks / Like

    Re: Camera Mount

    In my experience it is often better to make items like this so the water can come and go as it pleases, sometimes trying to seal things up just causes water to get trapped.
    Mike

  9. #7
    Join Date
    Sep 2014
    Posts
    1,703
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by Don52 View Post
    This project was to build a mount for a forward-facing camera for a power boat. The camera mount will attach to the bottom of the roof of the cockpit. The channel detail will be mounted to the bottom of the roof of the cockpit and will support the cables that go to the camera. The purpose of the camera is to provide excellent forward visibility even when the boat occupants are in sub-optimal locations. The first picture shows my friend and customer Ray holding the completed camera mount. It is ready for powder coating.

    1. Camera Mount
    Name:  1. Camera Mount.jpg
Views: 561
Size:  93.3 KB

    This was mostly a machining project, but I did have one weldment. Unfortunately, the weld maxed out my Miller Dynasty 200 DX welder. The foot was Ύ” x 1” x 4” Aluminum and the channel was 1/8” x 1” x 2”. I used the following parameters for the TIG weld:

    A/C Current output: 200 amps.
    Balance: 70% Electrode Negative
    Frequency: 50 Hz
    Electrode: 3/32” Tri Mix from Arc Zone.
    Shielding Gas: 75% Argon 25% He
    Shielding flow rate: 15 CFH

    Below is picture of one weld and a second picture of the entire 8’ weldment:

    2. Foot welded on
    Name:  2. Foot welded on.jpg
Views: 566
Size:  111.4 KB

    3. Entire channel
    Name:  3. Entire channel.jpg
Views: 554
Size:  71.5 KB

    The next picture shows the access cover removed to gain access to the cable.

    4. Access cover removed
    Name:  4.  Access cover removed.jpg
Views: 553
Size:  105.6 KB

    And here is the access cover installed.

    5. Access cover installed
    Name:  5. Access cover installed.jpg
Views: 556
Size:  108.3 KB
    If you clean the aluminum nicely, make sure it is a perfect fit up, you can use Straight polarity DC or DCEN. Do not pay attention to the slag that forms on the weld, just poke the welding rod into the molten puddle cook it in and move slightly forward and repeat. You can weld 1" thick aluminum like that. The bead is small but extremely strong. You have to wait till the heat builds up in part though before you start adding wire. I would suggest a practice piece before you try it on something you have a lot of work in. I have welded hundreds of feet using that technique it is an extremely strong weld, stronger than an AC weld.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  10. #8
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by William McCormick View Post
    If you clean the aluminum nicely, make sure it is a perfect fit up, you can use Straight polarity DC or DCEN. Do not pay attention to the slag that forms on the weld, just poke the welding rod into the molten puddle cook it in and move slightly forward and repeat. You can weld 1" thick aluminum like that. The bead is small but extremely strong. You have to wait till the heat builds up in part though before you start adding wire. I would suggest a practice piece before you try it on something you have a lot of work in. I have welded hundreds of feet using that technique it is an extremely strong weld, stronger than an AC weld.

    Sincerely,

    William McCormick
    Thanks, I will give it a try.

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  11. #9
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    Name:  9ca0184d1349f7cd9d64788b47ac47e2--going-dutch-netherlands.jpg
Views: 320
Size:  45.5 KB

    Ya think they used stern cameras back in the day??

  12. #10
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by farmersammm View Post
    Ya think they used stern cameras back in the day??
    What a beautiful boat.

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  13. Likes farmersammm liked this post
  14. #11
    Join Date
    Mar 2021
    Location
    Near Roanoke, VA
    Posts
    228
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by farmersammm View Post


    Ya think they used stern cameras back in the day??
    I was on a 3,400 ton destroyer in the US Navy,, back in the early 1970's,,,
    We had no cameras,, and I do not remember seeing a rear viewing watch person,,
    There may have been one,, but, I hardly ever remember that ship operating in reverse,,, so maybe rear "eyes" were not needed?
    We did have a rear bridge,, and there was usually someone up there. (most of the ships controls were duplicated there)
    Maybe that guy looked back if needed?

  15. Likes farmersammm liked this post
  16. #12
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by Don52 View Post
    What a beautiful boat.

    -Don
    It's the Morgan https://www.mysticseaport.org/explore/morgan/

    Was one of the first plastic model ships I built as a kid, that's why I remember it.

  17. Likes William McCormick liked this post
  18. #13
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    We romanticize the old ships, but if you ever go on one, you see how they lived on those things. I can see why the press gangs had to be.

  19. #14
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    I've looked at some ships logs from that time, and you'd be amazed at how many people went overboard. YOU HAD TO GET ALONG WITH YOUR MATES IN THOSE DAYS, OR YOU'D BE TREADING WATER.

  20. Likes William McCormick liked this post
  21. #15
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    Anyways...........I like your work. Sometimes I bust your balz, but it's all for fun.

  22. #16
    Join Date
    Dec 2018
    Posts
    4,944
    Post Thanks / Like

    Re: Camera Mount

    in fun

  23. #17
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by farmersammm View Post
    It's the Morgan https://www.mysticseaport.org/explore/morgan/

    Was one of the first plastic model ships I built as a kid, that's why I remember it.
    Thanks for the link. I enjoyed reading about it.

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  24. Likes farmersammm liked this post
  25. #18
    Join Date
    Mar 2014
    Location
    Troy MI
    Posts
    393
    Post Thanks / Like

    Re: Camera Mount

    And this is what it looks like powder coated.

    Name:  91341491-C857-4532-BE9E-06835292614C.jpg
Views: 221
Size:  161.0 KB

    -Don
    Smith Oxyacetylene Torch
    Miller Dynasty 200DX
    Lincoln SP-250 MIG Welder
    Clausing/Coldchester 15" Lathe
    16" DuAll Saw
    15" Drill Press
    7" x 9" Swivel Head Horizontal Band Saw
    20 Ton Arbor Press
    Bridgeport
    Lincoln LE 31 MP & Lincoln 210 MP

  26. Likes ccogg, Shootr liked this post
  27. #19
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,867
    Post Thanks / Like

    Re: Camera Mount

    Quote Originally Posted by William McCormick View Post
    If you clean the aluminum nicely, make sure it is a perfect fit up, you can use Straight polarity DC or DCEN. Do not pay attention to the slag that forms on the weld, just poke the welding rod into the molten puddle cook it in and move slightly forward and repeat. You can weld 1" thick aluminum like that. The bead is small but extremely strong. You have to wait till the heat builds up in part though before you start adding wire. I would suggest a practice piece before you try it on something you have a lot of work in. I have welded hundreds of feet using that technique it is an extremely strong weld, stronger than an AC weld.

    Sincerely,

    William McCormick
    Definitely not dc positive, maybe on some thin stuff like 16 gauge. 1/8 tungsten can only handle about 85 amps or so. And on negative you need helium to break the layer on the aluminum that the ac cleans and eats through.

  28. #20
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    9,867
    Post Thanks / Like

    Re: Camera Mount

    I do apologize for insulting your intelligence William! Yes you are right it can be welded on dc- It did weaken the base metal a lot. Very easy to bend after welding, little tricky to get the rod in right tooName:  BA1B797E-F8B5-48E2-A378-A22F80047EC9.jpg
Views: 105
Size:  68.1 KB

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,623,548,464.95714 seconds with 15 queries