    Cutting Disassembling Steel Grate

    Long time reader, Great people here!

    Thanks in advance for any help you can give me

    I have a 48 x 48 steel bar grate that has 2 sides of 1/4 bars with 3/16 bar sandwiched between to join them

    Name:  20210513_094155.jpg
Views: 276
Size:  129.4 KB

    I'm trying to remove the bars from one side and reorient them on the other side

    The goal is to make the openings smaller and lighten it a bit

    I've tried a cutting wheel, recip saw, and plasma torch. All of which have their upside and down sides in time and consumables

    I realize that this may just be the nature of the beast, but I just feel like I'm missing something obvious

    If anyone has any experience with grates, maybe you could give me some suggestions

    Thanks!

  2. #2
    Join Date
    Jun 2012
    Location
    Sebeka and Bemidji MN
    Posts
    14,835
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    Buy more material (1/4" rod is cheap), cut more bars and weld them on the other side.

    On second thought, just make a new one - way faster
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  3. #3
    Join Date
    May 2021
    Location
    Landrum, SC
    Posts
    27
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    ^^^Dave has a good idea there^^^
    Unfortunately there in really no easy way to do what your doing the way your doing it or an easier way to do it.
    Lincoln 330 MPX
    Modified Tombstone
    Lincoln Activ8X / LN-25X-TVT
    Magnum PRO 250LX GT Spool Gun
    Ton of Torches OFC-A / OFG-A
    SMAW FCAW GMAW

  4. #4
    Join Date
    May 2017
    Posts
    4
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    That's what I thought, just didn't want to overlook something obvious

  5. #5
    Join Date
    Dec 2003
    Location
    Fairfield,CT
    Posts
    1,422
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    Yup.. Make a new one.
    www.tjsperformance.com
    Dynasty 300 DX
    HTP 240
    HTP Microcut 380
    Hyperthem 85
    JD2 Hyd Bender and HF Hyd Ring Roller all in one =(Frankenbender)
    Bpt. Mill/DRO
    4' x 8' CNC Plasma Table
    Instagram: tjsperformance
    YT: TJS Welding and Fabrication

  6. #6
    Join Date
    May 2017
    Posts
    4
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    I just keep thinking about the wire pipe cutters but I've never seen one done in a portable

    Something like a portable band saw

    Anyway, thanks again to all

  7. #7
    Join Date
    Sep 2013
    Posts
    1,519
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    Quote Originally Posted by mreinsmith View Post
    I just keep thinking about the wire pipe cutters but I've never seen one done in a portable Something like a portable band saw
    The 1/4" bars would be "easy" to snip off with some large bolt cutters, and then you'd just be left with grinding down the stubs where they're welded to the main body. The problem is that you're then left with a bunch of short bits that aren't really reusable to fill in the other side. Of course, buying some 1/4" round bar in long pieces is cheap and easy, so it's not like you absolutely have to use the cut-offs to do the filling in.


  8. #8
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    4,210
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    What will be its use. It it must be used then i would use a thin cutoff wheel. Cut vee notch at the weld. Seem like as much work as removing them in pieces.

    It has not been my experience that making grating is easy. Fixturing, spacing, checking , rechecking, bending distorted bars, then discovering you were 1/8 inch off and the last bar shows the difference.

  9. #9
    Join Date
    May 2017
    Posts
    4
    Post Thanks / Like

    Re: Cutting Disassembling Steel Grate

    I have several of these, so at the moment I am making a equipment storage cart and shelves

    I also wanted to make a plasma cutting table (although the powder coating burning off might be a an issue with that)

    Cutting off the bars around the perimeter is fairly easy

    That should give me enough to make add to the grid, for the rest I'm just going to cut them off to save weight

    I am going to try the V Cuts because that might actually help lining them up when rewelding

    I had an old stick welder that I donated to a friend of a friend. I'm kicking myself now because it had an attachment for "fusing/melting" bars together (I forget what they call that process)

    That would have been helpful DOH!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,627,662,437.21843 seconds with 14 queries