    Hi everyone,
    Very disappointed with my Temco Hammer crimper. Does not make a tight crimp no matter how many times I hit it with my 3 lb drilling hammer.
    What’s the secret to a Quality Crimp on this ultra fine stranded welding cable ?
    Thanks in advance

  2. #2
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    4,823
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by Jonath108 View Post
    Hi everyone,
    Very disappointed with my Temco Hammer crimper. Does not make a tight crimp no matter how many times I hit it with my 3 lb drilling hammer.
    What’s the secret to a Quality Crimp on this ultra fine stranded welding cable ?
    Thanks in advance
    A bigger hammer... I have a very similar crimper on every truck for field repairs and have had no issues. In the shop I use one in the 55 ton hydraulic press. I also like to use the Tweco lugs with the extended barrel with room for two crimps.
    Are you having pull outs or does it just not "look right"? On real fine stranded stuff sometimes a lug one size smaller will work better.

  3. Likes farmall liked this post
  4. #3
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by 12V71 View Post
    A bigger hammer... I have a very similar crimper on every truck for field repairs and have had no issues. In the shop I use one in the 55 ton hydraulic press. I also like to use the Tweco lugs with the extended barrel with room for two crimps.
    Are you having pull outs or does it just not "look right"? On real fine stranded stuff sometimes a lug one size smaller will work better.
    Thank you,
    I am able to pull the cable out with not much force. I am using long barrel 1/0-2/0 copper lugs. I do put double crimps as well.
    I do not have much room when I push the bare multi stranded wire into the lug. I am also getting grooves at the underside of the lug from the Temco hammer crimp tool. I am not sure if that is also a problem.

  5. #4
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    I do not crimp.
    I only solder for good condition at ampage.

    Dave

    Quote Originally Posted by Jonath108 View Post
    Hi everyone,
    Very disappointed with my Temco Hammer crimper. Does not make a tight crimp no matter how many times I hit it with my 3 lb drilling hammer.
    What’s the secret to a Quality Crimp on this ultra fine stranded welding cable ?
    Thanks in advance

  6. Likes Jonath108 liked this post
  7. #5
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    4,823
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by Jonath108 View Post
    Thank you,
    I am able to pull the cable out with not much force. I am using long barrel 1/0-2/0 copper lugs. I do put double crimps as well.
    I do not have much room when I push the bare multi stranded wire into the lug. I am also getting grooves at the underside of the lug from the Temco hammer crimp tool. I am not sure if that is also a problem.
    You're going to get grooves... hit it hard, then hit it harder. I've been using that style crimper for 40 years, there is no "overdoing it".

  8. Likes Jonath108, CAVEMANN liked this post
  9. #6
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Thank you
    I will beat the heck out of it.!

  10. #7
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Very good luck

    Dave

    Quote Originally Posted by 12V71 View Post
    You're going to get grooves... hit it hard, then hit it harder. I've been using that style crimper for 40 years, there is no "overdoing it".

  11. #8
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by smithdoor View Post
    Very good luck

    Dave
    Thank You !

  12. #9
    Join Date
    Oct 2014
    Posts
    1,142
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Your barrel is too big.

    Fine strand wire is more compact than the wire those were made to fit .

    Cut some strands off and put them in with the end to tighten it up in there before you crimp it. The barrel needs to be snug on the strands before you crimp. Go down one size and it may fit properly.

    Many electrical supply houses rent real press tools. Swing in and ask if you could make a couple crimps with one. No comparison in results but the wire still has to fit the barrel snug first. Sloppy wire fit makes for a sloppy crimp.
    Last edited by danielplace; 05-19-2021 at 11:16 AM.

  13. Likes Jonath108 liked this post
  14. #10
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,660
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    I would try and jam some copper shim material in there. A piece cut out of copper tubing works well. You want the absolute tightest fit possible before crimping. Tinning the end with solder may help but I'm not a fan of solder as I've seen connections get hot and fail but thats mainly a battery cable thing.

  15. #11
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    One advantage of soldering is you reuse the lug.
    But after using solder I no longer need to replace any lugs.

    One problems I had was employees will do a renumbered on anything this includes crimp lugs.
    In most shops have a torch handy so take a minute to solder.

    Dave

    FYI To big of lug just add more solder will do.

    Quote Originally Posted by danielplace View Post
    Your barrel is too big.

    Fine strand wire is more compact than the wire those were made to fit .

    Cut some strands off and put them in with the end to tighten it up in there before you crimp it. The barrel needs to be snug on the strands before you crimp. Go down one size and it may fit properly.

    Many electrical supply houses rent real press tools. Swing in and ask if you could make a couple crimps with one. No comparison in results but the wire still has to fit the barrel snug first. Sloppy wire fit makes for a sloppy crimp.
    Last edited by smithdoor; 05-19-2021 at 11:45 AM.

  16. #12
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by danielplace View Post
    Your barrel is too big.

    Fine strand wire is more compact than the wire those were made to fit .

    Cut some strands off and put them in with the end to tighten it up in there before you crimp it. The barrel needs to be snug on the strands before you crimp. Go down one size and it may fit properly.

    Many electrical supply houses rent real press tools. Swing in and ask if you could make a couple crimps with one. No comparison in results but the wire still has to fit the barrel snug first. Sloppy wire fit makes for a sloppy crimp.
    Thank you

  17. #13
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by smithdoor View Post
    One advantage of soldering is you reuse the lug.
    But after using solder I no longer need to replace any lugs.

    One problems I had was employees will do a renumbered on anything this includes crimp lugs.
    In most shops have a torch handy so take a minute to solder.

    Dave

    FYI To big of lug just add more solder will do.
    Thank You

  18. #14
    Join Date
    Oct 2014
    Posts
    3,729
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by M J D View Post
    I would try and jam some copper shim material in there. A piece cut out of copper tubing works well. You want the absolute tightest fit possible before crimping. Tinning the end with solder may help but I'm not a fan of solder as I've seen connections get hot and fail but thats mainly a battery cable thing.
    Several stingers and ground clamps come with a piece of thin shim stock to wrap around the cable to make it fit tighter. A good crimp or tight bolt is usually all you need. Soldering isn't common on simple connections.

  19. Likes Jonath108 liked this post
  20. #15
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,660
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by Welder Dave View Post
    Several stingers and ground clamps come with a piece of thin shim stock to wrap around the cable to make it fit tighter. A good crimp or tight bolt is usually all you need. Soldering isn't common on simple connections.
    I'm well aware of that, he's using crimp on lugs. Some of the lugs are sized for more than 1 size cable. If they don't fit fairly snug in the crimp on lug they won't crimp properly and hold securely. In this case the shim would take up some of the space, allowing a proper crimp.
    Miller xmt304, Miller S22 p12, Miier Maxstar SD, Miller 252 w 30A, Miller super32p12, Lincoln Ranger 9, Thermal Arc 181I with spoolgun, Hypertherm 10000 ,Smith torches. Esab 161lts miniarc.

  21. #16
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    5,379
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    I agree with smithdoor. I solder all mine with acid core solder then soak it in strong baking soda water to neutralize any acid that worked up in the strands.
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"
    Hobart G-213 portable
    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  22. #17
    Join Date
    Mar 2018
    Location
    Sechelt, BC
    Posts
    307
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Crimping is way better than soldering, the crimp (ahem) welds the cable strands into one lump on the lug. Soldering, you are gluing the cable in place with acid, two kinds of metal, one of which can fracture.
    Do not believe everything that you think.

  23. #18
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    You may want think about using elevators. The cables are lead connections.
    Remember you smart phones use solder.

    If like smashing things use crimp type using a hammer.

    Dave

    Quote Originally Posted by Xsbank View Post
    Crimping is way better than soldering, the crimp (ahem) welds the cable strands into one lump on the lug. Soldering, you are gluing the cable in place with acid, two kinds of metal, one of which can fracture.

  24. Likes Jonath108 liked this post
  25. #19
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Thanks for all of your advice !

  26. #20
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    One I found to handy is box of brass 1/2" NC nuts. If lose one it a pain to find one.
    But looking for box on internet can save day.
    I even have brass All-thread for new studs.
    My shop was over 30 minutes from closest hardware store, it saved a few long trip to have few replacement parts in shop.

    Dave

    Quote Originally Posted by Jonath108 View Post
    Thanks for all of your advice !

  27. #21
    Join Date
    Oct 2014
    Posts
    3,729
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by M J D View Post
    I'm well aware of that, he's using crimp on lugs. Some of the lugs are sized for more than 1 size cable. If they don't fit fairly snug in the crimp on lug they won't crimp properly and hold securely. In this case the shim would take up some of the space, allowing a proper crimp.
    I was agreeing with you. I think it's also important to only strip the insulator back till it fits up against the lug. Have seen a lot of cables showing the exposed copper and it can/will cause premature failure.

  28. #22
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    5,660
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by Welder Dave;8814That 072
    I was agreeing with you. I think it's also important to only strip the insulator back till it fits up against the lug. Have seen a lot of cables showing the exposed copper and it can/will cause premature failure.
    That about stripping only enough and adding a section of good heat shrink tubing over the stem of the lug is also a good idea.

  29. #23
    Join Date
    Oct 2015
    Location
    NW New Jersey
    Posts
    798
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    maybe go down on lug size and try something like a #0 to #1 crimp lug to see if its a better fit. The wire should be a little snug going in.
    Airco 250 ac/dc Heliwelder Square wave
    Miller Synchrowave 180 sd
    Miller Econo Twin HF
    Lincoln 210 MP
    Dayton 225 ac/dc
    Victor torches
    Snap-On YA-212
    Lotos Cut60D

  30. Likes Jonath108 liked this post
  31. #24
    Join Date
    Feb 2021
    Location
    NY
    Posts
    84
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    Quote Originally Posted by smithdoor View Post
    One I found to handy is box of brass 1/2" NC nuts. If lose one it a pain to find one.
    But looking for box on internet can save day.
    I even have brass All-thread for new studs.
    My shop was over 30 minutes from closest hardware store, it saved a few long trip to have few replacement parts in shop.

    Dave
    can you explain how you use 1/2” NC brass bolts ? I am sure the studs are just steel as well as the washer and nut.
    thanks

  32. #25
    Join Date
    Mar 2018
    Location
    Clovis California
    Posts
    2,741
    Post Thanks / Like

    Re: How to Properly Crimp 1/0 ultra flex cable ?

    It is stud size on most welders.
    The nut holds the copper connector you just solder to cable.

    Most studs use 1/2" brass .

    The low cost welders will almost any size as found out.
    After I retired and sold my business I purchased a small welder from Harbor Frieght it used monkey threads aka metric.

    Dave

    FYI if the monkey threads fail or nut runs away I plan to real American threads 1/2" NC like all American welders use.

    Quote Originally Posted by Jonath108 View Post
    can you explain how you use 1/2” NC brass bolts ? I am sure the studs are just steel as well as the washer and nut.
    thanks
    Last edited by smithdoor; 05-21-2021 at 04:54 PM.

  33. Likes Jonath108 liked this post

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
Page generated in 1,628,094,451.54876 seconds with 12 queries