    I have an xmt 350 that just exploded the capacitors, will cost about 1600 to fix. I found a powcon for sale. I was wondering, are these less expensive to fix than the XMT? I am sort of pissed about how much they want for the IGBTs in it. I dont mind fixing stuff, just getting screwed on the parts sucks. Would I be able to fix a powcon down the line if I buy it?

  2. #2
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,850
    Post Thanks / Like

    Re: POWCON 300sm vs XMT350

    problem is finding the parts. with powcon, arc products and now arcon all closed nobody has parts. If you search hard and watch cap sizes you might be able to replace the invert caps and output caps before they blow and cause something else to fail.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,624,527,977.60201 seconds with 13 queries