+ Reply to Thread
Results 1 to 3 of 3

Thread: Everlast 62i power factor correction

  1. #1
    Join Date
    Sep 2007
    Posts
    35
    Post Thanks / Like

    Everlast 62i power factor correction

    Any one know if the 62i plasma has power factor correction. I am looking at buying one to drive one off a 12kva generator with a 32 amp receptacle when away from the workshop but experience has shown me some machines which invariably are the cheap generic chinese stuff are a mixed bag when it comes to generator use. The ones with power factor correction seem to be the ones to get for generator use.

    I know the specs for the 62i say 10kw generator required, but is that for flat out?

  2. #2
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    5,227
    Post Thanks / Like

    Re: Everlast 62i power factor correction

    Cheap or not, many machines have a PFC lower than 99%.

    We recommend using only clean power output generators. 10kw is what you need if we recommend it. That is based off the inrush not continuous. .

    Regardless, we recommend the generator output be considered "clean" which is 5% or less THD.

    Many companies have this. One of the best, but lowest priced models is the Northern Tool PowerHorse line.

    The problems aren't so much with the "cheap chinese plasma cutters", as it is with the cheaply made generators which are designed for maximum profitability designed only to run resistive loads and not electronic ones.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  3. #3
    Join Date
    Sep 2007
    Posts
    35
    Post Thanks / Like

    Re: Everlast 62i power factor correction

    Yea I have worked out my generator should run it OK. It will get loaded up pretty well though. It is a low THD generator, under 4%.

    I think I will order one as there are very limited options in this country for single phase 60 amp plasma cutters.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,297,700.55618 seconds with 20 queries