HTP tig cooler hose
Does anyone know where I can find replacement hose for the HTP cooler?
I feel it’s some kind of metric size possibly?
I’ve tried a couple different hoses
3/8
5/16
And it’s either too tight or too loose.
I’d like about 6 feet if I can get it
Miller 211
Hypertherm PM 45
1961 Lincoln Idealarc 250
HTP 221
True Wisdom only comes from Pain.
-
-
Re: HTP tig cooler hose
5/16" is tight, so 8.5mm would be better if available. But I made 5/16" work.
-
Post Thanks / Like - 2 Likes, 0 Dislikes
-
Re: HTP tig cooler hose
looks to be 8mm ID.5/16 will be slightly smaller but should fit .a negligible 0.06 mm or 0.003 in smaller.
mcmaster and grainger have metric stuff available.
-