  1. #26
    Join Date
    Jul 2020
    Posts
    529
    Post Thanks / Like

    Re: Building up base, machining/tapping weld metal?

    Getting closer...

    I need to track down a 1/4" NPT tap. I have a 1/8" and something seems to hit me that I bought a 1/4" NPT a couple years ago so I need to dig a bit in my stuff boxes to see if I can find it.

    There is plenty of meat on either side of the side port for threading. Again, it will not be subject to much pressure at all.

    I am not sure how much more clean up I'll do on the shape of the manifold - it doesnt matter. All that matters is the placement of the holes (I'll flush it pretty good to degrease and get the chips out from inside etc).

    Name:  20210523_192807 cropped.jpg
Views: 151
Size:  158.6 KB

    Name:  20210523_192818 cropped.jpg
Views: 157
Size:  136.8 KB

  2. #27
    Join Date
    Jul 2020
    Posts
    529
    Post Thanks / Like

    Re: Building up base, machining/tapping weld metal?

    I found a tap the right size. I thought I bought one for a project about 3-4 years ago and ended up not using it. So I dug for it a bit and I found it. The tap worked OK - I didn't chip any teeth. It was a slow boat to China to get through carefully but it worked - with oil every so often and lots of backing out to clear chips. I think it will hold up for round 2 for the bigger manifold next, not sure when I'll get to it but I'm getting there slowly.

    Name:  20210524_190737.jpg
Views: 142
Size:  110.0 KB

    Name:  20210524_190748.jpg
Views: 147
Size:  76.5 KB



    These are all the local pieces in the set up. The hose will be shortened to what I need for the unit. The supply hose connects to the union (that is the larger female thread you see on the stack coming off the pancake regulator).

    Name:  20210524_193357.jpg
Views: 143
Size:  213.9 KB

  3. #28
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Building up base, machining/tapping weld metal?

    Not sure what you are making
    But this stuff works great on tapered threads....
    I never use teflon tape anymore.
    Name:  rector.jpg
Views: 122
Size:  66.9 KB
    .
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

  4. Likes FlyFishn liked this post
  5. #29
    Join Date
    Oct 2014
    Posts
    2,135
    Post Thanks / Like

    Re: Building up base, machining/tapping weld metal?

    Quote Originally Posted by John T View Post
    Not sure what you are making
    But this stuff works great on tapered threads....
    I never use teflon tape anymore.
    Name:  rector.jpg
Views: 122
Size:  66.9 KB
    .
    Just don't use it on pool equipment/chlorine or you will have more leaks than you can shake a stick at. One case where tape is best.

  6. #30
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    7,979
    Post Thanks / Like

    Re: Building up base, machining/tapping weld metal?

    Quote Originally Posted by danielplace View Post
    Just don't use it on pool equipment/chlorine or you will have more leaks than you can shake a stick at. One case where tape is best.
    Good point.

    you got me... That IS the one place I use teflon tape.

    although I have been known to get pissed off at a niggling leak and just PVC glue the damn thing...
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.

+ Reply to Thread

Quick Reply Quick Reply

Register Now

Please enter the name by which you would like to log-in and be known on this site.

Please enter a password for your user account. Note that passwords are case-sensitive.

Please enter a valid email address for yourself.

A) Welding/Fabrication Shop
B) Plant/Production Line
C) Infrastructure/Construction/Repair or Maintenance/Field Work
D) Distributor of Welding Supplies or Gases
E) College/School/University
F) Work Out of Home

A) Corporate Executive/Management
B) Operations Management
C) Engineering Management
D) Educator/Student
E) Retired
F) Hobbyist

Log-in

Posting Permissions

  • You may post new threads
  • You may post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,713,272,127.05332 seconds with 22 queries